In this work, an experimental research on a low voltage DC magnetron plasma sputtering (0-650) volt is used for coating gold on a glass substrate at a constant pressure of argon gas 0.2 mbar and deposition time of 30 seconds. We focused on the effects of operating conditions for the system such as, electrode separation and sputtering current on coated samples under the influence of magnetic flux. Electron temperature and electrons and ions densities are determined by a cylindrical single Langmuir probe. The results show the sensitivity of electrode separation lead to change the plasma parameters. Furthermore, the surface morphology of gold coated samples at different electrode separation and sputtering current were studied by atomic force microscopy (AFM). The AFM analysis showed that the variation of average grain diameter and average grain height is nonlinear with a minimum value of average grain diameter 90 nm at electrode separation of 4 cm and 30 mA sputtering current.
The drive of this exploration is to investigate the mucoadhesive assets of A. indica (Azadirachta indica) fruit mucilage by incorporating it into mucoadhesive microspheres with Acyclovir (AVR) as a model drug. The study was performed to check the impact of the mucilage proportion on particle size and swelling index. Nine batches of AVR mucoadhesive microspheres were made with varying proportions of Polyacrylic acid 934P and A. indica fruit mucilage (AIFM). A central composite design with design expert software to check the impact of dependent variables (A. indica mucilage and Polyacrylic acid 934 P levels) on particle size and swelling index as a response. As part of congeniality studies, the batches w
... Show MoreIn this work the diode planer magnetron sputtering device was
designed and fabricated. This device consists of two aluminum discs
(8cm) diameter and (5mm) thick. The distance between the two
electrodes is 2cm, 3cm, 4cm and 5cm.
Design and construction a double probe of tungsten wire with
(0.1mm) diameter and (1.2mm) length has been done to investigate
electron temperature, electron and ion density under different
distances between cathode and anode. The probes were situated in
the center of plasma between anode and cathode.
The results of this work show that, when the distance between
cathode and anode increased, the electron temperature decreased.
Also, the electron density increases with the increasing
Abstract:Two-dimensional crystal has been achieved and controlled with the aid of DC electric field applied between two electrodes at 5 millimeters separating distance between them. Sol-gel method has been used to prepared nanosilica particle which used in this work as well as TiO2 nanopaowder. The assembly of the silica particles is due to the interaction between the electrical force, the particles dipole, and the interaction between the particles themselves. When a DC voltage is applied, the particles accumulated and crystallized on the surface between the electrodes. The Light diffraction demonstrates that the hexagonal crystal is always oriented with one axis along the direction of the field. The particles disassemble when the field is
... Show MoreThe focus of this work is on systematically understanding the effects of packing density of the sand grains on both the internal and bulk mechanical properties for strip footing interacting with granular soil. The studies are based on particle image velocimetry (PIV) method, coupled with a high resolution imaging camera. This provides valuable new insights on the evolution of slip planes at grain-scale under different fractions of the ultimate load. Furthermore, the PIV based results are compared with finite element method simulations in which the experimentally characterised parameters and constitutive behaviour are fed as an input, and a good level of agreements are obtained. The reported results would serve to the practicing engineers, r
... Show MoreThe corrosion behavior of bare and chemical conversion coated (through anodizing) aluminum ASA 606 I in stagnant chromic acid solutions . Solutions of 2, 6 & J O wt. % Cr03 at 45°C, have been investigated using polarization technique. The anodizing experiments were conducted under fixed conditions of 35 minute exposure time and 30 volt supplied voltage. The most important feature achieved was the great difference in behavior between the anodic polarization curves for bare and anodized aluminum in different concentrations of chromic acid solutions.
Because of Cadmium selenide quantum dots (CdSe quantum dots) has a tuning energy gap in the visible light range, therefore; it is provided a simple theoretical model for the absorption coefficient of CdSe quantum dots, where the absorption coefficient determines the extent to which the light of a material can penetrate a specific wavelength before it is absorbed. CdSe quantum dots have an energy gap can be controlled through two effects: the temperature and the dot size of them. It is found that; there is an absorption threshold for each directed wavelength, where CdSe quantum dots begin to absorb the visible spectrum at a size of 1.4 nm at room temperature for a directed wavelength 3