Background: Nowadays there is an increasing of the emphasis on aesthetic, dentist have been concerned about providing aesthetics and functional removable partial dentures to their patients and this was make the mission more difficult because of the goal now is achieving optimal aesthetic of the denture - while maintaining retentive, stable, and conservative to the health of supporting tooth and supporting tissue. The traditional use of metal clasp like cobalt-chromium, gold, stainless-steel and titanium hampers esthetics because of its obvious display conflicts with patient’s prosthetic confidentiality. Acetal resin (poly oxy methylene) may be used as alternative denture clasp material. This material was promoted primarily on the basis of its superior esthetic. Material and method: In this study, Acetal resin of Flexite and co-cr alloy of Wirocast companies were used. Four metal models of two premolars and two molars were surveyed to have 0.25mm and 0.5mm undercut depth for each one of the materials. eighty clasps were prepared and tested by testing machine to measure the load required to dislodge Acetal and co-cr clasps of 2mm. thickness (for premolar and molar). Tensile test were utilized for both Acetal resin and co-cr. tensile values will be used in special formula to calculate the amount of deflection. Results: The results of this study revealed that Acetal resin clasp of molar with 0.5mm undercut depth have the higher retentive force, and premolar with 0.25 mm undercut depth have the lowest retentive force as compared to co-cr. Also Acetal had lower values of the tensile strength as compared to co-cr alloy but it had higher deflection value than co-cr and it can withstand higher deflections than those of co-cr before having permanent deformation or fracture Conclusions: Acetal resin can be used with limitation as an alternative to co-cr alloy clasps in removable partial dentures.
This research includes a study of dezincification by corrosion from brass alloys in three types of media, which are acidic solution, basic and slat solution in different percentages. The study show the higher dezincification occurs in basic solution which decrease the fatigue properties where the fatigue properties are inversely proportional with dezincification.
SIFCON is characterized as a construction material of high ductility and very high strength. It is suitable for concrete structures used for special applications. However, the density of SIFCON is much higher than that of Fiber Reinforced Concrete (FRC) due to the need for a large amount of high-density steel fibers. This work examines the split tensile behavior of modified weight slurry infiltrated fiber concrete utilizing a mixture of two types of fibers, steel fiber, and polyolefin fiber. For the investigation, 30 cylinders and 15 cubes were poured. The used volume fraction (V.F) is (6 %) and the use of five series once as each type separately and once a hybrid in proportions of 2/3 polyolefin with 1/3 steel fiber and
... Show MoreThe improvement of the mechanical soil characteristics of jet grouting technique is very attractive. The jet grouted soil cement columns in soft is a complicated issue because it depends on a number of factors such as, soil nature, mixture, influence among soil and grouting materials, jetting force of nozzle, jet grouting and water flow rate, rotation and lifting speed. This paper discusses the estimation of shear strength parameters of soil-cement column (soilcrete) in soft clayey soil based on the relationships between the unconfined compressive and split tensile strength for the soilcrete and the effect of the jet grouting and water pressure in the values of cohesion and internal f
The aim of present work is to improve mechanical and fatigue properties for Aluminum alloy7049 by using Nano composites technique. The ZrO2 with an average grain diameter of 30-40 nm, was selected as Nano particles, to reinforce Aluminum alloy7049 with different percentage as, 2, 4, 6 and 7 %. The Stir casting method was used to fabricate the Nano composites materials due to economical route for improvement and processing of metal matrix composites. The experimental results were shown that the adding of zirconium oxide (ZrO2) as reinforced material leads to improve mechanical properties. The best percentage of improvement of mechanical properties of 7049 AA was with 4% wt. of ZrO2 about (7.76% ) for ultim
... Show MoreThis study uses an Artificial Neural Network (ANN) to examine the constitutive relationships of the Glass Fiber Reinforced Polymer (GFRP) residual tensile strength at elevated temperatures. The objective is to develop an effective model and establish fire performance criteria for concrete structures in fire scenarios. Multilayer networks that employ reactive error distribution approaches can determine the residual tensile strength of GFRP using six input parameters, in contrast to previous mathematical models that utilized one or two inputs while disregarding the others. Multilayered networks employing reactive error distribution technology assign weights to each variable influencing the residual tensile strength of GFRP. Temperatur
... Show MoreA theoretical study was done in this work for Fatigue , Fatigue Crack Growth (FCG) and stress factor intensity range for steel . It also includes Generalized Paris Equation and the fulfillment of his equation which promises that there is a relation between parameters C and n . Usig Simple Paris Equation through which we concluded the practical values of C and n and compared them with the theoretical values which have been concluded by Generalized Paris Equation . The value of da/dN and ∆K for every material and sample were concluded and compared with the data which was used in
... Show MoreTensile strength is a critical property of Hot Mix Asphalt (HMA) pavements and is closely related to distresses such as fatigue cracking. This study aims to evaluate methods for assessing fatigue cracking in Asphalt Concrete (AC) mixes. In order to achieve optimum density at different binder contents, the mixes were compressed using a gyratory compactor. Tensile strength was assessed using the Indirect Tensile (IDT) and Semi-Circular Bend (SCB) tests. The results showed that the tensile strength measured by the SCB test was consistently higher than that measured by the IDT test at 25 °C. In addition, the SCB test showed a stronger correlation between increasing binder content and tensile strength. For binder contents ranging from 4
... Show MoreAA3003-H14 aluminum alloy plates were welded by friction stir welding and TIG welding.
Fatigue properties of the welded joints were evaluated based on the superior tensile properties for
FSW at 1500 rpm rotational speed and 80 mm/min welding speed. However, there is not much
information available on effect of welding parameters with evolution of fatigue life of friction stir
welds. The present study experimentally analyzed fatigue properties for base, FSW, and TIG welds
of AA 3003-H14 aluminum alloy. Fatigue properties of FSW joints were slightly lower than the
base metal and higher than TIG welding.
The compressive residual stresses generated by shot peening, is increased in a direct proportional way with shot peening time (SPT). For each metal, there is an optimum shot peening time (O.S.T) which gives the optimum fatigue life. This paper experimentally studied to optimize shot peening time of aluminium alloy 6061-T651 as well as using of and analysis of variance (ANOVA).
Two types of fatigue test specimens’ configuration were used, one without notch (smooth) and the other with a notch radius (1,25mm), each type was shot peened at different time. The (O.S.T) was experimentally estimated to be 8 minutes reaching the surface stresses at maximum peak of -184.94 MPa.
A response surface methodology (RSM) is presen