Steel fiber aluminum matrix composites were prepared by atomization technique. Different air atomization conditions were considered; which were atomization pressure and distance between sample and nozzle. Tensile stress properties were studied. XRF and XRD techniques were used to study the primary compositions and the structure of the raw materials and the atomized products. The tensile results showed that the best reported tensile strength observed for an atomization pressure equal to 4 mbar and sample to nozzle distance equal to 12 cm. Young modulus results showed that the best result occurred with an air atomization pressure equal to 8 mbar and sample to nozzle distance equal to 16cm
Aluminum alloy 5052 had been anodized by sulfuric acid as an electrolyte under constant voltage and the anodic oxide film produce will be testing by potentiostatic anodic polarization .Two variables, which were considered as important variables, were studied. These variables are anodizing time 15,30 min. and sealing time 10,20 min., and the test by potentiostatic anodic polarization through electro chemical polarization measurements in solutions of 1N na2so4 ( PH= 1 ). The results are discussed in light of the rate of ionic current flow through the coating during anodic polarization measurements.
The aim of this work is to evaluate some mechanical and physical
properties (i.e. the impact strength, hardness, flexural strength,
thermal conductivity and diffusion coefficient) of
(epoxy/polyurethane) blend reinforced with nano silica powder (2%
wt.). Hand lay-up technique was used to manufacture the composite
and a magnetic stirrer for blending the components. Results showed
that water had affected the bending flexural strength and hardness,
while impact strength increased and thermal conductivity decreased.
In addition to the above mentioned tests, the diffusion coefficient
was calculated using Fick’s 2nd law.
This work aimed to study the effect of laser surface treatment on the mechanical characteristics and corrosion behaviour of grey cast iron type A159. Many technical applications used conventional surface treatment, but laser surface hardening has recently been used to enhance the surface properties of many alloys. The mechanical characteristics, including microstructure, microhardness, and wear resistance of A159 grey cast iron, were studied, in addition to corrosion behaviour. The experimental laser parameters in this work were 0.9, 1.2, and 1.5 KW power with continuous wave carbon dioxide lasers with scanning speeds of 10 and 12 mm/s were used. The results found that phase-transitional alterations in microstructure were influenced by lase
... Show MoreThe objectives of this study revolve around identifying the extent of funding impact on the future of the printed Iraqi press, and whether it threatens their chances of survival, stating the extent of technological development on the income of the printed newspaper, and identifying the causes of the financial crisis on the newspaper.
This research is classified as descriptive research, and the researcher used the survey method, and adopted the questionnaire of the views of the contactors, in five Iraqi newspapers (morning - extent - time - the way of the people - the call).
The research community included (68) respondents, whereby the comprehensive inventory method was used to define the research community, and the researcher used 
The objectives of this study revolve around identifying the extent of funding impact on the future of the printed Iraqi press, and whether it threatens their chances of survival, stating the extent of technological development on the income of the printed newspaper, and identifying the causes of the financial crisis on the newspaper. This research is classified as descriptive research, and the researcher used the survey method, and adopted the questionnaire of the views of the contactors, in five Iraqi newspapers (morning - extent - time - the way of the people - the call). The research community included (68) respondents, whereby the comprehensive inventory method was used to define the research community, and the researcher used t
... Show MoreThis research studies the possibility of producing Bone China with available local and geological substitutes and other manufactured ones since it’s traditionally produced by Bone ash, Cornish stone, and China clay, while the substitutes are Kaolin instead of China clay and Feldspar potash instead of Cornish stone. Because of the unavailability of Feldspar in Iraq, it was substituted with the manufactured alternative Feldspar. Bone ash was prepared from cow bones with heating treatments, grinding and sifting. The alternative Feldspar was prepared by chemical analysis of the natural Feldspar potash with local materials that include Dwaikhla Kaolin, Urdhuma Silica sand, Potassium Carbonate, and Sodium Carbonate. The mixture was burned at
... Show More
Background: Polymethylmethacrylate (PMMA) is the most ‎commonly used mâ€aterial in denture construction. This material is ‎far from ideal in fulfilling the‎ mechanical requirements, like low impact and transverse strength and poor thermal conductivity are present in this material. The purpose of this study was to study the effect of addition a composite which include 1%wt silanized silicone dioxide nano fillers (SiO2) and 1wt% oxygen plasma treated polypropylene fiber (PP) on some properties of heat cured acrylic resin denture base material (PMMA). Materials and methods: One hundâ€red (100) prepared specimens were divided into five groups according to the tests, each group consisted of 20 specimens and t
Background: This in vitro study was carried out to evaluate the effect of various endodontic irrigants (sodium hypochlorite, ethylene diaminetetracetic acid and normal saline) on sealing ability of (Biodentine, mineral trioxide aggregate, and amalgam) used to repair furcal perforations. Material and methods: One hundred and twenty extracted human molars with divergent roots were used in this study. A standard root canal access cavity was prepared in each tooth and furcal perforation was made and was standardized by using k file size 100 instrument to get a perforation of (1.32mm) in diameter .The teeth were randomly divided in to three groups of 40 teeth according to the type of material used to repair the perforations (Group A: The furcal
... Show More 
        