Marginal Discrepancy and Fracture Resistance of CAD/CAM Ceramill Sintron Metal Copings with Different Porcelain Materials
...Show More Authors

Background: This study was performed to compare the marginal fit changes and facture resistance of metal ceramic crowns constructed from Ceramill Sintron metal coping veneered with three different porcelain veneering materials (Vita Master Koromikos VMK, Willi Geller Creation CC and GC initial MC), also to evaluate the influence of thermocycling on load at fracture. Materials and Methods: Master brass die was scanned ,then metal coping was designed and milled from Ceramill Sintron blank to get 60 metal copings, then divided randomly into three groups(20 sample), then veneered with porcelain: VITA, Creation or GC. The marginal gaps were measured before and after porcelain veneering then marginal fit changes was calculated. Fracture resistance test was done by Instron®, the master die was duplicated to sixty analogs then each analog was fixed into acrylic base. After that each crown was cemented onto the corresponding die analog. Ten samples of each group were subjected to compressive loading to fracture and other ten subjected to thermocycling followed by compressive loading to fracture. Result and Conclusion: The result of marginal fit changes showed that GC group had the lowest marginal gap follow by VITA and Creation. While VITA group showed the highest fracture resistance follows by GC then Creation. Thermocycling process did not significantly reduce the load at fracture for all groups.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Wed Mar 15 2023
Journal Name
Journal Of Baghdad College Of Dentistry
Crystallization firing effect on the marginal discrepancy of the IPS. emax CAD crowns using two different CAD/CAM systems
...Show More Authors

Background: Marginal adaptation is critical for long – term success of crown and bridge restoration. Computer aided design / computer aided manufacture (CAD/ CAM) system is gaining more importance in the fabrication of dental restoration. Objective: The aim of this study is to evaluate the effect of crystallization firing on the vertical marginal gap of IPS. emax CAD crowns which fabricated with two different CAD/CAM systems .Materials and Methods: Twenty IPS e.max CAD crowns were fabricated. We had two major groups (A, B) (10 crowns for each group) according to the CAD/CAM system being used: Group A: fabricated with Imes - Icore CAD/CAM system; Group B: fabricated with In Lab Sirona CAD/CAM system. Each group was subdivided into two s

... Show More
View Publication Preview PDF
Scopus (2)
Crossref (1)
Scopus Crossref
Publication Date
Wed Dec 14 2016
Journal Name
Journal Of Baghdad College Of Dentistry
Comparison of the Marginal Fitness of the Ceramic Crowns Fabricated with Different CAD/CAM Systems (An In Vitro Study)
...Show More Authors

Background: The marginal fit is the most characteristic that closely related to the longevity or success of a restoration, which is absolutely affected by the fabrication technique. The objective of present in vitro study was to evaluate the effect of four different CAD/CAM systems on the marginal fit of lithiµm disilicate all ceramic crowns. Materials and Methods: Adentoform tooth of a right mandibular first molar was prepared to receive all ceramic crown restoration with deep chamfer finishing line (1mm) and axial reduction convergence angle of 6 degree, dentoform model duplicated to have Nickel-Chromiµm master die. Thirty two stone dies produce from master die and distributed randomly in to four groups (8 dies for each group) accor

... Show More
View Publication Preview PDF
Crossref (3)
Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
An evaluation of the influence of different finishing lines on the fracture strength of full contour zirconia CAD/CAM and heat press all-ceramic crowns
...Show More Authors

ABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin ceme

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The Marginal Fitness of CAD/CAM All Ceramic Crowns Constructed by Two Typesof Direct Digitization Techniques (An In Vitro Study)
...Show More Authors

Background: In capturing a negative image, the digital impression secures a digital record for the purposeof designing and creating restorations. The introduction of scanning system presents a paradigm shift in the way of the dental impression procedure and encourages the accuracy of obtained restoration especially in the marginal area as a result of producing accurate final impression The digital system offers many advantages over the Conventional method.. The objective of this present in vitro study was to evaluate the marginal fitness of all ceramic crowns fabricated by direct digital scanning of the prepared tooth using two types of intra-oral cameras (Bluecam camera with strip light projection technique and Omnicam camera with video sa

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
An in vitro evaluation of fit of the crowns fabricated by zirconium oxide-based ceramic CAD/CAM systems, before and after porcelain firing cycles and after glaze cycles
...Show More Authors

Background: The objective of this in vitro study was to evaluate the vertical marginal fit of crowns fabricated with ZrO2 CAD/CAM, before and after porcelain firing cycles and after glaze cycles. Materials and Methods: An acrylic resin model of a left maxillary first molar was prepared and duplicated to have Nickel-Chromium master die. Ten die stone dies were sent to the CAD/CAM (Amann Girrbach) for crowns fabrication. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) before (Time 0) and after porcelain firing cycles (Time 1) and after glaze cycles (Time 2) using a light microscope at a magnification of ×100. One way ANOVA LSD tests were performed to determine wh

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 13 2017
Journal Name
Journal Of Baghdad College Of Dentistry
A study to compare the internal fitness and marginal gap between single crowns and crowns within three-unite bridge of zirconia substructure fabricated by CAD-CAM system. (An In vitro study)
...Show More Authors

ABSTRACT Purpose: the aim of this in vitro study was to compare the marginal gap and internal fitness between single crowns and the crowns within three-unit bridges of zirconium fabricated by CAD-CAM system. Materials and methods: A standard model from ivoclar company was used as a pattern to simulate three-units bridge (upper first molar and upper first premolar) as abutments used to fabricate stone models, eight single crowns for premolar and eight of three units bridges. Crowns and bridges fabricated by CAD-CAM system were cemented on their respective stone models then sectioned at the mid-point buccolingaully and misiodistaly and examined under stereomicroscope. Result: the marginal gap in premolar crowns and premolar within bridge we

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sun Jan 01 2023
Journal Name
Brazilian Dental Science
Effect of adhesive primer application on shear bond strength of self-adhesive cement to tooth structure and two different CAD/CAM milled blocks
...Show More Authors

View Publication
Crossref (1)
Scopus Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Fracture resistance of endodontically treated premolars with extensive MOD cavities restored with different composite restorations (An In vitro study)
...Show More Authors

Background: This in vitro study evaluated the fracture resistance of weakened endodontically treated premolars with class II MOD cavities restored with different composite restorations (Low-shrinkage Filtek P90, nanohybrid Filtek Z250 XT and SDR bulk fill). The type and mode of fracture were also assessed for all the experimental groups. Materials and Method: Fifty human adult maxillary premolar teeth were selected for this study. Standardized extensive class II MOD cavities with endodontic treatment were prepared for all teeth, except those that were saved as intact control. The teeth were divided into five groups of ten teeth each (n=10): (Group 1) intact control group, (Group 2) unrestored teeth with endodontic treatment, (Group 3) resto

... Show More
View Publication Preview PDF
Publication Date
Wed Jun 15 2022
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of Artificial Aging Test on PEEK CAD/CAM Fabricated Orthodontic Fixed Lingual Retainer
...Show More Authors

Background: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.

Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.

Results: The artificially aged retainers showed a marginally

... Show More
View Publication Preview PDF
Scopus (2)
Crossref (4)
Scopus Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Fracture strength of laminate veneers using different restorative materials and techniques (A comparative in vitro stuy)
...Show More Authors

Background: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CA

... Show More
View Publication Preview PDF