Background: Esthetic treatment is the options of patient seeking orthodontic treatment. Therefore this study was conducted to measure the concentration of Aluminum, Nickel, Chromium and Iron ions released from combination of monocrysralline brackets with different arch wires immersed in artificial saliva at different duration, to evaluate the corrosion point on different parts of the orthodontic appliances before and after immersion in artificial saliva, and to evaluate the corrosion potential of each group of the orthodontic appliances. Material and methods: Eighty orthodontic sets prepared. Each set represents half fixed orthodontic appliance, from the central incisor to the first molar, for the maxillary arch, each set consisted of molar band, five brackets, half arch wire and ligature elastic.These sets are divided into two groups: Group A: with monocrystalline brackets divided into five subgroups (each subgroup has ten sets), but differ in arch wires, as numbered stainless steel, nickel-titanium, thermally activated, coated stainless steel and coated nickel-titanium arch wires respectively. Group B: with stainless steel brackets divided into three subgroups (also each subgroup has ten sets), but differ in arch wires, as numberedstainless steel, nickel-titanium, and thermally activated arch wires respectively. Used optical microscope to check the corrosion points, and used potentiostat techniques to indicate corrosion rate and tendency. Results: The greatest concentration of Aluminum and nickel ions release during the 1st week in group A, then sharply decreased in the 2nd week. The release of chromium ion released increase with increase intervals, while iron ion released decrease with increase time. Both nickel and chromium ions increase with increase intervals in group B,while iron increase to the maximum at 3rd weeks, then began to degrease. Optical microscope displayed pitting, crevices, and intergranular corrosion. Potentiostat techniques indicated that increase corrosion when used stainless steel and coated nickel titanium than others arch wires with group A, while corrosion increase with nickel titanium than stainless steel arch wires with group B. Conclusions: Non-significant difference in the total nickel, chromium and iron release in group B. Aluminum and iron increase in A4 and A5, while nickel and chromium increase in A1 and A2.The total released amounts of metals ions in both groups were less than the amounts of daily intake.
This research focuses on improvement of the corrosion behaviour of commercial pure titanium (Ti) grade II when exposed to Hank’s solution through different surface treatments. The disc shape of titanium samples were constructed to be divided according to their surface treatment. The first experimental group the Ti sample was exposed to computer numerical control (CNC) fiber laser machine. Whereas, the other experimental group the Ti sample was only coated with Polyetherketon keton (PEKK) by using carbon dioxide (CO2) laser technique while the last experimental group the Ti sample was treated with CNC fiber laser followed by PEKK coating by using CO2 laser technique. All were compared with the untreated control group. The electrochemical a
... Show MoreThe region of Kirkuk and its surrounding areas, including (Baba, Jambour, Qara Chuq, Qaiyarah, Demir Dagh, Bai Hassan, Taq Taq, Makhul, Gilabat as well as southern Mosul and the cities of Erbil and Sulymania, are known as one of the oldest discovered oil fields in northern Iraq. This area presents a significant opportunity for further organic geochemical analysis to describe maturation zones and estimate economically generated hydrocarbons with particular reference to the Sargelu formation, to enhance hydrocarbons productivity. To assess the potential of these oil fields, it is essential to perform correlation, comparisons, and geochemical analyses of the data collected from exploration wells in the surrounding area. This appro
... Show MoreSilver nanoparticles synthesized by different species
The nanostructured Manganese dioxide/Carbon fiber (CF) composite electrode was prepared galvanostatically using a facile method of anodic electrodeposition by varying the reaction time and MnSO4 concentration of the electrochemical solution. The effects of these parameters on the structures and properties of the prepared electrode were evaluated. For determining the crystal characteristics, morphologies, and topographies of the deposited MnO2 films onto the surfaces of carbon fibers, the X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), and atomic force microscopy (AFM) techniques were used, respectively. It found that the carbon fibers were coated with γ-MnO2 with a density that increased with increasing the de
... Show MoreAbstract
This work involves the manufacturing of MAX phase materials include V2AlC and Cr2AlC using powder metallurgy as a new class of materials which characterized by regular crystals in lattice. Corrosion behavior of these materials was investigated by Potentiostat to estimate corrosion resistance and compared with the most resistant material represented by SS 316L. The experiments were carried out in 0.01N of NaOH solution at four temperatures in the range of 30–60oC. Polarization resistance values which calculated by Stern-Geary equation indicated that the MAX phase materials more resistant than SS 316L. Also cyclic polarization tests confirme
... Show MoreInternal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone
... Show MoreInternal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone
... Show More