Background: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive resin. Shear bond strength was measured by using Tinius Olsen universal testing machine. After debonding, each bracket and zirconium surface were examined and adhesive remnant index was registered. The difference in shear bond strength among groups was analyzed by using ANOVA test. The adhesive remnant index was assessed using Chi-square test. Results: The 2nd laser group had the highest mean value of shear bond strength then the 1st laser group followed by the sandblasting group, while the control group had the least value, non-significant difference in the shear bond strength was found between the laser groups and highly significant difference was found between all other comparable groups. Non-significant difference in the site of bond failure was found between the laser groups and sandblasting group, and between the two laser groups. Conclusion: The laser conditioning method showed higher value of shear bond strength than the sandblasting conditioning method.
Apical meristems, lateral buds, anthers of immature flowers and immature embryos of chickpea ( Cicer arietinum L.) were cultured on MS media with different growth regulators and incubated for 6 weeks at 25-27?C with 16 hrs photoperiod for callus initiation. Results indicated that 1 and 0.1 mg/l of 2,4-D and BA were suitable for callus initiation when apical meristems and lateral buds were used. While 2 and 0.5 mg/l of both growth regulators were essential for immature embryos. It was noticed that using chickpea anthers of the MS medium must contain 1mg/l 2ip and 0.5 mg/l IAA. However, MS medium supplemented with 1-3 mg/l of BA and 2,4-D respectively was good for callus initiation from lateral buds, anther and immature embryos.
... Show MoreBackground: Poly (methyl methacrylate) has several disadvantages (poor mechanical properties) like impact and transverse strength. In order to overcome these disadvantages, several methods were used to strengthen the acrylic resin by using different fibers or fillers. This study was conducted to evaluate the effect of Plasma treatment of the fiber on mechanical properties Poly (methyl methacrylate) denture base material. Materials and methods: Specimens were prepared from poly methyl metha acrylic (PMMA) divided according to present of fiber into 4 groups (first group without fiber as control group, second group with Plasma treated polyester fibers, third group with Plasma treated polyamide fibers and fourth group Plasma treated combination
... Show MoreRouting is the process of delivering a packet from a source to a destination in the network using a routing algorithm that tries to create an efficient path. The path should be created with minimum overhead and bandwidth consumption. In literature, routing protocols in VANET were categorized in many ways, according to different aspects. In the present study, we prefer the classification based on the number of hops to reach the destination node. In literature, these are single-hop and multi-hops protocols. We first discuss the two types and then compare the MDDV (multi-hops protocol) with VADD (single-hop protocol). The comparison is theoretically and experimentally implemented by providing a network environment consisting of SUMO, VIENS and
... Show MoreIn this study the simple pullout concrete cylinder specimen reinforced by a single steel bar was analyzed for bond-slip behavior. Three-dimension nonlinear finite element model using ANSYS program was employed to study the behavior of bond between concrete and plain steel reinforcement. The ANSYS model includes eight-noded isoperimetric brick element (SOLID65) to model the concrete cylinder while the steel reinforcing bar was modeled as a truss member (LINK8). Interface element (CONTAC52) was used in this analysis to model the bond between concrete and steel bar. Material nonlinearity due to cracking and/or crushing of concrete, and yielding of the steel reinforcing bar were taken into consideration during the analysis. The accuracy of this
... Show MoreBreak in the bond and its impact on the difference of scholars
In this study the simple pullout concrete cylinder specimen reinforced by a single steel bar was analyzed for bond-slip behavior. Three-dimension nonlinear finite element model using ANSYS program was employed to study the behavior of bond between concrete and plain steel reinforcement. The ANSYS model includes eight-noded isoperimetric brick element (SOLID65) to model the concrete cylinder while the steel reinforcing bar was modeled as a truss member (LINK8). Interface element (CONTAC52) was used in this analysis to model the bond between concrete and steel bar. Material nonlinearity due to cracking and/or crushing of concrete, and yielding of the steel reinforcing bar were taken into consideration during the analysis. The accuracy of t
... Show MoreThe main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and
The main objective of this work was to adopt an environmentally friendly technology with enhanced results. The technology of magnetic water (MW) treatment system can be used in concrete mixture production instead of potable water (PW) to improve both workability and strength. Two types of concrete were adopted: normal concreter production with two grades 25 and 35 MPa and the self-compacted concrete (SCC) with 35 MPa grade. The concrete mixes containing MW instead of PW results showed that, for 25 MPa grade, an improvement in a compressive strength of 15.1, 14.8, and 10.2% was achieved for 7, 28, and 90 days, respectively. For 35 MPa grade, an improvement of 13.6, 11.5, and