Nanoparticle has pulled in expanding consideration with the developing enthusiasm for nanotechnology which hold potential as essential segments for development applications. In the present work, a copper nanoparticle is manufactured as a suspension in distilled water by beating a bulk copper target with laser source (532 nm wavelength, 10 ns pulse duration and 10 Hz repletion rate) via method. UV- visible absorption spectra and AFM analysis has been done to observe the effect of repetition rate for the pulsation of laser. Copper nanoparticles (Cu-NPs) were successfully synthesized with green color. The Cu- NPs have very high purity because the preparation was managed in aqueous media to eliminate ambient contaminations. Absorption spectrum shows peaks at 450 nm- 700 nm µm due to the generation of Cu-NPs.
The size and the concentration of the gold nanoparticles (GNPs)
synthesized in double distilled deionized water (DDDW) have been
found to be affected by the laser energy and the number of pulses.
The absorption spectra of the nanoparticles DDDW, and the
surface plasmon resonance (SPR) peaks were measured, and found to
be located between (509 and 524)nm using the UV- Vis
spectrophotometer. SPR calculations, images of transmission
electron microscope, and dynamic light scattering (DLS) method
were used to determine the size of GNPs, which found to be ranged
between (3.5 and 27) nm. The concentrations of GNPs in colloidal
solutions found to be ranged between (37 and 142) ppm, and
measured by atomic absorptio
This research aims to find a method to synthesize nanoparticles of important metals in the fields of medicine and electronics, with high purity small in size and narrow size distribution. And it characterized by simplicity, efficiency and high productivity. To achieve this aim the effects of laser irradiation on silver and copper colloids prepared by exploding wire technique in double distilled and deionized water (DDDW) have been studied. The laser irradiation was performed using laser radiation fluence about 4 J/cm2 at 532 nm wavelength. Additional irradiation of colloids resulted in the changes of particles morphology, which were monitored by absorption spectroscopy and transmission electron microscopy methods. It was found that both
... Show MoreIn this article Silver nanoparticles have been synthesized through physical method where the Nd-YAG laser has been used.The antimicrobial activities of these silver nanoparticles were investigated on two types of bacteria Escherichia coli and Staphylococcus aureus. These bacteria were used as representatives of Gram-negative and Gram-positive bacteria, respectively. Two experiments have been made The first one was to test the effectiveness of silver nanoparticles as an antimicrobial agent on Gram negative bacteria Escherichia coli and Gram positive bacteria Staphylococcus aureus, while the other one (susceptibility Test) was to evaluate antimicrobial agents effective against bacteria resistant to multiple antibiotics. This study showed t
... Show MoreThe natural polyphenolic compound that cinnamon contains is well known for its various biological activities, a broad variety of pharmacological and therapeutic properties. Diversified biomedical and pharmacological applications benefit from organic nanoparticles with controlled properties. Bioactive and non-toxic, cinnamon nanoparticles (CNPs) can be effective antibacterial agents. Driven by this idea, we prepared spherical CNPs using liquid (PLAL) pulse laser ablation technique and defined those NPs. Using Q-switched Nd : YAG With a wavelength of 1064 nm pulse laser of constant energy 500 mj , And different laser pulses ( 250 , 500 , 750 , 1000 ) pulse /sec a pure cinnamon target submerged in
... Show MoreIn this study, graphene oxide (GO) and reduced graphene oxide were synthesized by pulsed Nd:YAG laser with a fundamental wavelength (1064 nm) focused on the pure graphite target which was immersed in distilled water. Different pulse energies were applied in two cases; with and without magnetic field. The synthesized GO and rGO nanoparticles were characterized by UV-visible spectroscopy, X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy and atomic force microscopy (AFM) with and without magnetic field. The data show the presence of a magnetic field which illustrated increasing oxygen functional groups of GO. This caused a change in the morphology of the surface of GO, increasing crystallite size from 12.19 nm to 71.2
... Show MoreSilver nanoparticles (Ag-NPs) have unique properties as antibacterial effects against locally isolated clinical Escherichia coli. In this study, the evaluated the antibacterial activity of AgNPs, which were synthesized by laser ablation, against locally isolated clinical Escherichia coli on nutrient agar media in vitro. Then assessed the toxicity of the bactericidal dose in albino rats in vivo with hematological, liver, and kidney functions as vital parameters. AgNPs were synthesized by pulsed laser ablation in liquid (PLAL). AgNPs’ shape and nano size were characterized by atomic force microscopy (AFM), UV-vis spectroscopy, and scanning electron microscopy (
... Show MorePulsed laser ablation in liquid (PLAL) has become an increasingly important technique for metals production and metal oxides nanoparticles (NPs) and others. This technique has its many advantages compared with other conventional techniques (physical and chemical). This work was devoted for production of zirconia (ZrO2) nanoparticles via PLAL technique from a solid zirconium target immersed in a wet environment in order to study the effect of this environment on the optical properties and structure of ZrO2 nanoparticles. The solutions which used for this purpose is distilled water (D.W). The produces NPs were characterized by mean of many tests such as UV-visible (UV-Vis.), transmission electron microscope (TEM) and Z-Potential. The UV-Vis.
... Show MorePulsed laser ablation in liquid (PLAL) technique can produce high purity nanoparticles, it is a top-down physical method based on the principle of dividing metal ion bulk precursors into metal atoms, this method was used in this work to synthesis cobalt nanoparticals (CoPNs) with the use of Nd: YAG laser with two wavelengths (355 nm) and (532 nm) at energies (500 mJ) and (600 mJ) respectively, with number of pulses (1000,1100, 1200, 1300, and 1400) for each wavelength. The properties of the prepared nanoparticles were studied by UV-Vis, XRD, SEM with EDX, AFM, and FTIR analysis and then its antibacterial activity was studied by applying it on two types of bacteria with gram-positive (Staphylococcus aureus, Streptococc
... Show MoreLaser ablation of a silver target immersed in distilled water using Nd:YAG laser with a fundamental wavelength of 1064nm was carried out to fabricate silver nanoparticles (Ag NPs) with different laser energy in the presence and absence of magnetic field. UV-Visible spectrum showed that the nanoparticles are almost spherical in shape. The number of Ag NPs increased by increasing laser energy while their particle size was reduced by increasing laser energy without magnetic field. In the presence of magnetic field, the size of Ag NPs increased slightly by increasing laser energy. According to AFM results, the presence of magnetic field did not affect the average diameter of Ag NPs. The presence of a magn
... Show MoreIn this work we study the influence of the laser pulse energy and ablation time on the aluminum nanoparticles productivity during nanosecond laser ablation of bulk aluminum immersed in liquid.
Aluminum nanoparticles were synthesized by pulsed laser ablation of Al targets in ethanol for 3-8 minutes using the 1064 nm wavelength of a Nd:YAG laser with energies of 300-500 mJ per pulse.The laser energy was varied between 300 and 500 mJ/pulse, whereas the ablation time was set to 5 minutes. UV-Visible absorption spectra was used for the characterization and comparison of products.