Background: The aim of this study was to evaluate the push-out bond strength of four different obturation materials to intraradicular dentin and to determine the failure mode. Materials and method: forty straight palatal roots of the maxillary first molars teeth were used in this study, the roots were instrumented using crown down technique and rotary EndoSequence system, the roots were randomly divided into four groups according to the materials used for obturation (n=10).Group (1): AH Plus sealer and gutta-percha. Group (2): Activ GP glass ionomer sealer and Activ GP gutta-percha (Activ GP system). Group (3): Bioceramic sealer and Bioceramic gutta-percha. Group (4): GuttaFlow2 sealer and gutta-percha. For all groups single cone obturation technique was used. After incubation period of one week, the roots were embedded in clear acrylic resin and each root sectioned into three levels apical, middle and cervical. The bond strength was measured using computerized universal testing machine, each section fixed in the machine so that the load applied from apical to coronal direction at 0.5mm/min speed and the computer drew curve to show the higher bond force before dislodgment of the filling material. After de-bonding each sample was examined under Stereomicroscopic and the type of failure mode was recorded. Results: showed a non significant difference between AH plus group and Bioceramic group. AH Plus group showed a very highly significant difference with Activ GP group and a highly significant difference with GuttaFlow2 group. There were significant differences between coronal level and both apical and middle levels with no significant differences between apical and middle levels within each group. Conclusion: AH plus group showed the highest mean of bond strength in comparing to other tested groups
Background: The aim of this study was to evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic adhesive systems after exposure to aging media (water storage and acid challenge). Materials and methods: Eighty human upper premolar teeth were extracted for orthodontic purposes and randomly divided into two groups (40 teeth each): the first group in which the bonded teeth were stored in distilled water for 30 days at 37°C, and the second group in which the bonded teeth were subjected to acid challenge. Each group was further subdivided into four subgroups (10 teeth each) according to the type of adhesive system that would be bonded to metal brackets: either non-fluoride releasing adhesive (NFRA),
... Show MoreSteel-concrete-steel (SCS) structural element solutions are rising due to their advantages over conventional reinforced concrete in terms of cost and strength. The impact of SCS sections with various core materials on the structural performance of composites has not yet been fully explored experimentally, and in this work, both slag and polypropylene fibers were incorporated in producing eco-friendly steel-concrete-steel composite sections. This study examined the ductility, ultimate strength, failure modes, and energy absorption capacities of steel-concrete-steel filled with eco-friendly concrete, enhanced by polypropylene fiber (PPF) to understand its impact on modern structural projects. Eco-friendly concrete was produced by the partial
... Show MoreObjectives: This study aims to assess and compare the micro-shear bond strength (μSBS) of a novel resin-modified glass-ionomer luting cement functionalized with a methacrylate co-monomer containing a phosphoric acid group, 30 wt% 2-(methacryloxy) ethyl phosphate (2-MEP), with different substrates (dentin, enamel, zirconia, and base metal alloy). This assessment is conducted in comparison with conventional resin-modified glass ionomer cement and self-adhesive resin cement. Materials and methods: In this in vitro study, ninety-six specimens were prepared and categorized into four groups: enamel (A), dentin (B), zirconia (C), and base metal alloys (D). Enamel (E) and dentin (D) specimens were obtained from 30 human maxillary first premolars e
... Show MoreBackground: The purpose of this study was to compare regional bond strength at middle and cervical thirds of the root canal among glass fiber-reinforced composite (FRC) endodontic posts cemented with different cements, using the push-out test to compare the performance (retention) of two types of luting cements; polycarboxylate cement and Zinc phosphate cement used to cement translucent fiber post and to compare the result of the push-out test at different storage times;1 week ,1month and 2 months. Materials and methods: Ninety caries-free, recently extracted single-rooted human teeth with straight root canals was used in this study, The root canals were endodontically instrumented at a working length of 0.5 mm from the apex by m
... Show MoreBackground: Antibacterial action of root canal filling is an important factor for successful root canal treatment, so the aim of the study was to identify and to compare the antimicrobial effect of new sealer (GuttaFlow) to commonly used endodontic sealers (AH Plus, Apexit and EndoFill) against four endodontic microbes. Materials and methods: Twenty patients aged (30-40) years with infected root canals were selected. Four types of microorganisms were isolated from root canals (E faecalis, Staphylococcus aureus, E coli and Candida albicans) and cultured on Mueller Hinton agar Petri-dishes. After identification and isolation of bacterial species, agar diffusion method was used to assess the antibacterial action of four contemporary endodontic
... Show MoreThrough an experimental program of eighteen specimens presented in this paper, the bond strength between reinforcing bar and rubberized concrete was produced by adding waste tire rubber instead of natural aggregate. The fine and coarse aggregate was replaced in 0%, 25%, and 50% with the small pieces of a waste tire. Natural aggregate replacement ratio, rebar size, embedded rebar length, the rebar yield stress of rebar, cover, and concrete compressive strength were studied in this investigation. Ultimate bond stress, bond stress-slip response, and failure modes were presented. The experimental results reported that a reduction of 19% in bond strength was noticed in 50% replaced rubberized concrete compared with convention
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreBackground: Common and persistent isolate ina the teeth following failed therapy of the root canal is the gram-positive facultative bacterium Enterococcus faecalis and Escherichia coli, which develop biofilm through a complicated process that results in the formation of a biofilm. Enterococcus faecalis and Escherichia coli are significant factors that cause chronic periradicular lesions after root canal therapy. Aim: This study aimed to treat the root canal tooth infected with Escherichia coli and Enterococcus faecalis Methods: In this study biofilm formation was done for Escherichia coli in growth phase cultured in a brain heart broth Enterococcus faecalis and Escherichia coli cultured in Luria-Bertani (LB) infusion medium for 18 hrs. Then
... Show MoreBackground: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surfa
... Show More