TiO2 thin films have been deposited at different concentration of
CdO of (x= 0.0, 0.05, 0.1, 0.15 and 0.2) Wt. % onto glass substrates
by pulsed laser deposition technique (PLD) using Nd-YAG laser
with λ=1064nm, energy=800mJ and number of shots=500. The
thickness of the film was 200nm. The films were annealed to
different annealing (423 and 523) k. The effect of annealing
temperatures and concentration of CdO on the structural and
photoluminescence (PL) properties were investigated. X-ray
diffraction (XRD) results reveals that the deposited TiO2(1-x)CdOx
thin films were polycrystalline with tetragonal structure and many
peaks were appeared at (110), (101), (111) and (211) planes with
preferred orientation along 2Ɵ around 27.30. The results of
photoluminescence (PL) emission show that there are two peaks
positioned are around 320 nm and 400 nm for predominated peak
and 620 nm and 680 nm for the small peaks.
In this paper, a new seven-parameter Mittag-Leffler function of a single com-plex variable is proposed as a generalization of the standard Mittag-Leffler function, certain generalizations of Mittag-Leffler function, hypergeometric function and confluent hypergeometric function. Certain essential analytic properties are mainly discussed, such as radius of convergence, order, type, differentiation, Mellin-Barnes integral representation and Euler transform in the complex plane. Its relation to Fox-Wright function and H-function is also developed.
Phenol oxidation by Fenton's reagent (H2O2 + Fe+2) in aqueous solution has been studied for the purpose of learning
more about the reactions involved and the extent of the oxidation process, under various operating conditions. An initial
phenol concentration of 100 mg/L was used as representative of a phenolic industrial wastewater. Working temperature
of 25C was tested, and initial pH was set at 5.6 . The H2O2 and the Fe+2 doses were varied in the range of
(H2O2/Fe+2/phenol = 3/0.25/1 to 5/0.5/1). Keeping the stirring speed of 200 rpm.
The results exhibit that the highest phenol conversion (100%) was obtained under (H2O/Fe+2/phenol ratio of 5/0.5/1)
at about 180 min. The study has indicated that Fenton's oxidation i
Physical adsorption by nitrogen gas was studied on seven commercial platinum reforming catalysts (RG-402, RG-412, RG-432, RG-451, RG 422,RG-482, PS-10), four prepared platinum catalysts (0.1%Pt/alumina, 0.2 %Pt/alumina, 0.45 %Pt/alumina and 0.55% Pt/alumina), and -alumina support. Physical adsorption was carried out by using Accelerated Surface Area and Porosimetry (ASAP 2400 device) at 77 K . The results indicate that the surface area in genaral decreases with increasing platinum percentage, high platinum loaded (0.45% and 0.55%) it was found that the percent increasing in surface area was lower than those obtained for low platinum loaded catalysts , and at very higher platinum loading 0.6 %Pt , some reduction in surface area was
... Show MoreBackground: The present study aimed to determine the influence of the different types of mouth wash on discoloration of different orthodontic ceramic, sapphire brackets and adhesives. Materials and methods: The sample composed of 120 ceramic brackets and 120 sapphire brackets, the brackets were divided according to bond material into three groups of 40 brackets include unbounded brackets, chemically cured (no-mix) bonded brackets and Light cured bonded brackets all these groups were further subdivided according to mouth wash type into three groups with 10 brackets each which include; Listerine, cetrimide, chlorhexidine 0.2%, and one control group which immersed in artificial saliva; then Staining measurements were performed with UV-Visibl
... Show MoreThe MTX was converted to MTX nanoparticles by the modified method based on changing the pH gradually . For the first time MTX NPs+Meropenem complex were prepared and evaluated as a potential tool to overcome antimicrobial resistance and to improve pharmacokinetics of the drug, the results showed that the antibacterial activity of complex (MTX NPs plus MEM) has increased (from 1( µg/ml) to >0.5( µg/ml) for p1 , from 2( µg/ml) to 1( µg/ml) for p10 and from 8( µg/ml) to 4( µg/ml) for p48).
in this work the polymides were prepared as rthemally stable polymers by diffrent ways