Lead-free ferroelectric nano ceramics of BaZrxTi1-xO3 (x=0.1, 0.2 and 0.3) were prepared by means of microwave assisted chemical route. The structural, dielectric and electrical properties were examined. The crystalline structure of the specimens was studied by X-ray diffraction patterns. All the samples showed pure single phase of perovskite structure with space group of I4/mcm. X-ray diffraction data illustrated that there is no secondary phases exist. Structural and electrical properties of barium titanate ceramics are influenced significantly by small additions of Zr. The electrical conductivity showed higher values at x=0.2 and decreased at higher Zr content. The Hall charge mobility is found to decrease with Zr addition. The negative sign of the
Hall coefficient RH confirms the dominant n-type conduction in all samples. The charge carrier concentration decreased with Zr content increase. Suggested potential application for this ceramics compound is in high storage multilayer capacitors and ferroelectric applications.
Thin films of tin disulphide SnS2 with different thicknesses (2500,4000,5000)A0 have been prepared by chemical spray pyrolises technique on substrate of glass with temperature (603)K . The effect of thickness on the optical properties of SnS2 has been studied.the optical study that includes the absorptance and transmittance spectra in the wavelength range (300900)nm demonstrated that the value of absorption coefficient (α) ) was greater than (104 cm-1) the electronic transitions at the fundamental absorption edge were of the indirect kind whether allowed and forbidden . Absorption edge shift slightly towards higher wave length.The value of energy gaps (Eg) for all the films prepared are decreased with inc
... Show MoreThin films of BhSe3 have being deposited on glass substrates of
about 80 - 172 ± 14 nm thickness from an aqueous solution bath at temperature 293 K for period 0.5 to 6.0 hours using alchemical bath deposition method .
The films are characterized by X-ray diffraction, X-ray
florescent techniques and optical transmittance spectra measurements in the rang 350 - 400 nm at 293 K. And shows that as deposited films are amorphous and a transition to polycrystalline state has taken place after annealing them at 373 K, for 30 minutes, But they will be dan1aged
... Show MoreThin films of highly pure (99.999%) Tellurium was prepared by high vacuum technique (5*10-5torr), on glass substrates .Thin films have thickness 0.6m was evaporated by thermal evaporation technique. The film deposited was annealed for one hour in vacuum of (5*10-4torr) at 373 and 423 K. Structural and electrical properties of the films are studies. The x-ray diffraction of the film represents a poly-crystalline nature in room temperature and annealed film but all films having different grain sizes. The d.c. electrical properties have been studied at low and at relatively high temperatures and show that the conductivity decreases with increasing temperature at all range of temperature. Two types of conduction mechanisms were found to d
... Show MoreSamarium ions (Sm +3), a rare-earth element, have a significant optical emission within the visible spectrum. PMMA samples, mixed with different ratios of SmCl3.6H2O, were prepared via the casting method. The composite was tested using UV-visible, photoluminescence and thermogravimetric analysis (TGA). The FTIR spectrometry of PMMA samples showed some changes, including variation in band intensity, location, and width. Mixed with samarium decreases the intensity of the CO and CH2 stretching bands and band position. A new band appeared corresponding to ionic bonds between samarium cations with negative branches in the polymer. These variations indicate complex links between the Sm +3 ion and oxygen in the ether group. The optical absorption
... Show MoreAt a temperature of 300 K, a prepared thin film of Ag doped with different ratios of CdO (0.1, 0.3, 0.5) % were observed using pulse laser deposition (PLD). The laser, an Nd:YAG in ?=1064 nm, used a pulse, constant energy of 600 mJ ,with a repetition rate of 6 Hz and 400 pulses. The effect of CdO on the structural and optical properties of these films was studied. The structural tests showed that these films are of a polycrystalline structure with a preferred orientation in the (002) direction for Ag. The grain size is positively correlated with the concentration of CdO. The optical properties of the Ag :CdO thin film we observed included transmittance, absorption coefficient, and the energy gap in the wavelength range of 300-1100
... Show Moreواحدة من أكثر مواد السيراميك الهيكلية الواعدة هي كربيد السيليكون(SiC) ، حيث له خصائص حرارية وكهروميكانيكية ممتازة. هذه الخصائص مفيدة ل CMC لتعزيز أداء المركب خاصة عند إضافات النانو المتكاملة. في هذا البحث, تم تصنيع مركب SiC من SiC بثلاثة تركيزات مع ZnO و Si. تم اختبار الخواص المغناطيسية لجميع المخاليط باستخدام مراقبة العينة الاهتزازية (VSM). تم تلبيد العينات الخضراء في فرن التلبيد عند 1600 درجة مئوية في بيئة النيتروجي
... Show MoreIn this research, we study the changing structural properties of ZnO with changing annealing temp., in the range (473-773)K prepared by chemical bath deposition method at temp. (353)K, where deposited on glasses substrates at thickness (500±25)nm, the investigation of (XRD) indicates that the (ZnO) films are polycrystalline type of Hexagonal.
The results of the measuring of each sample from grain size, microstrain, dislocation density, integral breadth, shape factor and texture coefficient, show that annealing process leads to increase the grain size (26.74-57.96)nm, and decrease microstrain (0.130-0.01478), dislocation density (1.398-0.297)*1015
... Show MoreIn this work, biocompatible gold nanoparticles were synthesized by reducing the chloroauric acid with ascorbic acid as a reducing agent. Colloidal gold nanoparticles were stabilized through nontoxic acacia gum sodium hydroxide .Synthesizing gold nano particle is confirmed by the change in color of chloroauric acid from yellow to ruby red and brown color depending on the stabilizers. The gold nanoparticles were characterized by UV-Visible spectrophotometer. Where the peak of the absorbance of surface plasmon resonance (SPR) was observed between the wave length 526 and 535 nm. The results of zeta potential were found in rang (-19, -40 mv), AFM and TEM images show two different shapes, hexagonal and spherical and the size of gold nanopartic