Abstract Background: One of the most important methods to replace lost teeth is dental implants. In order to increase the strength of connection of the implant with the jaw bone to provide early loading after placement, implant is coated by different coating materials that achieved that purpose. The aim of this study was to evaluate the influence of coating CP Ti implant with calcium carbonate on the strength of bone-implant interface after two and six weeks of implantation in rabbit femur bone by torque removal test, histological and histomorphometric analysis. Materials and methods: Coating the surface of commercially pure titanium screws with extra pure synthetic calcium carbonate via electrophoretic deposition method (EPD) was done. The surface of disc samples after coating was checked by optical microscopy, X-ray diffraction examination and measurement of coating thickness. Ten male white French rabbits were prepared for implantation. Forty screws were implanted in the femur bone, two implant screws in each femur bone. The first screw is coated with calcium carbonate and compared with the second uncoated screw. Rabbits are divided into two groups according to the healing periods 2 and 6 weeks. By torque removal, the osseointegration is measured. Single screw from each group was used for histological and Histomorphometric analysis. Results: There was significant increased mean torque removal for screws coated with calcium carbonate compared with uncoated screws. Histological examination showed an increase in the growth of bone cells for coated screws, and the histomorphometric analysis showed an increase in new bone formation percent (NBFP). Conclusion: Coating the surface of the CP Ti implant with calcium carbonate via electrophoretic deposition method had great effect in increasing the osseointegration than uncoated surface.
Background: This study report the corrosion behavior of commercially pure titanium and Ti-6Al-4V alloy samples without coating and with hydroxyapatite, partial stabilized zirconia and mixture of partial stabilized zirconia and hydroxyapatite coating and comparison between them through electrochemical polarization tests in 37 0 C Hank's solution. Materials and methods: Electrophoretic deposition technique (EPD) was used to achieve the coating from each one of three types of the coating materials (HAP, PSZ and mixture of 50% HAP and 50%PSZ) on Cp Ti and Ti-6Al-4V alloy samples. The electrochemical corrosion test was performed when samples were exposed to Hank's solution prepared in the laboratory and the polarization potential, corrosion rate
... Show MoreIN this work, a titanium dental implant was modified by electro-polymerized of 4-allyl-2-methoxyphenol (Eugenol) using direct current lower than 3.5 volt. The modification of titanium dental implant was achieved to improve its corrosion resistant. Fourier transform infrared spectroscopy (FTIR) was employed to confirm the electro-polymerization of Eugenol to Poly Eugenol (PE) on pure titanium. Deposition of PE on titanium was confirmed by X-ray diffraction and was characterized by thermogravimetric analysis (TGA). The surface morphology of polymeric film were examined through scanning electron microscopy (SEM). Coated titanium by (PE) revealed a good corrosion protection efficiency even at temperature ranged (293-323)K in artificial saliva.
... Show MoreBackground: Dental implants provide a unique treatment modality for the replacement of a lost dentition .This is accomplished by the insertion of relatively an inert material (a biomaterial) into the soft and hard tissue of the jaws, there by providing support and retention for dental prostheses. Low level laser therapy (LLLT) is an effective tool used to prompt bone repair and remodeling, this has referred to the biostimulation effect of LLLT. The Aim of this study was to evaluate the effects of inflammatory cells on osseointegration of CpTi implant irradiated by low level laser. Materials and Methods: thirty two adult New Zealand white rabbits, received titanium implants were inserted in the tibia. The right side is considered as experime
... Show MoreBackground: Dental implant surface technologies have been evolving rapidly to enhance a more rapid bone formation on their surface and improve implant therapy.Implant threads should be designed to increase surface contact areathat induced better stability. In addition, implant surface coating with Flaxseed was used to enhance bone formation at the bone-implant interface. Materials and methods: Ninety-six commercially pure titanium (CpTi) screws were implanted in rabbits' tibiae and divided into three groups as dual-threaded group, flaxseed-coated group and control group. All groups were evaluated mechanically, histologically and radiographically after each healing periods (2, 4, 6 and 8) weeks and the resulting data were statistically analy
... Show MoreAim: To evaluate the wettability and microhardness of Zirconium (ZrO2) dental material when coated with different concentrations of Faujasite. Materials and methods: 30 circular disks produced from ZrO2, then each group is classified into 10 control groups, 10 coated groups with 3% Faujasite, and 10 coated groups with 7% faujasite by electro-spun tool to study variable properties in hardness and water contact angle of implant materials. Results: This study stated the high hardness in 7% of faujasite concentration for ZrO2, in addition, the contact angle decreased gradually until reach 0 ᵒ in 7% concentration of faujasite with ZrO2 Conclusion: Water contact angle (WCA) declined till disappeared in (7% wt.) of faujasite coated with the Z
... Show MoreBackground: The insertion torque (IT) values and implant stability quotient (ISQ) values are the measurements most used to assess primary implant stability. This study aimed to assess the relationship between ISQ values and IT. Materials and methods: This study included 24 patients with a mean (SD) age of 47.9 (13.64) years (range 25-75 years). The patients received 42 dental implants (DI), 33 in the mandible and 9 in the maxilla. The DI were installed using the motorized method with 35 Ncm torque, When DI could not be inserted to the requisite depth by the motorized method, a hand ratchet was used and the IT was recorded as ˃ 35 Ncm. Implant stability was measured utilizing Osstell® ISQ. The secondary stability was measured after 16
... Show MoreBackground: Platelet-rich fibrin (PRF) is a simple, low cost and minimally invasive way to obtain a natural concentration of autologous growth factors and is currently being widely experimented in different fields of medicine for its ability to aid the regeneration of tissue with a low healing potential. Fields of application are sports medicine, orthopedics, dentistry, dermatology, ophthalmology, plastic and maxillofacial surgery, etc. The rationale for using platelets in so many fields for the treatment of different tissues is because PLTs constitute a reservoir of critical GFs and cytokines, which may govern and regulate the tissue healing process that is quite similar in all kinds of tissues. Materials and Methods: Screw titanium implan
... Show MoreBackground:In this study,TiO2 layer was thermally grown as a diffusion barrier on CP Ti substrate prior to electrophoretic deposition of HA coatings, to improve the coating’s compatibility also macro and micro pores in nano Hydroxyapatite dual coatings were created and their effect on the bond strength between the bone and implant was evaluated. Materials and methods: Electrophoretic Deposition technique (EPD) was used to obtain coatings for each one of four types of Hydroxyapatite(HA)on CP Ti screws (micro HA, nano HA, dual nano HA with micro pores, dual nano HA with macro pores) where carbon particles used as fugitive material to be removed by thermal treatment to create porosity.For examination of the changes occurred on the subs
... Show MoreObjective: Evaluation of the poly ether keton keton polymer (PEKK) coating material on the commercial pure titanium disks (CP Ti) with or without laser surface structuring. Design: In vitro experimental study of PEKK polymer coated material on the CP Ti disks with or without laser surface structuring. Materials and methods: coating the surface of the commercial pure titanium (CP Ti) disks with PEKK polymer was performed via using frictional mode CO2 laser, then the samples disks analyzed by using FESEM. Results: the FESEM reveal good adherence and distribution of the PEKK coated material over the CP Ti substrate by using the frictional mode CO2 laser at 2 watt and 6 ms pulse duration. Conclusion: the frictional mode CO2 laser considered an
... Show MoreAim: To evaluate the commercial pure titanium disks that structuring by laser in two design (dot and groove) each one with three different laser scan (5, 15 and 25) and comparing with titanium surface that not subjected to any surface structuring (control) through measuring the wettability test and surface roughness test. Materials and methods: Structuring on the surface of the commercial pure titanium (CP Ti) disks was performed via using fiber laser CNC machine in two design (dot and groove) in three different laser scans (5, 15 and 25), then the structuring disks analyzed with the control group by atomic force microscope and water contact angle test. Results: The results of this study showed that the surface roughness and the wettability
... Show More