ABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the color parameters (Lightness, axis a* of chroma and axis b*of chroma) immediately after cementation, after 150 and 300 hours of aging. The specimens were subjected to artificial accelerated aging in Accelerated Weathering Tester. Color change greater than 3.3 was considered unacceptable. One-way ANOVA, paired t-tests and Bonferroni adjusted t-test were used for statistical analysis (p <0.05). Results: Artificial aging caused high significant color change in both ceramic types, but there were non-significant difference in color change among the three resin cements used. The color change was between1.997-14.8 after 150 hours and it was between 2.179-15.68 after 300 hours. The color change of e.max discs after aging were within acceptable limit<3.3 whereas Vita Enamic specimens had shown unacceptable color change >3.3 after aging. Conclusions: The majority of color change after aging related to veneering materials while resin cement have only slight effect on color change after aging. IPS e.max had shown an acceptable color change after aging, so it is suitable for fabrication of restorations in esthetic zone while Vita Enamic should not be used in esthetic zone since it has poor color stability according to the results of this study.
Background: Dental stone casts come into contact with impression materials and becomes susceptible to cross contamination from saliva and blood. This study was done to evaluate the physical and mechanical properties of dental stone type IV after treatments with various disinfecting agents and regimes (methods). Materials and Methods: Type IV dental stone and different types of disinfecting agents were used and divided into seven groups: G1: dental stone without disinfection (control group), G2: dental stone mixed with silver nitrate powder 0.5% , G3: dental stone mixed with silver nitrate powder 1%, G4: dental stone mixed with copper sulfate powder 0.5%, G5: dental stone mixed with copper sulfate powder 1% ,G6: dental stone immersed in prop
... Show MoreThe field experiment was conducted in garden of Department of Biology, College of Education for Pure Sciences (Ibn- Al-Haitham), University of Baghdad during the season of growth (2014-2015). The experiment aimed to study the effect of citric acid with two concentration 10, 20 mg. L-1 and glutamic acid with two concentration 50, 100 mg. L-1 on growth and yield of broad bean (Vicia faba). The results were showed an increased in plant height, leaves number. Plant dry weight, chlorophyll content flowers number, absolute growth rate, crop growth rate, legume length and dry weight, legumes number, seed dry weight compared with control plants.
The study aimes to investigate the effects of leaves & fruits ethanolic extract of Duranta repens L. on biological performance for all stages of life cycle of the mosquito Culex pipiens piepiens L., For this purpose the mosquitoes were reared in the laboratory till the fourth generation .Different concentrations of leaves (800,1000,1200,1400ppm) and fruits (800,1000,1200ppm) were tested on (eggs,larval stages,pupal stages and the adult stages). The results revealed that the extracts gave highest mortality rate for the eggs at(100%) compared with control,fruits extract shown highest mortality rate of the four larval instars (100%)at 1200ppm compared with leave extract at(80,50,33.33,20%).Also the extract caused a high mortality rate for pupa
... Show MoreThe seedlings of vegetables are exposed to stress states, especially through the first period, due to injuring their roots by transplanting or heavy rain , so it is necessary to provide an available nutrient to recover the growth and increase their early yield, which means more income for farmers. In this regard, an experiment was conducted in the College of Agricultural Engineering Sciences, Agriculture Faculty, University of Baghdad, Iraq to study the effect of different types and concentrations of mineral fertilizers as starter solutions by using high nitrogen (N), high phosphorus (P) and neutral fertilizers (Q) at three levels which were 4 g/l (S1), 8 g/l (S2) and 12 g/l (S3) on broccoli growth and yield. The results showed tha
... Show MoreFiber reinforced polymer composite is an important material for structural application. The diversified application of FRP composite has taken center of attraction for interdisciplinary research. However, improvements on mechanical properties of this class of materials are still under research for different applications. In this paper we have modified the epoxy matrix by Al2O3, SiO2 and TiO2 nano particles in glass fiber/epoxy composite to improve the mechanical and physical properties. The composites are fabricated by hand lay-up method. It is observed that mechanical properties like flexural strength, hardness are more in case of SiO2 modified epoxy composite compare to other nano
... Show MoreSn effect on the phase transformation behavior, microstructure, and micro hardness of equiatomic Ni-Ti shape memory alloy was studied. NiTi and NiTiSn alloys were produced using vacuum induction melting process with alloys composition (50% at. Ni, 50% at.Ti) and (Ni 48% at., Ti 50% at., Sn 2% at.). The characteristics of both alloys were investigated by utilizing Differential Scanning Calorimetry, X- ray Diffraction Analysis, Scanning Electron Microscope, optical microscope and vicker's micro hardness test. The results showed that adding Sn element leads to decrease the phase transformation temperatures evidently. Both alloy samples contain NiTi matrix phase and Ti2Ni secondary phase, but the Ti2Ni phase content dec
... Show MoreThis experiment was performed to investigate the effect of dietary supplementation with flax seed on the egg quality of laying quail. A total of 320 Japanese quail (Coturnix coturnix japonica) wk old were allocated to 4 treatment groups with 4 replicates containing 20 quail each. Birds were fed a commercial diet containing 0% (C), 2% (T1), 4% (T2), or 6% (T3) flax seed. Birds received water and diet ad libitum during the total period of the experiment. Egg quality characteristics were monitored over 3 consecutive 21-day periods. Egg quality criteria involved in this experiment involved egg weight, yolk diameter, yolk height, yolk weight, albumen height, albumen weight, shell weight, shell thickness, Haugh unit, albumen percentage, yolk perc
... Show MoreIn this paper a thin films of selenium was prepare on substrates of n-Si by evaporation in a vacuum technique with thickness about 0.5μm. And then an annealing process was done on samples at two temperature (100 and 200) C ° in a vacuum furnace (10-3 torr).
Some structural, optical and mechanical properties of prepared thin films were measured. Results showed that the prepared film was the crystallization, optical transmittance and micro hardness of the prepared thin films increased significantly after annealing.
Abstract : Silicone elastomer is widely used as the material of choice for fabricating maxillofacial prosthesis. However, silicone properties are far from ideal; low tear strength, low tensile strength and insufficient elasticity are the most undesirable properties. The purpose of this study was to evaluate the effect of addition of nano SiO2filler on tear strength, tensile strength, elongation at break, hardness and color of Cosmesil M-511 HTV maxillofacial silicone elastomer. Nano SiO2was added to the silicone base in concentrations of 4%, 5% and 6% by weight. Silicone with 0% nano filler served as a control. Tear test was done according to ISO 34-1. Tensile and elongation test was done according to ISO 37. Shore A hardness test was done