Background: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CAD/CAM blocks (IPS e. max CAD) and Group D: Restored with resin nano ceramic CAD/CAM blocks (Lava Ultimate Restorative). Standard preparations were done using Ceramic Veneer Set (Komet). Indirect laminate veneers were cemented with the Relyx Veneer Cement (3M ESPE) and all specimens were stored in distilled water at 37°C for 2 weeks. The load was applied on the occlusal part of the veneer at 45˚ to long axis of the tooth using universal testing machine. Results were analyzed with one-way ANOVA and LSD tests. Specimens were examined by stereomicroscope at a magnification of 20x to evaluate the mode of failure. Results: Control group showed higher mean of fracture strength with highly significant difference in comparison to the experimental groups (P<0.01). (Group A) showed higher mean of fracture strength with statistically significant difference in comparison to (Group B and Group D). On the other hand the difference between (Group A and Group C) was statistically highly significant. Statistically non-significant difference was found among the three indirectly restored groups. Conclusions: All veneers used in this study can be considered as acceptable treatment in the premolars region for patients with normal biting force. Direct composite veneer is the most favorable technique in term of fracture strength, while IPS e. max CAD laminate veneers were least likely to fracture and most likely to completely debond.
Background: The aims of the study were to evaluate the unclean/clean root canal surface areas with a histopathological cross section view of the root canal and the isthmus and to evaluate the efficiency of instrumentation to the isthmus using different rotary instrumentation techniques. Materials and Methods:The mesial roots of thirty human mandibular molars were divided into six groups, each group was composed of five roots (10 root canals)which prepared and irrigated as: Group one A: Protaper system to size F2 and hypodermic syringe, Group one B: Protaper system to size F2 and endoactivator system, Group two A:Wave One small then primary file and hypodermic syringe, Group two B:Wave One small then primary file and endoactivator system, Gr
... Show MoreBackground: The bond strength of the root canal sealers to dentin seems to be a very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate the shear bond strength of four different obturation systems using push-out test. Materials and methods: Forty straight palatal roots of the maxillary first molars teeth were used in this study, these roots were instrumented using crown down technique and ProTaper system, instrumentation were done with copious irrigation of 2.5% sodium hypochlorite and 17% buffered solution of EDTA was used as final irrigant followed by distilled water, roots were randomly divided into four groups according to the obturation system (ten teeth for each g
... Show MoreBackground: Lack of durability of the bond of the dental adhesive systems to tooth structure is one of the most important problems in tooth colored restorative work. This in vitro study was performed to evaluate the effect of 2% chlorhexidine gluconate(CHX) on dentin bond strength by using total etch adhesive system at twenty-four hours and three months of water storage. Material and methods:A flat dentin surface was prepared for forty sound human maxillary premolar teeth which were acid etched with 36% phosphoric acid gel after being divided randomly into four groups of ten teeth each according to storage time and CHX application, theCHX was applied for 60 seconds before adhesive application for groups I and III which were tested after twe
... Show MoreBackground: This study was aimed to investigate the effect of three lingual button (Nickel free / rectangular base, Nickel free / round base and Composite) and bonding environment, wet and dry enamel surface, on: the shear bond strength (SBS) of light and self-cured Resin Modified Glass Ionomer Cements, and the debonding failure sites. Materials and method: One hundred twenty no-carious, free of cracks maxillary first premolar teeth were selected. Three types of orthodontic lingual buttons were used in this study: Nickel free / rectangular base, Nickel free / round base and Composite buttons. The teeth were divided into two groups of sixty teeth each. One group was used for testing the chemically cured GC Fuji Ortho Resin modified Glass Io
... Show MoreBackground: Denture relining is the process of resurfacing of the tissue side of the ill fitting denture, the bond strength at the relining-denture base interface is most important for denture durability.The aim of present study was to evaluate the shear bond strength between the thermosens as relining material and different denture base materials that bonded by thermo fusing liquid. As this corrective procedureis the common chair side procedure in the dental clinic. Material and method: Sixty samples were prepared and divided into three main groups according to the type of denture base materials.Group (A) referred to the heat cure acrylic samples which consisted of 20 samples. Group (B) referred to the high impact acrylic samples which con
... Show MoreBackground: Endodontically treated teeth have low resistance to fracture against occlusal forces. The strengthening effect of bonded esthetic onlay restoration on weakened tooth has been reported. This study aimed to assess the fracture resistance of endodontically treated premolars restored with composite with and without cuspal coverage by using direct and indirect techniques. Indirect technique done by CAD/CAM system (computer aided design –computer aided manufacturer) and laboratory processing. Material and methods: Forty human extracted maxillary premolars of approximately comparable sizes were divided into four groups: Group (A): Ten endodontically treated teeth directly filled with Filtek Z250xt without cuspal coverage. Group
... Show MoreBackground:sThe aims of this study were to evaluate and compare the ability of three different techniques to obdurate simulated lateral canals, evaluate the effect of the main canal curvature on obturation of lateral canals and compare the gutta-percha penetration between coronal and apical lateral canals. Materials and methods: Resin blocks with 30 straight and 30 curved were used in this study. Each canal has two parallel lateral canals. The main canal has 0.3 mm apical diameter and 0.04 taper. The canals were divided into six groups according to canal curvature and obturation techniques used (n=10): Groups C1 and C2: straight and curved canals obturated with continuous wave technique using E&Q masterTM system. Groups O1 and O2: straight
... Show MoreBackground: Ideal root canal obturation depends on many factors; one of them is good sealing of root canal without pores. The aim of this study was to determine the radiographic density of GuttaFlow® 2 with different obturation techniques using spiral computed tomography. Materials and Methods: Forty palatal roots of permanent maxillary first molar were used in this study. Following working length determination, root canal was prepared using rotary PROTAPER universal system. They were randomly divided into four groups of 10 roots each, the groups are Conventional lateral condensation with Apexit Plus sealer, Conventional lateral condensation with GuttaFlow® 2 as a sealer, Soft Core Regular with GuttaFlow® 2 as a sealer and singl
... Show MoreObjective: To evaluate the effect of mouth rinses (Biofresh and ZAK) on the surface micro hardness
of two light cure restorative material (Tetric ceram ivoclar-vivadent) and (3M Z 250) dental
composite.
Methodology: The microhardness values of (sixty) composite specimens were measured at the top
surfaces after 24 hours of immersion in different solutions (Biofresh, Zak mouth wash and distilled
water as control). Comparison done using descriptive statistics (mean, SD, SEM, minimum and
maximum values) and inferential statistics (ANOVA and LSD) test.
Results: The biofresh mouth rinse which has high alcohol containing has less effect on
microhardness of tetric ceram than the zak &distiled water , while the effect