Background: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three groups (n = 10) according to the debond times: I: debond after 24 hour, II: debond after 7 days and III: debond after 30 days. Within 24 hr, half of the sample was thermocycled manually for 500 complete cycles between 5/55°C and the remaining sample was stored in distilled water at room temperature and water was changed daily until debond time for each group was performed. The adhesive remnant index was tested under 20X magnification lens using stereomicroscope. Results and Conclusions: Both bracket types demonstrated high shear bond strength values before thermocycling (P?0.05), whereas after 500 thermocycles, there were significant changes in shear bond strength resulted in marked reduction in the stainless steel brackets than in the sapphire brackets (P?0.05). Shear bond strength values increased with time for both stainless steel and sapphire brackets with and without thermocycling (P?0.05). The tendency of bond failure was increased at the bracket/adhesive interface rather than enamel/bracket interface in the stainless steel brackets whereas at the enamel/bracket interface rather than bracket/adhesive interface in the sapphire brackets.
Hypertension is one of the main causes of heart disease; beta- blockers play a crucial role in the management of patients with essential hypertension. Bisoprolol is one of the widely used drugs for the treatment of hypertension. Bisoprolol tablets were prepared by two methods (direct and wet) using different proportion and types of diluents, different binder types and forms, then evaluated for, weight variation, hardness, friability, disintegration time and dissolution rate. The results were compared with a reference Bisoprolol tablet.
Both methods of preparation wet and direct compression method gave good results, which are consistent with the requirements of British Pharmacopeia and United States Pharmacopeia. It was found that
... Show MoreBackground: The ideal force-delivery system must: provide optimal tooth moving forces that elicit the desired effects, be comfortable and hygienic for the patient, require minimal operator manipulation and patient cooperation and provide rapid tooth movement with minimal mobility during orthodontic therapy, the elastomeric chains have the greatest potential to fulfill these requirements. Materials and Methods: This in vitro study was designed to determine the effect of three different mechanisms for canine retraction : (6-3 , 6-5-3 and chain loop ) on the load relaxation behavior of three types of elastomeric chains : (maximum clear , maximum silver and extreme silver) from the same company (Ortho Technology company) with two different bran
... Show MoreBackground: Orthodontic force is considered to stimulate cells in the periodontium to release many mediators such as cytokines which play a responsible role for periodontal and alveolar bone remodeling, bone resorption and new bone deposition. Aim of this study was carried out to estimate changes of the (interleukin-one beta, tumor necrosis factor – alpha and C-reactive protein) levels in unstimulated whole saliva during the leveling stage of orthodontic tooth movement. Materials and methods: The sample consisted of thirty adult patients (12 males and 18 females) with ages ranges (19-23) years. Each sample had Class I and Class II malocclusion dental classification and required bilateral extraction of their maxillary first premolars, und
... Show MoreThe advancement of cement alternatives in the construction materials industry is fundamental to sustainable development. Geopolymer is the optimal substitute for ordinary Portland cement, which produces 80% less CO2 emissions than ordinary Portland cement. Metakaolin was used as one of the raw materials in the geopolymerization process. This research examines the influence of three different percentages of sulfate (0.00038, 1.532, and 16.24) % in sand per molarity of NaOH on the compressive strength of metakaolin-based geopolymer mortar (MK-GPM). Samples were prepared with two different molarities (8M and 12M) and cured at room temperature. The best compressive strength value (56.98MPa) was recorded with 12M w
... Show MoreThe relation between the output power and wavelengths for a 532nm 3W frequency doubled diode pumped solid state laser pumped Ti:Sapphire crystal is investigated. A 20 femtosecond pulse at 800 nm is obtained. A 320 mW is found to be the highest power at 800nm. Below this wavelength value and above the power was found to deviate from highest output value.
Background: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H O
... Show MoreThe present study aims to investigate the long-term histopathological, and physiological effects of different concentrations of a commercially available energy drink (Tiger) on liver and kidney of young mice. Sixteen Balb/c male mice,6 -week old, were divided into 4 groups (n=4). Two groups consumed the energy drink at a concentration of 28µl energy drink/ml water. One group were killed after 10 days (T1), another group were killed after 20 days (T2). Other group of mice consumed the energy drink at a final concentration of 14µl/ml for 20 days (T3). The last group was provided only with water and served as control. Mice of all groups drank around 3 ml per day. The histopathological study on liver of treated groups showed many changes s
... Show More