Background: tooth debonding was one of the major reasons for denture repair. With the use of recently introduced thermoplastic denture base materials the problem of tooth debonding increased due to the nature of the bond between these materials and the acrylic teeth. This study was aimed to assess the bond of the acrylic teeth to conventional heat cure acrylic resin and to thermoplastic resin denture base material and methods to enhance it. Materials and methods: acrylic resin teeth were bonded to heat cure acrylic resin with and without wetting the ridge laps of the teeth with monomer and acrylic teeth with prefabricated retentive holes, unmodified and modified, in their ridge laps were processed with Valplast thermoplastic resin denture base material. The samples were subjected to tensile forces till failure. Results: In general the chemical bond strength of acrylic teeth and heat cure acrylic resin was greater than the mechanical bond strength of the teeth with the Valplast thermoplastic denture base material. Wetting the acrylic resin teeth with monomer enhanced the bond strength with heat cure acrylic resin by 88%. Modifying the prefabricated retentive means of the acrylic resin teeth enhanced the bond strength with the Valplast thermoplastic resin denture base material by 58% Conclusion: wetting the ridge laps of the teeth can increase the bond strength of acrylic teeth and the conventional heat cure resin. A partial solution for the debonding of teeth from Valplast thermoplastic resin dentures is by modifying the prefabricated retentive means for the acrylic teeth to increase the bond strength.
Background: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreBackground: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile b
... Show MoreBackground: Acrylic resin polymer s used in prosthodontic treatment as a denture base material for several decades. Separation and debonding of artificial teeth from denture bases present a laboratory and clinical problem affect patient and dentist. The aim of this study is to evaluate the effect of oxygen plasma and argon plasma treatment of acrylic teeth and thermocycling on bonding strength to hot cured acrylic resin denture base material. Materials and Methods: Sixty denture teeth (right maxillary central incisor) are selected. The denture teeth are waxed onto the beveled surface of rectangular wax block according to Japanese standard for artificial teeth. The control group consisted of 20 denture teeth specimen without any treatment.
... Show MoreBackground: The combination of thermoplastic nylon resin materials and auto polymerizing resin is necessary in some situation for repair and adjustment. This study evaluated shear bond strength between thermoplastic nylon material (flexible) and auto polymerizing acrylic resin subjected to holes and silica coated layer. Materials and Method: Forty five (45) specimens were prepared from flexible acrylic bonded to auto-polymerizing acrylic resin and divided into three groups according to the surface treatments as follows: Group A: 15 specimens of flexible acrylic bonded with cold-cure acrylic by holes. Group B: 15 specimens of flexible acrylic bonded with cold-cure acrylic by silica coated layer. Group C: 15 specimens of flexible acrylic bon
... Show More
This work aims to investigate the tensile and compression strengths of heat- cured acrylic resin denture base material by adding styrene-butadiene (S- B) to polymethyl methacrylate (PMMA). The most well- known issue in prosthodontic practice is fracture of a denture base. All samples were a blend of (90%, 80%) PMMA and (10%, 20%) S- B powder melted in Oxolane (Tetra hydro furan). These samples were chopped down into specimens of dimensions 100x10x2.5mm to carry out the requirements of tensile tests. The compression strength test specimens were shaped into a cylinder with dimensions of 12.7mm in diameter and 20mm in length. The experimental results show a significant increase in both tensile and compression strengths when compared to cont
... Show MoreBackground: Recently, Poly propylene fibers with and without plasma treatment have been used to reinforce heat cure denture base acrylic but, so far some of properties like tensile strength , wettability and wear resistance not evaluated yet, the aim of the study is to clarify the influence of incorporation of treated and untreated fibers on these properties. Materials and methods: Twenty one specimens were fabricated for every tested property(tensile strength, wear resistance and wettability) that classified into three groups(control, untreated poly propylene fibers reinforced specimens and Oxygen plasma treated group)and for each test sevens amples were used(n=7). Tensile strength was tested using Instron universal testing machine, wear
... Show MoreBackground: The geriatric patients wearing removable partial dentures are increasing in proportion. At the same time, the root caries prevalence accompanied by gingival recession is increasing. A variety of vehicles can deliver fluoride into the oral cavity, including fluoride mouth-rinse, fluoride dentifrice, topical fluoride, and fluoride-releasing restorative materials, all of which effectively prevent root caries and suppress recurrent caries. This study aimed to evaluate the effect of sodium fluoride addition on some mechanical properties of heat cure acrylic denture base material. Material and method: A total of 90 samples were prepared in this study, then divided into three main groups according to the type of test used (hardness, te
... Show MoreSoaking dentures with disinfection solutions is an effective way of keeping dentures in a healthy status; however, immersions in these solutions have a negative effect on the bond strength of denture base and denture teeth. The aim of this study was to evaluate the bond strength between denture acrylic teeth and heat-cured Poly (methyl methacrylate) denture base material (with and without nano silica) after disinfection with different chemical disinfectants for a simulated period of six months. One hundred specimens of maxillary central incisors attached to PMMA were divided into two groups; 50 specimens of PMMA without nano silica and 50 specimens of PMMA reinforced with 5 wt% of nano silica. Specimens of each group were immersed in five i
... Show MoreObjective: To evaluate and compare the effect of mechanical surface treatment (groove, aluminum oxide particles)
with 45 degree bevel type of joint on tensile bond strength of acrylic specimens repaired by two curing methods
(microwave and water both).
Methodology: Eighty specimens (80) were prepared from pink heat cure acrylic resin. They were divided into two
main groups (40 specimen repaired by microwave energy and 40 specimens repaired by water bath method).Each
group can be divided into four subgroups of ten according to the surface treatment. The control group A was left
intact, group B received no surface treatment, group C and D received surface treatment by (groove, 50 m aluminum
oxide particles). Specimens