ABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the color parameters (Lightness, axis a* of chroma and axis b*of chroma) immediately after cementation, after 150 and 300 hours of aging. The specimens were subjected to artificial accelerated aging in Accelerated Weathering Tester. Color change greater than 3.3 was considered unacceptable. One-way ANOVA, paired t-tests and Bonferroni adjusted t-test were used for statistical analysis (p <0.05). Results: Artificial aging caused high significant color change in both ceramic types, but there were non-significant difference in color change among the three resin cements used. The color change was between1.997-14.8 after 150 hours and it was between 2.179-15.68 after 300 hours. The color change of e.max discs after aging were within acceptable limit<3.3 whereas Vita Enamic specimens had shown unacceptable color change >3.3 after aging. Conclusions: The majority of color change after aging related to veneering materials while resin cement have only slight effect on color change after aging. IPS e.max had shown an acceptable color change after aging, so it is suitable for fabrication of restorations in esthetic zone while Vita Enamic should not be used in esthetic zone since it has poor color stability according to the results of this study.
By measuring Adropin, fasting blood glucose (FBG), cholesterol, high-density lipoprotein (HDL), triglycerides (TG), low-density lipoprotein (LDL), and very low-density lipoprotein (VLDL) in the sera of Iraqi patients with MetS and type 2 diabetes mellitus (T2DM), the current study was designed to compare some crucial markers in metabolic syndrome (MetS) sera and diabetic patients (T2DM) with control. Twenty female subjects were divided into three groups: group I=40 with MetS and group II=40 with T2DM, and 40 healthy subjects were employed as a control group. Compared to the control group, Adropin levels in the Mets group and T2DM group decreased significantly (p < 0.05). In contrast, none of the patient groups (MetS and T2DM)
... Show MoreAbstract: The aim of this study is to assess the effectiveness of 940 nm diode laser in comparison to Endoactivator in elimination of smear layer in terms of radicular dentin permeability and ultra-structural changes of root canal walls by SEM evaluation. Twenty-eight single-rooted extracted lower premolars were instrumented up to size X4 (protaper Next, Dentsaply) and divided into two experimental groups according to the irrigation system, G1; activated by EndoActivator and G2; activated by Diode laser 940 nm, CW mode, 1.7 W. Afterward, the roots were made externally impermeable, filled with 2%methylene blue dye, divided horizontally into three segments representing the apical, middle, and coronal thirds then examined under stereo- micr
... Show MoreBackground: one of the complications of power bleaching is surface roughness of enamel which increases the possibility of post bleaching teeth discoloration. The aim of the present study is to evaluate the effect of toothpaste containing nano hydroxyapatite, NovaMin and kin sense fluoride on surface roughness of human tooth enamel after laser bleaching with 35% hydrogen peroxide bleaching gel. Materials and Methods: Twenty human enamel incisors were cleaned and their labial surface polished up to #1200, then categorized into four equal groups; first group kept without bleaching as a control group, while the remaining three experimental groups were bleached with 35% hydrogen peroxide, and each group treated with a restore paste containing o
... Show MoreIn this work, MWCNT in the epoxy can be prepared at room temperature and thickness (1mm) at different concentration of CNTs powder. Optical properties of multi-walled carbon nanotubes (CNTs) reinforced epoxy have been measured in the range of (300-800)nm. The electronic transition in pure epoxy and CNT/epoxy indicated direct allowed transition. Also, it is found that the energy gap of epoxy is 4.1eV and this value decreased within range of (4.1-3.5)eV when the concentration of CNT powder increased from (0.001-0.1)% respectively.
The optical constants which include (the refractive index (n), the extinction coefficient (k), real (ε1) and imaginarily (ε2) part of dielectric constant calculated in the of (300-800)nm at different concent
The problem of the study and its significance:
Due to the increasing pressures of life continually, and constant quest behind materialism necessary and frustrations that confront us daily in general, the greater the emergence of a number of cases of disease organic roots psychological causing them because of severity of a lack of response to conventional treatments (drugs), and this is creating in patients a number of emotional disorders resulting from concern the risk of disease
That is interested psychologists and doctors searchin
... Show MoreTo evaluate the shear bond strength and interfacial morphology of sound and caries-affected dentin (CAD) bonded to two resin-modified glass ionomer cements (RMGICs) after 24 hours and two months of storage in simulated body fluid at 37°C.
Sixty-four permanent human mandibular first molars (32 sound and 32 with occlusal caries, following the International Caries Detection and Assessment System) were selected. Each prepared substrate (sound and CAD) was co
Back ground: This in vitro study was carried out to investigate the effect of post space regions (coronal, middle and apical), Time and the mode of polymerization (dual, self-cured) of the cements used on the bond strength between translucent fiber post and root dentin by using push-out test. Materials and Methods: Forty eight extracted mandibular first premolars (single root) were instrumented with ProTaper Universal system files (for hand use) and obturated with gutta percha for ProTaper and AH26® root canal sealer following the manufacturer instructions, after 24 hours post space was prepared using FRC postec® plus drills no.3 creating 8 mm depth post space. The prepared samples were randomly divided into two main groups (24 samples ea
... Show MoreThe Effect of Chicken Eggshell Extract on Microhardness of Artificially Induced Dental Erosion in Permanent Teeth (In Vitro Study), Shatha A Abbas*, Alhan A Qasim
Background: Sealers should demonstrate adhesive properties to dentin, decreasing the chance of endodontic treatment failure. Increased adhesive properties to dentin may lead to greater strength of the restored tooth, which may provide greater resistance to tooth fracture and clinical longevity of an endodontically treated tooth. The aim of this study was to evaluate the shear bond strength of Bioceramic iRoot SP sealer, AH plus sealer and Apexit plus sealer in absence or presence of smear layer using push out bond strength test. Materials and Methods: Sixty straight single roots of the mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments to achieve tapered canal walls, instrumenta
... Show MoreBackground and objectives: This study aimed at testing the effect of plastic sleeve or barrier, used to cover the guide of the light cure unit to prevent cross-infection, on the shear bond strength and site of bond failure of stainless steel and ceramic orthodontic brackets. Materials and methods: Forty orthodontic brackets; twenty stainless steel and twenty ceramic brackets bonded to forty extracted human maxillary first premolars using light cure adhesive cured with and without the use of a protective plastic barrier on the guide. Comparing the effect of this barrier on the shear bond strength and adhesive remnant index was performed using an independent t-test and Chi-square test. Results: The protective barrier had decreased the shear b
... Show More