The dielectric properties of the fabricated composites MgO:ZnO with various mixing ratios (100,75:25,50:50,25:75, and 100 wt. %)were investigated. The structure analysis was conducted using X-ray diffraction. The structure phase, crystallite size and purity of the fabricated MgO:ZnO composites were confirmed using X-ray diffraction spectra. The results declared that the diffraction spectrum of 100%MgO composite samples were compatible with cubic structure along the plane (200) while the structures of residual composite's samples were compatible with hexagonal structures. The crystal size of the most pronounced plane (101) for crystal growth was changed from 30.4 nm to 53.2 nm by increasing ZnO ratio from 25 to 100wt%. The dielectric properties were studied as function of frequency over the range (50Hz-10MHz). The a.c conductivity σa.c(ω) showed power low dependence for the full frequency range except for the composites samples of 0 and 75 %wt. ZnO which showed d.c region in the low frequency range. The exponent (s) values which represents the slope of ln σa.c(ω) and ln(ω) changed in non-regular manner by increasing the ZnO ratio. The dielectric constant ε1 and the dielectric loss ε2 increased with the increase of the ZnO ratio up to 75% ZnO and then decreased with further increase of ZnO ratio. The dielectric loss peaks observed in the plot diagram of ε2 against ln(ω) is found to shift towards the high-frequency side which indicates the decrease of relaxation time and prompt movement of charge carriers .The polarizability values (α) estimated from the COLE –COLE diagram increased from 0.112 to 0.467 when the ratio of ZnO changed from 0 to 50wt.% which referred to reduction of the intermolecular forces. While (α) reduced drastically at 75wt.% ZnO which referred to the growing of the intermolecular forces.
Iraqi calcium bentonite was activated via acidification to study its structural and electrical properties. The elemental analysis of treated bentonite was determined by using X-ray fluorescence while the unit crystal structure was studied through X-ray diffraction showing disappearance of some fundamental reflections due to the treatment processes. The surface morphology, on the other hand, was studied thoroughly by Scanning Electron microscopy SEM and Atomic Force Microscope AFM showing some fragments of montmorillonite sheets. Furthermore, the electrical properties of bentonite were studied including: The dielectric permittivity, conductivity, tangent loss factor, and impedance with range of frequency (0.1-1000 KHz) at different temperatu
... Show MoreIn this work, one configuration was used to study the electrical discharge resulting from the dielectric barrier. This configuration consists of a sheet of epoxy/Al composite with dimensions of 75 mm in length, 25 mm in width, and 3 mm in thickness. This panel is located at the center of the electrodes, so that the distance between each of the electrodes and the plate is 2 mm and plasma is generated at these distances. The relationship between voltage and current with changing the frequency of the equipment as well as changing the area of exposure to the upper electrode or changing its length has been studied. The length of the top electrode varies at 0, 10, 20, 30, and 40 mm from the center of the electrodes producing exp
... Show MoreIn this study, aluminum alloyAA6061-T6 was joined by a hot press process with three types of material; polyamide PA 6.6 (nylon), 1% carbon nanotube/PA6.6 and 30% carbon fiber/PA6.6 composites. Three parameters were considered in the hot pressing; temperature (180, 200 and 220°C), pressure (2, 3, 4, 5 and 6 bar) and time of pressing (1, 2, 3, 4 and 5 minutes for 200ºC, and 0.25, 0.5, 0.75, 1 and 1.25 minutes for220ºC). Applied pressure has great effect on shear strength of the joint, corresponding to bonding time and temperature. Maximum shear strength was 8.89MPa obtained for PA6.6 at bonding conditions of 4 bar, 220ºC and 0.75 minute. For 30% carbon fiber/PA6,6 shear recorded was
This research study the effect of surface modification and copper (Cu) plating carbon fiber (CF) surface on the thermal stability and wettability of carbon fiber (CF)/epoxy (EP) composites. The TGA result indicates that the thermal-stability of carbon fiber may be enhanced after Cu coating CF. TGA curve showed that the treatment temperature was enhanced thermal stability of Ep/CF, this is due to the oxidation during heating. The Cu plating increased the thermal conductivity, this increase might be due to reduce in contact resistance at the interface due to chemical modification and copper plating and tunneling resistance.
The increase of surface polarity after coating cause decreas
... Show MoreCopper Phthalocyanine (CuPc) thin film with and without multi-walled carbon nanotubes (MWCNTs) is prepared using the solution based method and used in gas sensor and solar cell applications. The structural characteristics of the CuPc thin films showed a single peak around 7o with the preferred orientation for charge transportation. Using atomic force microscopy (AFM), morphological properties show a rough surface with some aggregates and ribbons. The optical absorption properties were determined using UV-Visible absorption spectroscopy; the optical band gap has varied after adding MWCNTs to CuPc. Electrical conductivity of CuPc:MWCNTs composite is higher than that of the pure CuPc. The CuPc thin film sensr have sh
... Show MoreEffect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.
Hand-lay up method was used to prepare the samples made of epoxy (EP) as a matrix reinforced with chopped carbon fibers (CCF). The fatigue behavior of epoxy resin /chopped carbon fiber composites was studied with different weight percentage of chopped carbon fibers (2.5%,5%,7.5%,10%,12.5%). The fatigue test was carried out under alternate bending method, which was made by applying sinusoidal wave with constant displacement (15mm), stress ratio R=-1,and loading frequency 10Hz, which is believed to give a negligible temperature rise during the test. The results of the maximum stress, fatigue strength, fatigue limit and fatigue life of the tested composites are calculated from stress(S)-number of cycles(N) (S-N) curves.
It was shown that