This research has studied the effect of addition glass fibers (woven and chopped)
and Zirconium oxide Nano-particles (ZrO2) with different weight percent to the
conventional poly (methyl methacrylate) (PMMA). The prepared Nano-crystalline
ZrO2 powder with particle size of about 95nm was syntheses directly by sol-gel
method. The gel dried at 100oC for 1 hour and annelid at 400oC for 3 hours.
The conventional acrylic resin prepared with 2:1 powder to liquid ratio to prepare
pure sample, composite samples prepared by reinforcing PMMA with woven or
chopped glass fiber (8, 12) wt.%, and reinforcing by (1,2,3) wt.% of prepared ZrO2
Nano-powder.
The structural tests include: (XRD, AFM, and FTIR). The crystallized phase
composition of dried ZrO2 powder after annealing in air at 400oC has been identified
by x-ray diffractometry (XRD). The grain size of dried ZrO2 Nano-particles by
atomic force microscope (AFM).
The impact strength (I.S.) was measured by using Charpy impact test. The
mechanical test done in order to compare the impact strength between pure and
composite samples. From the result, the reinforcing PMMA with glass fiber in two
forms (woven and chopped) improve the impact strength, while increasing of ZrO2
Nano powder loading led to decrease the impact strength.
Background: Poly (methylmethacrylate) is the most widely used material in denture fabrication. The characteristics of acrylic resin which support microorganism development can threaten the oral health of denture users. This study was assigned to prepareand incorporate Ag-Zn zeolite powder into heat cured denture base material as antimicrobial material and to investigate its effect on some properties of heat cured acrylic denture base materials. Materials and methods: Sliver –zinc zeolite was prepared by ion exchange method and characterized then incorporated into poly (methylmethacrylate) powder in0.5% by weight. Specimens were constructed and divided into 6 groups according to the using tests; each group was subdivided into 2 groups
... Show MoreBackground: Polymethyl methacrylate (PMMA) is used in denture fabrication and considered as the most reliable material for the construction of removable prosthodontic appliances. The material is far from ideal in fulfilling the mechanical requirements and the effect of autoclave processing has not been fully determined. The purpose of this study was to evaluate the effect of addition of salinized (ZrO2) Nano fillers in percentages 3%, 5% and 7% by weight on some properties of heat cured acrylic processed the by autoclave and compare it with 0% (control) group . Materials and methods: The silanized(ZrO2) Nano-particles was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.
... Show MoreBackground: The purpose of this study was to verify the influence of post- pressing time of acrylic resin (immediate, 6, 12 and 24 hour) on the dimensional accuracy of denture base whish is a critical factor in the retention and stability of the complete denture that may occur during polymerization shrinkage. Materials and Methods: Forty maxillary stone casts were poured in plastic mold (Columbia Dentoform corp. NEW YORK, type III dental stone (Geastone, Zeus Sri Loc.Tamburine Roccastrada, GR, Italy). The stone casts were randomly assigned into 4 groups of 10 specimens each according to the post-pressing times into (immediate, 6, 12 and 24 h.). Heat cure acrylic resin denture base was constructed according to the previously mentioned pressi
... Show MoreBackground: the aim of this study was to evaluate the effect of different surface acids treatments (37%phospjoric acid, 5%hydrofluoric acid, 1.23 acidulated phosphate fluoride) of feldspathic ceramic VITA 3D MASTER , and the effect of thermocycling on shear bond strength using a ceramic repair kit (ivoclar/vivadent). Material and Methods: sixty Nickel-Chromium metal base plates were prepared(9mm diameter,3mm depth) using lost wax technique, 2mm thick layer of ceramic(VITA 3D MASTER) fused to metal plates, all specimens were embedded in acrylic resin blocks except their examined surfaces and divided into 3 main groups 20 specimens each, Grp A: treatment with 37%phosphoric acid for 2 mins, Grp B: etching with 5% hydrofluoric acid for 2mins,
... Show MoreObjective(s): In the present study, glycerin is used as a substitute for tin-foil and cold mold seal (Alginate mould seal)
in the process of curing heat and cold-cure acrylic resin denture base against stone and plaster.
Methodology: 60 specimens were prepared from heat-cure acrylic resin and cold-cure acrylic resin denture base. The
study includes 12 groups of specimens depending on the type of processing, investment material and type of
separating medium that are used in curing process. Each group of them contains 5 specimens for each test.
Some of physical properties of the processed acrylic denture base that (water sorption and solubility) have been
compared with those processed using tin-foil and tin-foil substitut
Background: The purpose of this study was to evaluate the effect of addition of surface treated silicon dioxide Nano filler (SiO2) on some properties of heat cured acrylic resin denture base material (PMMA). The properties were impact strength, transvers strength, and surface hardness. Materials and methods: In addition to controlled group SiO2 powder was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.120 specimens were constructed and divided into 3 groups according to the test (each group consist of 40 specimens) and each group was subdivided into 4 sub-groups according to the percentage of added SiO2 (finally each subgroup consist of 10 specimens). The tests conducte
... Show MoreBackground: Poly propylene fibers with and without silane treatment have been used to reinforce heat cure denture base acrylic but, some mechanical properties like transverse strength, impact strength, tensile strength, hardness, wear resistance and wettability. Which are related to the clinical use of the prosthesis are not evaluated yet. The aim of the study is to identify the influence of incorporation of treated and untreated fibers on these properties Materials and methods: Eighty four heat cure acrylic specimens were constructed by conventional flasking technique. They were divided into six groups according to the tests and each group was subdivided into two subgroups control and experimental groups (seven samples for each subgroup
... Show MoreThe effects of three different additives formulations namely Lubrizol 21001, HiTEC 8722B and HiTEC 340 on the efficiency of VII namely OCP of three base lubricating oils namely 40 stock and 60 stock and 150 stock at four temperatures 40, 60, 80 and 100oC were investigated. The efficiency of OCP is decreased when blended with 4 and 8 wt% of Lubrizol 21001 for all the three base oil types. But it is increased when adding 4 wt% and 8 wt% of H-8722B in 40 stock. While for 60 stock and 150 stock the OCP efficiency decreased by adding 4 and 8 wt% of H-8722B. In the other hand, it is decreased with a high percentage by adding 4 and 8 wt% of H-340 for 60 stock and 150 stock and for 40 stock it is increased by adding 4 wt% of H-340 and decreased
... Show MoreBackground: The most widely used material for fabrication of denture base is poly methyl methacrylate, despite its popularity, the main problems associated with it as a denture base material are poor strength particularly under fatigue failure inside the patient mouth, impact failure outside the patient mouth, which are the main causes for fracture of denture, several studies was done to increase mechanical properties of denture base. The present study was conducted to evaluate and compare the effect of addition single walled carbon nanotubes in different concentrations to polymethyl methacrylate on some mechanical properties (surface hardness, surface roughness, impact strength and transverse strength). Materials and methods: Forty eight
... Show More