Background: Marginal adaptation is critical for long – term success of crown and bridge restoration. Computer aided design / computer aided manufacture (CAD/ CAM) system is gaining more importance in the fabrication of dental restoration. Objective: The aim of this study is to evaluate the effect of crystallization firing on the vertical marginal gap of IPS. emax CAD crowns which fabricated with two different CAD/CAM systems .Materials and Methods: Twenty IPS e.max CAD crowns were fabricated. We had two major groups (A, B) (10 crowns for each group) according to the CAD/CAM system being used: Group A: fabricated with Imes - Icore CAD/CAM system; Group B: fabricated with In Lab Sirona CAD/CAM system. Each group was subdivided into two subgroups pre-crystallized (Group A1, B1) and crystallized crowns (Group A2, B2). At four points on each aspect of the crown, marginal gaps were assessed on the master metal die by using digital microscope at a magnification of (110X) and image- J program. The measurement was done twice for each crown; before and after crystallization process.Results: The lowest mean of marginal gap before and after crystallization was (29.387±2.774μm) and (70.108±5.569μm) respectively for Group A (Imes - Icore system) and the highest mean value before and after crystallization was (51.728 ±3.774μm) and (84.071 ±4.567μm) respectively for Group B (Sirona system). Paired sample t-test result showed a statistically highly significant difference in marginal gap between all groups.Conclusions: The crystallization process increases the vertical marginal gap. Imes - Icore system showed the lower marginal gap than Sirona system. The two systems have an acceptable marginal gap
Background: The marginal fit is the most characteristic that closely related to the longevity or success of a restoration, which is absolutely affected by the fabrication technique. The objective of present in vitro study was to evaluate the effect of four different CAD/CAM systems on the marginal fit of lithiµm disilicate all ceramic crowns. Materials and Methods: Adentoform tooth of a right mandibular first molar was prepared to receive all ceramic crown restoration with deep chamfer finishing line (1mm) and axial reduction convergence angle of 6 degree, dentoform model duplicated to have Nickel-Chromiµm master die. Thirty two stone dies produce from master die and distributed randomly in to four groups (8 dies for each group) accor
... Show MoreBackground: This study was performed to compare the marginal fit changes and facture resistance of metal ceramic crowns constructed from Ceramill Sintron metal coping veneered with three different porcelain veneering materials (Vita Master Koromikos VMK, Willi Geller Creation CC and GC initial MC), also to evaluate the influence of thermocycling on load at fracture. Materials and Methods: Master brass die was scanned ,then metal coping was designed and milled from Ceramill Sintron blank to get 60 metal copings, then divided randomly into three groups(20 sample), then veneered with porcelain: VITA, Creation or GC. The marginal gaps were measured before and after porcelain veneering then marginal fit changes was calculated. Fracture resist
... Show MoreBackground: In capturing a negative image, the digital impression secures a digital record for the purposeof designing and creating restorations. The introduction of scanning system presents a paradigm shift in the way of the dental impression procedure and encourages the accuracy of obtained restoration especially in the marginal area as a result of producing accurate final impression The digital system offers many advantages over the Conventional method.. The objective of this present in vitro study was to evaluate the marginal fitness of all ceramic crowns fabricated by direct digital scanning of the prepared tooth using two types of intra-oral cameras (Bluecam camera with strip light projection technique and Omnicam camera with video sa
... Show MoreBackground: The objective of this in vitro study was to evaluate the vertical marginal fit of crowns fabricated with ZrO2 CAD/CAM, before and after porcelain firing cycles and after glaze cycles. Materials and Methods: An acrylic resin model of a left maxillary first molar was prepared and duplicated to have Nickel-Chromium master die. Ten die stone dies were sent to the CAD/CAM (Amann Girrbach) for crowns fabrication. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) before (Time 0) and after porcelain firing cycles (Time 1) and after glaze cycles (Time 2) using a light microscope at a magnification of ×100. One way ANOVA LSD tests were performed to determine wh
... Show MoreABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin ceme
... Show MoreABSTRACT Purpose: the aim of this in vitro study was to compare the marginal gap and internal fitness between single crowns and the crowns within three-unit bridges of zirconium fabricated by CAD-CAM system. Materials and methods: A standard model from ivoclar company was used as a pattern to simulate three-units bridge (upper first molar and upper first premolar) as abutments used to fabricate stone models, eight single crowns for premolar and eight of three units bridges. Crowns and bridges fabricated by CAD-CAM system were cemented on their respective stone models then sectioned at the mid-point buccolingaully and misiodistaly and examined under stereomicroscope. Result: the marginal gap in premolar crowns and premolar within bridge we
... Show MoreBackground: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.
Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.
Results: The artificially aged retainers showed a marginally
... Show MoreBackground: Maxillary first premolar with wide MOD cavity more susceptible to fracture. The aim of this study was to assess the influence of cavity design for cusp coverage on the fracture resistance of weakened maxillary first premolar restored with CAD/CAM hybrid ceramic versus nanohybide composite. Materials and Methods: Fifty six intact maxillary first premolars of approximately comparable sizes were divided into seven groups eight for each: Group A: Intact teeth (control group); Group B: teeth prepared for MOD inlay; Group C: teeth prepared for MOD onlay covering the lingual cusp; Group D: teeth prepared for MOD covering buccal and lingual cusps ,the previous three groups indirectly restored with nanohybrid composite (3M ESPE Z 250 X
... Show MoreObjective: This study evaluated the effect of immediate dentin sealing on the marginal adaptation of lithium disilicate overlays with three different types of resin-luting agents: preheated composite, dual-cure adhesive resin, and flowable composite. Materials and Methods: Forty-eight maxillary first premolars of similar size were prepared with a butt joint preparation design. The teeth were separated into two primary groups, each with twenty-four teeth: Group DDS: Delay dentin sealing (non-IDS) teeth were not treated. Group IDS: dentin sealing was applied immediately after teeth preparation. Each group was subsequently separated into three separate subgroups. Subgroups (DDS+Phc, IDS+Phc): cemented with preheated composite (Enamel plus HRi,
... Show More