Background: The surface properties of the titanium alloy plays a significant role in the bond of the dental implant with living bone and modification of the implant surface could enhance osseointegration. This study was aimed to investigate the effect of different durations of heat treatment on the surface properties of titanium alloy for dental implants. Materials and methods: Twenty disks of (Ti-6Al-4V) alloy were prepared. The sample was divided into four test groups to study the effect of different duration of heat treatment to the surface topography; surface chemistry, titanium oxide layer thickness, blood contact angle, & blood drop diameter of titanium alloy samples were investigated to evaluate the effect of different durations of heat treatment at a temperature of 750°C. Results: The surface topography, surface chemistry, titanium oxide layer thickness, blood contact angle, & blood drop diameter of titanium alloy samples improved highly significantly as the duration of heat treatment increased. Conclusions: The heat treatment of 750°C for 90 minutes showed the highest improvement in the surface properties which in turn will lead to enhancement in the osseointegration of the dental implant.
The study is about Maxwell , three dimensions of non – Newtonian fluid. Method of th Homotopy applied to analysis mass transfer and heat with thermophoresis effects. (Sc), Impact of therrmophoretic (𝜏), magnetic (M), Biot (γ), radiation (Rd),Schmidt Prandtle (Pr) parameters and ratio parameter(β) on concentration, temperature are offered in the paper.
Background: Alterations in the microhardness and roughness are commonly used to analyze the possible negative effects of bleaching products on restorative materials. This in vitro study evaluated the effect of in-office bleaching (SDI pola office +) on the surface roughness and micro-hardness of four newly developed composite materials (Z350XT –nano-filled, Z250XT-nano-hybrid, Z250-mico-hybrid and Silorane-silorane based). Materials and methods: Eighty circular samples with A3 shading were prepared by using Teflon mold 2mm thickness and 10mm in diameter. 20 samples for each material, 10 samples for base line measurement (surface roughness by using portable profillometer, and micro-hardness by usingDigital Micro Vickers Hardness Test
... Show MoreDespite the broad approbation of additive manufacturing technologies over diverse industries, printed parts’ performance, quality, and related build time are still greatly influenced by printing parameters. These parameters majorly affect mechanical strength, surface finish, dimensional accuracy, and overall production time of the printed part. Customized 3D printing layer thickness, speed, and acceleration are crucial parameters that affect the speedy printing process and final product quality. The current work considers layer thickness in addition to speed and high acceleration values effect on the surface quality, surface roughness and productivity time of 3D printed Polylactic Acid (PLA). The experimental methodology implemented withi
... Show MoreBackground: One effective second-generation triptan for migraine attacks is sumatriptan. Following oral use, it has a 40% restricted bioavailability because of the first-pass metabolism. Aim: To develop the best intranasal Solusomes formula as a substitute that delivers into the brain directly, improving its bioavailability, and removing the first-pass outcome was the aim of this effort. Methodology: We developed solute formulations based on the Box-Behnken design and subsequently produced them via thin-film hydration. The quality by design technique was used to establish a correlation between the formulation parameters (Soluplus® and phosphatidylcholine (PC) concentrations) and signif¬icant quality powers (entrapment efficiency (
... Show MoreAbstract
The toughening of epoxy resins with the addition of organic or inorganic compounds is of great interest nowadays, considering their large scale of applications. In the present work, composites of epoxy are synthesized with kaolin particles having different particle sizes as reinforcement. Composites of epoxy with varying concentration (0 to 40 weight %) of kaolin was prepared by using hand lay method. The variation of mechanical properties such as modulus of elasticity, yield, tensile, and compressive strength with filler content was evaluated. The composite showed improved modulus of elasticity and compressive properties on addition of filler. In contrast, the tensile and yield strength of the composite
... Show More