Evaluation of marginal gap at the composite/enamel interface in Class II composite resin restoration by SEM after thermal and mechanical load cycling (An in vitro comparative study)
...Show More Authors

Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtek™ P60 (packable composite), Filtek™ P90 (Silorane-based composite) and Sonic fill™ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtek™ P60 and single bond™ Universal adhesive using horizontal incremental technique, group (B)the teeth were restored with Filtek™ P90 and P90 system adhesive using horizontal incremental technique and group (C) the teeth were restored with Sonic fill™ composite and single bond™ Universal adhesive using bulk technique.After specimens were stored in distilled water at 37°C for 7 days, all specimens were subjected to thermocycling at (5° to 55 °C), then submitted to mechanical load cycling (intermittent axial force of 49N and a total of 50.000 cycles). The specimens were observed under scanning electron microscope at (2000 X) to measure marginal gap width (the distance between the dental wall and the restoration) at occlusal, proximal and gingival regions in micrometer using Tescan software, version 3.5. Data were analyzed statistically by one way ANOVA test and least significant difference tests. Results:The results showed that the silorane-based posterior composite (Filtek™ P90) showed significantly the least marginal gap width at the occlusal, proximal and gingival regions after the application of thermal changes and mechanical load cycling in comparison to the two methacrylate-based posterior composite Filtek™ P60 (packable) and the Sonic fill™ (nano-hybrid). Sonic fill™ bulk fill composite that relied on the vibration concept to lower the viscosity of high filler loaded composite material showed significantly lesser marginal gaps width at occlusal, proximal and gingival composite/enamel interface regions in comparison with Filtek™ P60 (packable composite) using horizontal incremental technique. The silorane-based composite (Filtek™ P90) showed non-significant difference in marginal gaps width at the three different regions. While, both methacrylate based Filtek™ P60 and Sonic fill™ composite showed significantly lesser marginal gap width at the occlusal region in comparison with gingival regions. Conclusion: None of the low-shrinkage composite restorative materials tested in this study totally prevented micro-gap formation at composite/enamel interfaces of Class II MO cavity.

View Publication Preview PDF
Quick Preview PDF
Publication Date
Mon Mar 13 2017
Journal Name
Journal Of Baghdad College Of Dentistry
Gingival microleakage of composite restorations with different bonding protocol in class II cavity treated with chlorhexidine (an in-vitro study)
...Show More Authors

ABSTRACT Background: One of the challenges to use chlorhexidine is its effect on the amount of microleakage after restoration; however, use of the materials with antibacterial properties after tooth preparation and before restoration has been widespread. The objective of this, in-vitro, study was to evaluate the influence of consepsis (chlorhexidine gloconate disinfectant) application on microleakage in class II cavities restored with light cured composite using universal adhesive system; etch and rinse technique –self etch technique. Materials and Methods: Forty class II cavities were prepared on mesial and distal surfaces of 20 non-carious mandibular third molars. The cavities were divided into four groups; (n =10 for each group).

... Show More
View Publication Preview PDF
Crossref
Publication Date
Mon Mar 31 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Aging effect of different types of composite resin restoration on shear bond strength to different orthodontic adhesives with sapphire bracket (In vitro comparative study)
...Show More Authors

Background: This study was performed to determine the effect of aging of different types of composite material restorations on: Shear bond strength (SBS) to light cure and no mix chemical cure orthodontic adhesives with sapphire bracket and the debonding failure sites. Materials and methods: One hundred forty four composite disks were made from three different composite resin materials which are: 3M Filtek Z250, 3M filtek Z350 and 3M Valux plus, each group with (48) disks each, then according to the duration of storage each group was subdivided into two equal groups one of them stored for one day and the other was stored for one month, then each group was further subdivided into two equal subgroups with (12) disks each one bonded with ligh

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 31 2025
Journal Name
Journal Of Baghdad College Of Dentistry
An Evaluation of Some Mechanical Properties of Autopolymerizing Acrylic Resin with the Modified One after Changing the Curing Environment: (In vitro Study)
...Show More Authors

Background: Studying and investigating the transverse strength(Ts), impact strength(Is), hardness (Hr) and surface roughness(Ra) of conventional and modified autopolymerizing acrylic resin with different weight percentages of biopolymer kraftlignin, after curing in different water temperatures; 40°C and 80°C. Material and Methods: Standard acrylic specimens were fabricated according to ADA specification No.12 for transverse strength, ISO 179 was used for impact testing, Shore D for hardness and profilometerfor surface roughness. The material lignin first dispersed in the monomer, then the powder PMMA is immediately added. Ligninadded in different weight percentages. Then cured using pressure pot (Ivomet) in two temperatures;40°C a

... Show More
View Publication Preview PDF
Publication Date
Sat Dec 28 2024
Journal Name
Dental Hypotheses
Assessment of Color Change of Artificial White Spot Lesions after Sandblasting with Bioactive Glass, Resin Infiltration, or Microabrasion Followed by Color Stability Test by pH Cycling: An in Vitro Study
...Show More Authors

Introduction: This study aimed to assess the color change of human teeth with artificial enamel white spot lesions (WSLs) after sandblasting with bioactive glass, resin infiltration, and microabrasion and to test color stability after pH cycling. Methods: Fifty extracted human mandibular first molars were randomly assigned into five groups: Sound, WSLs (untreated), and WSLs sandblasted with bioactive glass (Sylc), WSLs treated by resin infiltration (ICON), and WSLs treated by microabrasion (Opalustre), respectively. All specimens underwent a pH cycling procedure. The color parameters for each specimen were assessed using an Easyshade dental spectrophotometer at different time stages then the color changes (ΔE) were calculated. Results: The

... Show More
Preview PDF
Publication Date
Thu Jun 07 2018
Journal Name
Applied Physics A
Effect of incorporation of conductive fillers on mechanical properties and thermal conductivity of epoxy resin composite
...Show More Authors

View Publication
Crossref (45)
Crossref
Publication Date
Mon Mar 31 2025
Journal Name
Journal Of Baghdad College Of Dentistry
An in-vitro scan electron microscope comparative study of dentine-Biodentine interface
...Show More Authors

Background: Restoration of the gingival margin of Class II cavities with composite resin continues to be problematic, especially where no enamel exists for bonding to the gingival margin. The aim of study is to evaluate the marginal leakage at enamel and cementum margin of class II MOD cavities using amalgam restoration and modern composite restorations Filtek™ P90, Filtek™ Z250 XT (Nano Hybrid Universal Restorative) and SDR bulk fill with different restoratives techniques. Materials and method: Eighty sound maxillary first premolar teeth were collected and divided into two main groups, enamel group and cementum group (40 teeth) for each group. The enamel group was prepared with standardized Class II MOD cavity with gingival margin (1 m

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 31 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Remineralizing Toothpastes on Enamel Surface Roughness after Hybrid Laser Bleaching (An In vitro Study)
...Show More Authors

Background: one of the complications of power bleaching is surface roughness of enamel which increases the possibility of post bleaching teeth discoloration. The aim of the present study is to evaluate the effect of toothpaste containing nano hydroxyapatite, NovaMin and kin sense fluoride on surface roughness of human tooth enamel after laser bleaching with 35% hydrogen peroxide bleaching gel. Materials and Methods: Twenty human enamel incisors were cleaned and their labial surface polished up to #1200, then categorized into four equal groups; first group kept without bleaching as a control group, while the remaining three experimental groups were bleached with 35% hydrogen peroxide, and each group treated with a restore paste containing o

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 31 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The effects of various beverages on the shear bond strength of light-cured orthodontic composite (An in vitro comparative study)
...Show More Authors

Background: This study was conducted to assess the effects of various beverages on the shear bond strength of light-cured orthodontic composite used to bond stainless steel orthodontic brackets on human teeth and to determine the site of bonding failure of this material. Materials and Methods: Fifty extracted human premolars were selected and randomly divided into five equal groups each with 10 teeth according to the beverage type (Control, One Tiger, Milk, Green tea and Coffee). After bonding, the teeth were immersed in specific beverages for 5 minutes twice daily with equal intervening intervals then washed and stored in distilled water at 37º C for the reminder of the day. The process was carried out for 30 days. The samples were then

... Show More
View Publication Preview PDF
Publication Date
Wed Dec 14 2016
Journal Name
Journal Of Baghdad College Of Dentistry
Assessment of Enamel Surface after Debonding of Different Types of Esthetic Brackets (An In Vitro Study)
...Show More Authors

Background: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Sun Jan 01 2023
Journal Name
Dental Hypotheses
Effect of Dentin Surface Pretreatment With Chitosan Nanoparticles on Immediate and Prolonged Shear Bond Strength of Resin Composite: An in Vitro Study
...Show More Authors

View Publication
Scopus (1)
Crossref (1)