Abstract Background: One of the most important methods to replace lost teeth is dental implants. In order to increase the strength of connection of the implant with the jaw bone to provide early loading after placement, implant is coated by different coating materials that achieved that purpose. The aim of this study was to evaluate the influence of coating CP Ti implant with calcium carbonate on the strength of bone-implant interface after two and six weeks of implantation in rabbit femur bone by torque removal test, histological and histomorphometric analysis. Materials and methods: Coating the surface of commercially pure titanium screws with extra pure synthetic calcium carbonate via electrophoretic deposition method (EPD) was done. The surface of disc samples after coating was checked by optical microscopy, X-ray diffraction examination and measurement of coating thickness. Ten male white French rabbits were prepared for implantation. Forty screws were implanted in the femur bone, two implant screws in each femur bone. The first screw is coated with calcium carbonate and compared with the second uncoated screw. Rabbits are divided into two groups according to the healing periods 2 and 6 weeks. By torque removal, the osseointegration is measured. Single screw from each group was used for histological and Histomorphometric analysis. Results: There was significant increased mean torque removal for screws coated with calcium carbonate compared with uncoated screws. Histological examination showed an increase in the growth of bone cells for coated screws, and the histomorphometric analysis showed an increase in new bone formation percent (NBFP). Conclusion: Coating the surface of the CP Ti implant with calcium carbonate via electrophoretic deposition method had great effect in increasing the osseointegration than uncoated surface.
Background: Synthetic hydroxyapatite,(Ca10(PO4)6(OH2) can directly bond to bones without infection and fibrous encapsulation, thus is regarded as bioactive and biocompatible. The aim of the study was the estimation of microarchitecture bone parameters include bone mass (gm/cm2) cortical bone width (mm), thread width (mm), marrow space star volume analysis (V*m) and osteoblast, osteocyte cell number. Materials and methods: Ninety-six (96) commercially pure titanium CpTi) used in this study, (48) implants were coated with HA by dipping coating and (48) implants were used as control. They were inserted in (32) Newzland white rabbits and followed for 2 & 6 weeks. Mechanical torque removal test and histomorphometric analysis of bone microarchit
... Show MoreIn this research we investigated the corrosion behavior of the commertialy pure titanium and Ti-6Al-4V alloy that coated with hydroxyapatite by electrochemical deposition with applied voltage (6,9,12) Volt from aqueous solution containing Ca(NO3)2.H2O =7.0 gm/l , (NH4)2HPO4 =3.5 gm/l , Na(NO3)2 = 8.5 gm/l in order to improve the bonding strength of hydroxyapetite and medical metals and alloys and increasing the biocompatibility. The coating layer morphology was investigated by XRD, Optical microscope , and SEM tests, the corrosio tests was made by use senthesys simulated body fluid (SBF) , and we found that the propreate voltage for coatint on Ti was 9 Volt and for Ti-6Al-4Vwas12Volt.
Fibroblast growth factor-23, play an important role in atherosclerosis, endothelial dysfunction and vascular calcification. Sevelamer can improve vascular calcification, serum uric acid, low-density lipoprotein-cholesterol and Fibroblast growth factor-23. Aim of study Assessment the effect of sevelamer as phosphate binder against calcium carbonate on Fibroblast growth factor-23. Methods A prospective open-labelled study that included patients on hemodialysis. A total of 72 patients were screened, only 53 patients completed the 10 week period. Adults patients with serum phosphate as> 5.5 mg/dl were included. There were Group1: Includes 28 patients (19 males and 9 females receiving sevelamer carbonate (Renvela) tablet. Group 2: Include 25pati
... Show MoreBackground: Implant stability is considered one of the most important factors affecting healing and successful osseointegration of dental implants. The aims of the study were to measure the implant stability quotient (ISQ) values during the healing period and to determine the factors that affect implant stability. Materials and methods: Thirty patients enrolled in the study (17 female, 13 male). They received 44 Implantium® Dental Implants located as the following: 22 implants in maxillary jaw, 22 implants in mandibular jaw from them 17 implants in anterior segment and 27 in posterior segment. The bone density determined using interactive CT scan and classified according to the Misch bone density classification (29 implants in (D3), 15 i
... Show MoreBackground: Dental implants provide a unique treatment modality for the replacement of lost dentition .This is accomplished by the insertion of relatively inert material (a biomaterial) into the soft and hard tissue of the jaws, there by providing support and retention for dental prostheses. Low level laser therapy (LLLT) is an effective tool used to prompt bone repair and modeling post surgery; this has referred to the biostimulation effect of LLLT. The aims of this study were to evaluate the immmunohistochemical expression of vascular endothelial growth factor (VEGF) and transforming growth factor -beta (TGF-β) in experimental and control groups with mechanical test. Materials and Methods: Thirty two adult New Zealand white rabbits use
... Show MoreDue to the advantages over other metallic materials, such as superior corrosion resistance, excellent biocompatibility, and favorable mechanical properties, titanium, its alloys and related composites, are frequently utilized in biomedical applications, particularly in orthopedics and dentistry. This work focuses on developing novel titanium-titanium diboride (TiB2; ceramic material) composites for dental implants where TiB2 additions were estimated to be 9 wt.%. In a steel mold, Ti-TiB2 composites were fabricated using a powder metallurgy technique and sintered for five hours at 1200 °C. Microstructural and chemical properties were analyzed by energy dispersive X-ray spectroscopy (EDX), scanning electron microscopy (SEM), and X-ra
... Show MoreTitanium alloy (Ti-6Al-4V or Gr.23) was widely used as a dental alloy. In the current study, polymerization of eugenol (PE) on Gr.23 titanium alloys was conducted by an electrochemical process before and after being treated by Micro Arc Oxidation (MAO). The formed films were characterized by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). The corrosion behavior of Gr.23 alloy in an artificial saliva environment at a temperature range of 293–323 K has been studied and assessed by means of electrochemical polarization and impedance spectroscopy techniques. Three cases are taken into consideration; bare Gr.23, Gr.23 coated by PE, and Gr.23 coated by PE after MAO treatment. The maxi
... Show MoreBackground: Dental implant considers a unique treatment option for the replacement of missing dentition. The new trend of implants is looking for materials which accelerate bone formation in bone implant interface and enhance osseointegration to provide immediate loading directly after placement and decrease the time period which is disturbs patients and uncomfortable. The aim of the study was to evaluate the effect of nano zirconium oxide (ZrO2) and nano hydroxyapatite (Hap) mixture coating of screw shaped commercially pure titanium (cpTi) implants on bond strength at the bone implant interface with torque removal test and histological analysis in comparison with non coated implants. Materials and methods: Forty screws were machined from c
... Show More