Background: Adjustment of any premature occlusal contact of any zirconia restoration requires its polishing or glazing in order to restore the smoothness of the restoration. The objective of this in vitro study was to evaluate the effects of different polishing systems and glazing on the surface roughness of full-contour zirconia. Material and methods: Forty disks (diameter: 8 mm, thickness: 6.4 mm) were prepared from pre-sintered full-contoured zirconia block; they were colored and sintered in a high-temperature furnace at 1500˚C for 8 hours. The specimens were then leveled and finished using grinding and polishing machine and adjusted using diamond disk. The specimens were then randomly divided into four groups (n=10), group I involves samples that were polished using (karat diamond polishing set, Vita zahnfabrik, Germany), group II involves samples that were polished with (zirconia polishing kit, SMEdent, Shanghai, China), group III involves samples that were polished with (OptraFine® diamond polishing system, Ivoclar Vivadent, Germany), while group IV involves samples that were glazed using glazing medium (VITA Akzent Glaze AKZ 25, Vita zahnfabrik, Germany). Surface roughness values (Ra) (in µm) of all the specimens were recorded at each stage of surface treatment of zirconia disks (leveling and finishing, adjustment of the samples and polishing / glazing) using surface roughness tester. Statistical analysis was carried out using one-way ANOVA and LSD tests. Results: The results showed that the glazing group recorded the lowest surface roughness mean value, followed by (OptraFine® polishing system), then (zirconia polishing kit) and finally (karat polishing set) which showed the highest mean of surface roughness. For all groups, there was a statistically very high significant difference of (Ra) value before and after adjustment of the samples. Moreover, there was a statistically very high significant difference in (Ra) value when comparing the adjusted samples with the polished and glazed ones. Karat polishing set group showed a statistically highly significant difference with zirconia polishing kit group (P<0.01). Both, karat polishing set and zirconia polishing kit groups showed a statistically very highly significant difference (P<0.001) with (OptraFine® polishing system) and glazing groups. On the other hand, no statistically significant difference was found between glazing and (OptraFine® polishing system) groups (P>0.05). Conclusions: Adjusting full-contour zirconia with diamond bur or disk resulted in a significant increase in (Ra) that necessitates its polishing or glazing to restore the surface smoothness. Furthermore, both glazing and OptraFine® polishing system provided the best surface smoothness, so glazing can be substituted with chairside polishing using OptraFine® polishing system.
This study was conducted to determine the ability of water treatment system (Vortisand) to reduce some chemical and physical properties for tigris river raw water, It consisted of turbidity, electrical conductivity, pH, total hardness, calcium Hardness as well as temperature in order to determine the unit`s efficiency for reducing their concentration as compared to those in the water produced by some classical potable water projects (Dora and Wathba) in Baghdad. Samples were collected during the cold months (December 2016 and January 2017) and during the hot months (May and June 2017). The results showed that this system has the ability to reduce some properties such as turbidity, the values were 215NTU in raw water and decreased to NTU
... Show MoreA total number of 33 isolates of Pseudomoans aeruginosa were collected from different clinical samples, such as: burn, wound and urine from patients attending Al-Yarmouk teaching hospital and some private clinical laboratories in Baghdad city through the period from October to December 2016. On the other hand, 21 isolates of P. aeruginosa were collected from 38 different food samples; such as: vegetables and fruits, from different local markets in Baghdad city during the period from November to December 2016. All isolates were identified by using different bacteriological and biochemical assays and confirmed by Vitek-2 identification system. The antimicrobial susceptibility test for clinical and food isolates towards 17 antimicrobial a
... Show MoreA new, simple, sensitive and fast developed method was used for the determination of methyldopa in pure and pharmaceutical formulations by using continuous flow injection analysis. This method is based on formation a burgundy color complex between methyldopa andammonium ceric (IV) nitrate in aqueous medium using long distance chasing photometer NAG-ADF-300-2. The linear range for calibration graph was 0.05-8.3 mmol/L for cell A and 0.1-8.5 mmol/L for cell B, and LOD 952.8000 ng /200 µL for cell A and 3.3348 µg /200 µL for cell B respectively with correlation coefficient (r) 0.9994 for cell A and 0.9991 for cell B, RSD % was lower than 1 % for n=8. The results were compared with classical method UV-Spectrophotometric at λ max=280 n
... Show MoreDiabetic mellitus is one of the main risk factors of fungal infections because poor glycemic control is associated with a high level of glucose in blood and saliva which could be treated as nutrient to fungi. This study aimed to isolate and identification of pathogenic fungi from diabetic patient. 140 samples were taken from different places of human body from the national center of diabetic patients that related to Mustansiriyah University / college of medicine and Al-yarmuk Hospital in Baghdad. 84 sample (60%) tested positive to fungi and 56 sample (40%) tested negative to fungi. The most frequented fungi isolated have been chosen for molecular identification by PCR (Millerozyma farinosa and Candida orthopsilosis) using specific pri
... Show MoreThe current study was to examine the reliability and effectiveness of using most abundant, inexpensive waste in the form of scrap raw zero valent aluminum ZVAI and zero valent iron ZVI for the capture, retard, and removal of one of the most serious and hazardous heavy metals cadmium dissolved in water. Batch tests were conducted to examine contact time (0-250) min, sorbent dose (0.25-1 g ZVAI/100 mL and 2-8 g ZVI/100 mL), initial pH (3-6), pollutant concentration of 50mg/L initially, and speed of agitation (0-250) rpm . Maximum contaminant removal efficiency corresponding to (90 %) for cadmium at 250 min contact time, 1g ZVAI/ 6g ZVI sorbent mass ratio, pH 5.5, pollutant concentration of 50 mg/L initially, and 250 rpm agitation speed wer
... Show MoreEight new complexes with the general formula [M(L)2(H2O)2] were prepared resulting from the reaction of the new Schiff base ligand [(E)-5- ((2-hydroxybenzylidene)amino)-2-phenyl-2,4-dihydro-3H-pyrazol-3- one(L)] with metal ions [manganese, cadmium, zinc, copper, nickel, cobalt, Mercury Bivalent and tetravalent platinum. This ligand was derived from the reaction of the amine (5-amino-2-phenyl-2,4-dihydro3H-pyrazol-3-one) with Salicylaldehyde, which is linked to the metal ions via two atoms. The nitrogen is the isomethene group, and the oxygen is the hydroxide group of the pyrazoline ring. The prepared compounds were characterized using infrared spectroscopy, nuclear magnetic resonance spectroscopy, and ultraviolet spectroscopy, and from the
... Show MoreThe fluorescence emission of Rhodamine 6G (R6G) and Acriflavine dyes in PMMA polymer have been studied by changing the irradiation and exposure time of laser light to know the effect of this parameter. It was found that the fluorescence intensity decreases in the polymer samples doped dyes as the exposure time increases and then reaches stabilization at long times, this behavior called photobleaching, which have been shown in liquid phase less than solid phase. Using 2nd harmonic with wavelength 530 nm laser, the photobleaching effect in the two dye-doped polymers different solvent but same was studied. It was observed that photobleaching of by different solution and by using dip spin coating the photobleaching seem in liquid phase
... Show More