This research includes using epoxy resin and polyurethane resin to form a blend (EP+PU) with different resin ratios (90 – 10)%, (80 – 20)%, (70 – 30)%, and (60 – 40)% to achieve best ratio for impact strength as a function of better toughness; then reinforced with micro and nano (CdO) with weight fraction (0.02, 0.04, 0.06, 0.08). Mechanical properties were studied including hardness before and after exposure to UV irradiation. Results showed that the composite (nano CdO+ blend) had better properties compared with (micro CdO+ blend) composite. Also hardness show increases with increasing the weight fraction for all samples.
Many faces are exposed to degradation, discoloration, changes in humidity. The primary objective has improved some properties of hybrid nanocomposites materials that used for restoring of the function maxillofacial prosthesis and improving the esthetic. In the present research different lengths chopped and continuous of ultrahigh molecular weight polyethylene (UHMWPE) fiber was added at selected percentage (0.0, 0.2% and 1%) to polymer blend composite (95%SR /5%PMMA: 0.2% Pomegranate Peels Powder (PPP)) for developing the properties of silicone rubber used for the maxillofacial prosthesis applications. Some mechanical and physical properties were done on the all prepared samples. The results showed that all properties have improved when add
... Show MoreCdS Nps (inorganic material) was prepared by the chemical reaction method. ZnPc (organic material) and CdS thin films were prepared separately to compare their characterization with the hybrid BHJ blend ZnPc/CdS thin film (2ml:2ml) by spin coating technique. The structural and morphological properties of the prepared thin films have been measured by XRD and AFM respectively. The XRD pattern for both as-deposited and annealed CdS nanoparticle films shows a hexagonal structure. The crystallite size behavior of as deposited ZnPc films and annealing at 423K for 1h, 2h and 3h was approximately similar to the behavior of heat treated blended films. The grain size was measured by AFM, which decreaseds with annealing temperature for ZnPc films,
... Show MoreThis paper studies the effect of the solar indices (total sunspot no., solar wind density and coronal mass ejection linear speed) on F2- layer electron density, as well as, the comparison of seasonal variations of electron density of F2- layer, NmF2, for Mars at local noontime and for maximum and minimum solar cycles.
Results show that there is an inverse correlation between sunspot number, solar wind density, CME linear speed and ionosphere electron density for Mars, at maximum and minimum solar cycles. This correlation is clear when electron density is at minimum value.
... Show MoreIn the present work the Buildup factor for gamma rays were studied in shields from epoxy reinforced by lead powder and by aluminum powder, for NaI(Tl) scintillation detector size ( ×? ), using two radioactive sources (Co-60 and Cs-137). The shields which are used (epoxy reinforced by lead powder with concentration (10-60)% and epoxy reinforced by aluminum powder with concentration (10-50)% by thick (6mm) and epoxy reinforced by lead powder with concentration (50%) with thick (2,4,6,8,10)mm. The experimental results show that: The linear absorption factor and Buildup factor increase with increase the concentration for the powders which used in reinforcement and high for aluminum powder than the lead powder and decrease with inc
... Show MoreBackground: The purpose of this study was to evaluate the effect of addition of surface treated silicon dioxide Nano filler (SiO2) on some properties of heat cured acrylic resin denture base material (PMMA). The properties were impact strength, transvers strength, and surface hardness. Materials and methods: In addition to controlled group SiO2 powder was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.120 specimens were constructed and divided into 3 groups according to the test (each group consist of 40 specimens) and each group was subdivided into 4 sub-groups according to the percentage of added SiO2 (finally each subgroup consist of 10 specimens). The tests conducte
... Show MoreIn the recent years, the work in composite industry needed new ecofriendly resources to improve the original properties of current materials. Many researches attempted to find alternative additives to be used with the current systems which provide a new material that is environmentally friendly and has better performance than the synthetic counterparts. This paper presents the study of mechanical characteristics, including bending, impact, tensile and hardness tests, of date palm fiber (DPF)/ epoxy composite. The composite plate was constructed by hand-layup technique. The filler content values (wt %) were 5%, 10%, 15% and 20%. Young's modulus, impact strength and hardness were shown to be increased with increasing fiber content. Tensile
... Show MoreThis research is devoted to study the effect of different in weight percentage of Sio2 particles and glass fibers (5, 10, 15, 20) wt. % on the wear rate epoxy resin. The results show that the value of hardness increase with the increase for the weight percentage of reinforcing particles and fibers, while the wear rate decrease with the increase the load level of the reinforcing particles and fibers . The largest value of the hardness, and the lowest value of the wear rate for epoxy reinforced with 20% of SiO2, the wear rate increase in general with increasing the applied load.
Background: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.
Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.
Results: The artificially aged retainers showed a marginally
... Show MoreThe study aimed to determine the impact of energy for the north and south magnetic poles on the the growth of bacteria isolated from cases of tooth decay, 68 swabs were collected from surfaces of faulty tooth, the detected of Staphylococcus aureus
... Show More