In this research, Zinc oxide (ZnO)/epoxy nanocomposite was synthesized by simple casting method with 2wt. % ZnO concentration. The aim of this work was to study the effect of pH and composite dosage on the photocatalytic activity of ZnO/ epoxy nanocomposite. Scanning electron microscopy (SEM) technique images proof the homogeneous distribution of ZnO nanoparticles in epoxy. A synthesized nanocomposite samples were characterized by Fourier Transform Infrared spectrometer (FTIR) measurements. Two spectra for epoxy and 2wt.% ZnO/epoxy nanocomposites were similar and there are no new bonds formed from the incorporation of ZnO nanoparticles. Using HCl and NaOH were added to Methylene blue (MB) dye (5ppm) to gat pH values 3 and 8. The degradation of the dye was 90.816% were pH =8 after 180 min. under sun-light. The degradation was 6.131% were pH=3 after 240 min. under sun-light irradiation. It is found that the base solution help in accelerating the photocatalytic process, pH with high value provides greater concentration of hydroxyl ions which interact with h+ to form hydroxyl radicals OH- that give an enhancement degradation rate of dyes. The dose of ZnO was increased from 3g to 6g with Methylene blue MB (5ppm) the degradation was 94.3755% after 240 min. under sun-light irradiation. This means that increasing the dose of ZnO, the photocatalytic activity will be increased.
This work characterizes the fractographic features of the neat epoxy and ZrO2 epoxy nanocomposites. All samples were subjected to a tensile test to determine the tensile strength and tensile modulus. SEM images were used to study the morphology of the fractured surface. The fractographic of the fracture surfaces were studied by microstructure analysis program (j-images) to specify the effect of ZrO2 nanoparticles on tensile performance and failure mechanism for ZrO2 epoxy nanocomposites. The tensile test results show that the addition of ZrO2 nanoparticles (2, 4, 6, 8, and 10 vol.%) to the epoxy matrix leads to increase the tensile strength about 40% for optimal content of ZrO2 nanop
... Show MorePreparation of epoxy/ TiO2 and epoxy/ Al2O3 nanocomposites is studed and investigated in this paper. The nano composites are processed by different nano fillers concentrations (0, 0.01, 0.02 ,0.03, 0.04 ,0.05 ,0.07 and 0.1 wt%). The particles sized of TiO2,Al2O3 are about 20–50 nm.Epoxy resin and nano composites containing different shape nano fillers of (TiO2:Al2O3 composites),are shear mixing with ratio 1 to 1,with different nano hybrid fillers concentrations( 0.025 ,0.0 5 ,0.15 ,0.2, and 0.25 wt%) to Preparation of epoxy/ TiO2- Al2O3 hybrid composites. The mechanical properties of nanocomposites such as bending ,wearing, and fatigue are investigated as mechanical properties.
Metal oxide nanocomposites (MONCs) manufacturing is increasingly gaining popularity. The primary cause of this is the broad range of applications for such materials, which include fuel cells, photovoltaics, cosmetics, medicine, semiconductor packing materials, water treatment, and catalysts. Due to their size, stability, high surface area, catalytic activity, simplicity in fabrication, and selectivity for particular reactions. The MONCs with various morphologies have been created by physical, chemical, and biological processes, such as sol-gel, hydrothermal, co-precipitation, solvothermal, and microwave irradiation. Eugenol (4-allyl-2-methoxyphenol) is a major component of clove essential oil and it was found in various plant groups, has
... Show MorePreparation of epoxy/MgO and epoxy/SiO2 nanocomposites is
studding. The nano composites were processed by different nano
fillers concentrations (0, 0.01, 0.02, 0.03, 0.04, 0.05, 0.07 and
0.1 wt%). Epoxy resin and nanocomposites containing different
shape nano fillers of (MgO:SiO2 composites), are shear mixing with
ratio 1:1,with different nano hybrid fillers concentrations (0.025,
0.05, 0.1, 0.15, 0.2 and 0.25 wt%) to preparation of epoxy/(MgOSiO2)
hybrid nanocomposites. Experimental tests results indicate that
the composite materials have significantly higher modulus of
elasticity than the matrix material but the hybrid nanocomposites
have lower modulus of elasticity. The wear rate was decreased in
nanoc
Powder Silica (SiO2) was added to epoxy polymer with different weight percentages (3.75,7.5,11.25 and 15 wt%) for particle size  63 µm. Hand lay-up method it is used to prepared (Epoxy-Silica) composite, and cutting appropriate specimens for testing. Electrical strength varies nonlinearly with specimens thickness, also decreasing with average time for the rise of voltage decreases due to electro thermal effects. Clearly, electrical strength decreases with the increase of the proportion of added silica. The hardness, tensile strength and young modulus increased with the added silica increases due to changing in material characteristics from ductility to brittle. Microscopic cracks and irregularity deformation were a
... Show MoreThis work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.
Polycaprolactone is one of the natural biodegradable polymers mainly used in bioplastics production for packaging, usually composed of non-toxic compounds and biodegradable. The aim was to examine the role of zinc oxide (ZnO) nanopowder on the,wettability , thermal and anti-bacterial effect nanocomposites. Pure PCL and PCL-based bio- nanocomposites doped with various ratios of ZnO nanoparticles from 0% to 5wt% were prepared through the arrangement of throwing procedure. The results show that wettability properties in relation to ideal PCL and that they were increasingly hydrophobic from 57º.8 to 69º.53 because add ZnO nanocomposites,the thermal stability between 300 and 400 ° C makes them perfect for the application
... Show More