Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtek™ P60 (packable composite), Filtek™ P90 (Silorane-based composite) and Sonic fill™ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtek™ P60 and single bond™ Universal adhesive using horizontal incremental technique, group (B)the teeth were restored with Filtek™ P90 and P90 system adhesive using horizontal incremental technique and group (C) the teeth were restored with Sonic fill™ composite and single bond™ Universal adhesive using bulk technique.After specimens were stored in distilled water at 37°C for 7 days, all specimens were subjected to thermocycling at (5° to 55 °C), then submitted to mechanical load cycling (intermittent axial force of 49N and a total of 50.000 cycles). The specimens were observed under scanning electron microscope at (2000 X) to measure marginal gap width (the distance between the dental wall and the restoration) at occlusal, proximal and gingival regions in micrometer using Tescan software, version 3.5. Data were analyzed statistically by one way ANOVA test and least significant difference tests. Results:The results showed that the silorane-based posterior composite (Filtek™ P90) showed significantly the least marginal gap width at the occlusal, proximal and gingival regions after the application of thermal changes and mechanical load cycling in comparison to the two methacrylate-based posterior composite Filtek™ P60 (packable) and the Sonic fill™ (nano-hybrid). Sonic fill™ bulk fill composite that relied on the vibration concept to lower the viscosity of high filler loaded composite material showed significantly lesser marginal gaps width at occlusal, proximal and gingival composite/enamel interface regions in comparison with Filtek™ P60 (packable composite) using horizontal incremental technique. The silorane-based composite (Filtek™ P90) showed non-significant difference in marginal gaps width at the three different regions. While, both methacrylate based Filtek™ P60 and Sonic fill™ composite showed significantly lesser marginal gap width at the occlusal region in comparison with gingival regions. Conclusion: None of the low-shrinkage composite restorative materials tested in this study totally prevented micro-gap formation at composite/enamel interfaces of Class II MO cavity.
Background: Because of the demands for aesthetic orthodontic appliances have increased, aesthetic archwires have been widely used to meet patient's aesthetic needs. The color stability of aesthetic archwires is clinically important, any staining or discoloration will affect patient’s acceptance and satisfaction. This study was designed to evaluate the color stability of different types of aesthetic archwires after immersion into different types of mouth washes. Materials and methods: Four brands of nickel titanium coated aesthetic arch wires: Epoxy coated (Orthotechnology and G&H) and Teflon coated (Dany and Hubit) were evaluated after 1 week, 3 weeks and 6 weeks of immersion into two types of mouthwashes (Listerine with alcohol and
... Show MoreBackground: This study was formulated to compare the effect of 5%hydrofluoric acid in comparison to 37%phosphoric acid with and without the application of silane on bond strength of composite to porcelain. Materials and Methods: Specimen preparation was divided in to two phases, metal-disks fabrication (8mm-diameter and 4mm-thickness) and ceramic veneering. Thirty two specimens were prepared, sandblasted with 50 μm aluminum oxide, and divided into four groups of eight samples. Groups I and III were etched with 37%phosphoric acid while groups II and IV were etched with 5%hydrofluoric acid; and groups I and II were silaneted while groups III and IV were not. Heliobond, and resin composite were applied to each specimen using a plastic transpa
... Show MoreIn this paper, numerical and experimental studies on the elastic behavior of glass fiber reinforced polymer (GFRP) with stiffeners in the GFRP section's web (to prevent local buckling) are presented. The GFRP profiles were connected to the concrete deck slab by shear connectors. Two full-scale simply supported composite beams (with and without stiffeners) were tested under impact load (three-point load) to assess its structural response. The results proved that the maximum impact force, maximum deflection, damping time, and damping ratio of the composite beam were affected by the GFRP stiffeners. The experimental results indicated that the damping ratio and deflection were diminished compare
... Show MoreThis study compared in vitro the microleakage of a new low shrink silorane-based posterior composite (Filtek™ P90) and two methacrylate-based composites: a packable posterior composite (Filtek™ P60) and a nanofill composite (Filtek™ Supreme XT) through dye penetration test. Thirty sound human upper premolars were used in this study. Standardized class V cavities were prepared at the buccal surface of each tooth. The teeth were then divided into three groups of ten teeth each: (Group 1: restored with Filtek™ P90, Group 2: restored with Filtek™ P60, and Group 3: restored with Filtek™ Supreme XT). Each composite system was used according to the manufacturer's instructions with their corresponding adhesive systems. The teeth were th
... Show MoreBackground: The present study was conducted to evaluate the effects of different bleaching methods on the shear bond strength of orthodontic Sapphire brackets bonded to human premolars teeth using light cured composite resin and to determine the predominant site of bond failure. Materials and Methods: Thirty freshly extracted human premolars were selected and randomly divided into three groups (10 per group). These groups are: control (unbleached) group, hydrogen peroxide group (HP) 37.5% ; which is the in- office bleaching method group, carbamide peroxide group (CP) 16%; which is the at- home bleaching method group. After bleaching process was performed, all the teeth stored in distilled water in a sealed container at room temperature for
... Show MoreABSTRACT Background:Hydrogen absorption and related degradation in the mechanical properties of Ni-Ti based orthodontic wires has been demonstrated following exposure to fluoride prophylactic agents. This study was designed to investigate the effects of three fluoride containing agents on the load deflection characteristics of heat activated nickel titanium arch wires during unloading phase. Material and method: Eighty specimens of heat activated nickel titanium arch wires were obtained from Ortho Technology Company, half of which had a 0.016 inch round and 0.019x0.025 rectangular. Ten specimens from both wire size were immersed in one of the tested fluoride prophylactic agents (neutral sodium fluoride gel, stannous fluoride gel or phos-flu
... Show MoreBackground Obstructing dentinal tubules is a valuable approach for managing dentin hypersensitivity. Although various agents promote dentin remineralization, direct comparisons between theobromine, bioactive glass (BAG), and nano-hydroxyapatite (Nano-HAP) under simulated oral conditions remain limited. To fill this gap, this in vitro study aimed to evaluate and compare the effectiveness of these three treatments on exposed cervical dentin. The assessment focused on their chemical, morphological, and mechanical effects on dentin. Materials and methods Forty-eight human dentin slabs were obtained from the cervical portions of twelve sound premolar teeth. Baseline Raman spectroscopy and VMH tests were done to exclude outliers. All specimens we
... Show MoreThe paper presents mainly the dynamic response of an angle ply composite laminated plates subjected to thermo-mechanical loading. The response are analyzed by analytically using Newmark direct integration method with Navier solution, numerically by ANSYS. The experimental investigation is to fabricate the laminates and to find mechanical and thermal properties of glass-polyester such as longitudinal, transverse young modulus, shear modulus, longitudinal and transverse thermal expansion. Present of temperature could increase dynamic response of plate also depending on lamination angle, type of mechanical load and the value of temperature.