Background: The irradiation of teeth with a laser results in an interaction between the light and the biological constituents of the dental hard substance, which is converted directly into heat.This thermal effect is the cause of the structural and chemical enamel changes.The combined treatment of topical fluoride agent with laser may increase fluoride uptake, and reduce progression of caries-like lesions. The aim of this study was to measure the uptake of the acidulated phosphate fluoride and sodium fluoride to the buccal and lingual caries-like lesion enamel surfaces before and after irradiated by Nd-YAG laser in comparison with matching control group. Materials and methods: The sample consisted of 30 human healthy upper premolar teeth which were stored in 0.1% thymol solution after extracted. Every tooth divided into: buccal and lingual specimen, each specimen has a rectangular window which was divided to right and left halves (120 specimens). The sample was divided into 2groups (60 specimens) for buccal surface, and the same for lingual surface. The caries-like lesion was formed for all groups except control (1) each group treated with either acidulated phosphate fluoride 1.23% or sodium fluoride 2%, (30 specimens) which contain other subgroups, these are: (10 specimens) one half treated with fluoride agent only and another half as control (first group as control (1) without caries-like lesion, and the second group control (2) with caries-like lesion, then de-ionized water only). (10 specimens) treated with fluoride agent then irradiated by Nd-YAG laser; one half with program (1) (short pulse), andanother with program (2) (long pulse). (10 specimens) irradiated by Nd-YAG laser; one half with program (1) and another with program (2) then treated with fluoride agent. The specimens of enamel were sectioned and the fluoride uptake was determined with using fluoride sensitive electrode. Results: There was a significant difference between the buccal and lingual enamel surfaces regarding the fluoride uptake in sound tooth, while a non- significant difference was observed after artificial caries-like lesion formation. Conclusion: Irradiation of Nd-YAG laser program (1) to the buccal and lingual caries-like lesion surfaces of enamel before application of fluoride agents (APF, NaF) was significantly increase fluoride uptake than that of using laser after the application of fluoride agent, as well as from using laser of program (2) after and before the application of fluoride agent, and from using fluoride agent alone in the buccal and lingual surfaces.
Aim: The current study was aimed to determine the relationship between the orthodontic force applied by monobloc and the salivary level of alkaline phosphatase (ALP) and lactate dehydrogenase (LDH) enzymes, considering the time factor after insertion of the appliance and whether there is a correlation between these enzymes. Materials and methods: A sample of 28 growing patients requiring orthodontic treatment with myofunctional appliance (Monoblock) was taken for the current study with an age range 9 to 12 years,all patients had Angle's class II division 1 malocclusion with no or mild crowding, the sample was selected using simple random sampling. Only 16 subjects (10 males and 6 females) were included who follow certain inclusion criteria.
... Show MoreIn this research, the degradation of Dazomet has been studied by using thermal Fenton process and photo-Fenton processes under UV and lights sun. The optimum values of amounts of the Fenton reagents have been determined (0.07g FeSO4 .7H2O, 3.5µl H2O2) at 25 °C and at pH 7 where the degradation percentages of Dazomet were recorded high. It has been found that solar photo Fenton process was more effective in degradation of Dazomet than photo-Fenton under UV-light and thermal Fenton processes, the percentage of degradation of Dazomet by photo-Fenton under sun light are 88% and 100% at 249 nm and 281 nm respectively, while the percentages of degradation for photo-Fenton under UV-light are 87%, 96% and for thermal Fenton are 70% and 66
... Show MoreA laboratory experiment was carried out at the College of Agriculture University of Baghdad in 2017. The aim was to improve the anatomical and physiological traits of broad bean seedling under salt stress by soaking it in salicylic acid. The concentrations of salicylic acid were 0, 10, and 20 mg L-1 and the electrical conductivity levels were 0, 3, and 6 dS m-1. The complete randomized design was used with four replications. The increasing of salicylic acid concentration up to 10 mg L-1 led to increasing the stem cortex thickness, stem vascular bundles thickness, and root cortex thickness significantly by (34.9,36.7,and 55 µm) respectively, while the treatment of 20 mg L-1 led to decreasing these traits by (28.2, 27.8, and 48.1 µm
... Show MoreThis study conducted an analytical investigation on the behavior of concrete beams with openings reinforced by glass-fiber-reinforced polymer (GFRP) bars. In this study, five proposed beams reinforced by GFRP bars as flexural and shear reinforcement with openings were numerically examined. The variables were the opening orientation (vertical and horizontal) and the number of openings. These openings were located within the flexural zone of the proposed beams. The result shows that the vertical openings had a significant effect over the horizontal openings on reducing the ultimate load and increasing the mid-span deflection compared with the control beam. Moreover, the results showed t
Acrylic polymer/cement nanocomposites in dark and light colors have been developed for coating floors and swimming pools. This work aims to emphasize the effect of cement filling on the mechanical parameters, thermal stability, and wettability of acrylic polymer. The preparation was carried out using the casting method from acrylic polymer coating solution, which was added to cement nanoparticles (65 nm) with weight concentrations of (0, 1, 2, 4, and 8 wt%) to achieve high-quality specifications and good adhesion. Maximum impact strength and Hardness shore A were observed at cement ratios of 2 wt% and 4 wt%, respectively. Changing the filling ratio has a significant effect on the strain of the nanocomposites. The contact angle was i
... Show MoreIn this research, the degradation of Dazomet has been studied by using thermal Fenton process and photo-Fenton processes under UV and lights sun. The optimum values of amounts of the Fenton reagents have been determined (0.07g FeSO4 .7H2O, 3.5µl H2O2) at 25 °C and at pH 7 where the degradation percentages of Dazomet were recorded high. It has been found that solar photo Fenton process was more effective in degradation of Dazomet than photo-Fenton under UV-light and thermal Fenton processes, the percentage of degradation of Dazomet by photo-Fenton under sun light are 88% and 100% at 249 nm and 281 nm respectively, while the percentages of degradation for photo-Fenton under UV-light are 87%, 96% and for thermal Fenton are 70% and 66.8% at 2
... Show MoreThis work intends to develop an effective heavy metal-free modifier having properties comparable to traditional stabilizers and flame retardants, simultaneously being environmentally friendly and may be superior in many aspects. The important requirement focused on is: how to increase thermal stability and flame retardancy of flexible poly(vinyl chloride). Due to the typical materials now used with poly(vinyl chloride), which increases health and environmental concerns, utilizing a novel heavy metal-free additive will make poly(vinyl chloride) substantially safer. We have used an artificial silicate for this aim, which proved to be an efficient flame retardant and surprisingly showed excellent heat stabilizing effect. Thermal stabi
... Show MoreTitanium dioxide nanorods have been prepared by sol-gel template
method. The structural and surface morphology of the TiO2 nanorods was
investigated by X-ray diffraction (XRD) and atomic force microscopy
(AFM), it was found that the nanorods produced were anatase TiO2 phase.
The photocatalytic activity of the TiO2 nanorods was evaluated by the
photo degradation of methyl orange (MO). The relatively higher
degradation efficiency for MO (D%=78.2) was obtained after 6h of exposed
to UV irradiation.