Rare earth elements (Cerium, Lanthanum and Neodymium) doped CdS thin films are prepared using the chemical Spray Pyrolysis Method with temperature 200 oC. The X-ray diffraction (XRD) analysis refers that pure CdS and CdS:Ce, CdS:La and CdS:Nd thin films showed the hexagonal crystalline phase. The crystallite size determined by the Debye-Scherrer equation and the range was (35.8– 23.76 nm), and it was confirmed by field emission scanning electron microscopy (FE-SEM). The pure and doped CdS shows a direct band gap (2.57 to 2.72 eV), which was obtained by transmittance. The room-temperature photoluminescence of pure and doped CdS shows large peak at 431 nm, and two small peaks at (530 and 610 nm). The Current – voltage measurement in dark and illumination (100 mW/cm2, 183 mW/cm2 and 288 mW/cm2) condition. The photocurrent increases and the resistivity decreases with the light intensity increases. So film reveals photoconductivity phenomena suggesting it's useful for optoelectronic applications.
Thin film technology is one of the most important technologies
that have contributed to the development of semiconductors and their
applications in several industrial fields. The Iron Oxides (Fe20) and
(Co3O4) thin films and their applications are of importance, in that these
two materials are considered as important industrial materials, and used
in spectrally selective coating, temperature sensors, resistive heaters, and
photo cells.
Thin films of Iron Oxide (Fe20,), Cobalt Oxide (Co304) and
their mixtures in different ratios (75:25, 50:50, 25:75) were prepared by
the method of chemical spray pyrolysis deposition at different thicknesses
(77s t S200) nm on cover-glass substrates: thickness of (1) mm at
Alloys of Bi2[Te1-x Sex]3 were prepared by melting technique with different values of Se percentage (x=0,0.1,0.3,0.5,0.7,0.9 and 1). Thin films of these alloys were prepared by using thermal evaporation technique under vacuum of 10-5 Torr on glass substrates, deposited at room temperature with a deposition rate (12nm/min) and a constant thickness (450±30 nm). The concentrations of the initial elements Bi, Te and Se in the Bi2 [Te1-x Sex]3 alloys with different values of Se percentage (x), were determined by XRF,The morphological and structural properties were determined by AFM and XRD techniques. AFM images of Bi2[Te1-x Sex]3 thin films show that the average diameter and the average surface roughness inc
... Show MoreIn this work, vanadium pentoxide (V2O5) thin films were prepared using rf magnetron sputtering on silicon wafer and glass substrates from V2O5 target at 200 °C substrate temperature, followed by annealing at 400 and 500 °C in air for 2 h. The prepared thin films were examined by X-ray diffraction (XRD), forier transform infra-red spectroscopy (FTIR), UV-visible absorbance, and direct current coductivity to study the effects of annealing temperature on their structural and optical properties. The XRD analysis exhibited that the annealing promoted the highly crystallized V2O5 phase that is highly orientated along the c direction. The crystalline size increased from 22.5 nm to 35.4 nm with increasing the annealing
... Show MoreMany designs have been suggested for unipolar magnetic lenses based on changing the width of the inner bore and fixing the other geometrical parameters of the lens to improve the performance of unipolar magnetic lenses. The investigation of a study of each design included the calculation of its axial magnetic field the magnetization of the lens in addition to the magnetic flux density using the Finite Element Method (FEM) the Magnetic Electron Lenses Operation (MELOP) program version 1 at three different values of current density (6,4,2 A/mm2). As a result, the clearest values and behaviors were obtained at current density (2 A/mm2). it was found that the best magnetizing properties, the high
... Show MoreZinc oxide (ZnO) nanoparticles were synthesized using a modified hydrothermal approach at different reaction temperatures and growth times. Moreover, a thorough morphological, structural and optical investigation was demonstrated using scanning electron microscopy (SEM), x-ray diffraction (XRD), ultra-violate visible light spectroscopy (UV-Vis.), and photoluminescence (PL) techniques. Notably, SEM analysis revealed the occurrence of nanorods-shaped surface morphology with a wide range of length and diameter. Meanwhile, a hexagonal crystal structure of the ZnO nanoparticles was perceived using XRD analysis and crystallite size ranging from 14.7 to 23.8 nm at 7 and 8 ℎ𝑟𝑠., respectively. The prepared ZnO samples showed good abso
... Show MoreZnO nanostructures were synthesized by hydrothermal method at different temperatures and growth times. The effect of increasing the temperature on structural and optical properties of ZnO were analyzed and discussed. The prepared ZnO nanostructures were characterized by X-ray diffraction (XRD), UV–Vis. absorption spectroscopy (UV–Vis.), Photoluminescence (PL), and scanning electron microscopy (SEM). In this work, hexagonal crystal structure prepared ZnO nanostructures was observed using X-ray diffraction (XRD) and the average crystallite size equal 14.7 and 23.8 nm for samples synthesized at growth time 7 and 8 hours respectively. A nanotubes-shaped surface morphology was found using scanning electron microscopy (SEM). The optic
... Show MoreIt is shown that pure and 3% boron doped a-Si0.1Ge0.9:H and a-Si0.1Ge0.9:N thin films
could be prepared by flash evaporation processes. The hydrogenation and nitrogenation
are very successful in situ after depositing the films. The FT-IR analysis gave all the
known absorbing bonds of hydrogen and nitrogen with Si and Ge.
Our data showed a considerable effect of annealing temperature on the structural and
optical properties of the prepared films. The optical energy gap (Eopt.) of a-Si0.1Ge0.9
samples showed to have significant increase with annealing temperature (Ta) also the
refractive index and the real part of dielectric constant increases with Ta, however the
extinction coefficient and imaginary part of dielect
(Cu1-x,Agx)2ZnSnSe4 alloys have been fabricated with different Ag content(x=0, 0.1, and 0.2) successfully from their elements. Thin films of these alloys have been deposited on coring glass substrate at room temperature by thermal evaporation technique under vacuum of 10-5Torr with thickness of 800nm and deposition rate of 0.53 nm/sec. Later, films have been annealed in vacuum at (373, and 473)K, for one hour. The crystal structure of fabricated alloys and as deposited thin films had been examined by XRD analysis, which confirms the formation of tetragonal phase in [112] direction, and no secondary phases are founded. The shifting of main polycrystalline peak (112) to lower Bragg’s angle as compared to Cu2ZnSnSe4 angle refers to incorpora
... Show More