This work concerns the thermal and sound insulation as well as the mechanical properties of polymer matrix composite reinforced with glass fibers. These fibers may have dangerous effect during handling, for example the glass fibers might cause some damage to the eyes, lungs and even skin. For this reason the present work, investigates the behavior of polymer composite reinforced with natural fibers (Plant fibers) as replacement to glass fibers. Unsaturated Polyester resin was used as matrix material reinforced with two types of fibers, one of them is artificial (Glass fibers) and the other type is natural (Jute, Fronds Palm and Reed Fibers) by hand lay-up technique. All fibers are untreated with any chemical solvent. The Percentage of mixing was (90 wt. %) of the matrix while the weight fraction of each type of fibers was fixed (10 wt. %). The mechanical tests included impact and flexural strength tests. The results showed that the impact strength and flexural strength of the composites reinforced with Jute fibers is higher than that of Glass fibers and other natural fibers. The coefficients of thermal conductivity of the composites were measured by Lee's disc apparatus, the results show that the thermal insulation of the composite reinforced with jute fibers is higher than that of glass fibers and other natural fibers. The acoustic insulation of the composites reinforced with Jute fibers showed excellent result in insulation compared with glass fibers and other natural fibers.
A new heterocyclic Schiff bases ligand (HL) derived from condensation of 2-Amino-4-methylbenzothiazole with 4-Diethylaminosalicylaldehyde have been synthesized and characterized by (FTIR & UV.Vis) spectroscopies, (1H & 13C)NMR spectra, mass spectrum, elemental microanalysis (C,H,N,S). Metal complexes with Co(II), Ni(II), Cu(II), Zn(II) and Cd(II) ions have been also synthesized and characterized by (FTIR & UV.Vis) spectroscopies, flame atomic absorption, molar conductivity measurements and magnetic susceptibility. These studies indicate that the mole ratio (L:M) is (2:1) for Co(II) complex and (1:1) for other complexes. The spectral results indicate that the ligand coordinates with met
... Show MoreIn this research, damping properties for composite materials were evaluated using logarithmic decrement method to study the effect of reinforcements on the damping ratio of the epoxy matrix. Three stages of composites were prepared in this research. The first stage included preparing binary blends of epoxy (EP) and different weight percentages of polysulfide rubber (PSR) (0%, 2.5%, 5%, 7.5% and 10%). It was found that the weight percentage 5% of polysulfide was the best percentage, which gives the best mechanical properties for the blend matrix. The advantage of this blend matrix is that; it mediates between the brittle properties of epoxy and the flexible properties of a blend matrix with the highest percentage of PSR. The second stage
... Show MoreHeterocyclic systems, which are essential in medicinal chemistry due to their promising cytotoxic activity, are one of the most important families of organic molecules found in nature or produced in the laboratory. As a result of coupling N-(4-nitrophenyl)-3-oxo-butanamide (3) using thiourea, indole-3-carboxaldehyde, or piperonal, the pyrimidine derivatives (5a and 5b) were produced. Furthermore, pyrimidine 9 was synthesized by reacting thiophene-2-carboxaldehyde with ethyl cyanoacetate and urea with potassium carbonate as a catalyst. The chalcones 11a and 11b were synthesized by reacting equal molar quantities of 1-naphthaldehy
... Show MoreIn this investigation, the mechanical properties and microstructure of Metal Matrix Composites (MMCs) of Al.6061 alloy reinforced by ceramic materials SiC and Al2O3 with different additive percentages 2.5, 5, 7.5, and 10 wt.% for the particle size of 53 µm are studied. Metal matrix composites were prepared by stir casting using vortex technique and then treated thermally by solution heat treatment at 530 0C for 1 hr. and followed by aging at 175 0C with different periods. Mechanical tests were done for the samples before and after heat treatment, such as impact test, hardness test, and tensile test. Also, the microstructure of the metal matrix composites was examine
... Show MorePreparation and Identification of some new Pyrazolopyrin derivatives and their Polymerizations study
A new ligand complexes have been synthesis from reaction of metal ions of MnII , CoII , NiII , CuII , ZnII , CdII and PdII with schiff base [(E)-1-((2-amino-5-(3, 4, 5-trimethoxybenzyl) pyrimidin-4-ylimino) methyl) naphthalen-2-ol [HL)]. The prepared [HL] was characterized by FT-IR, UV-Vis spectroscopy, 1H13CNMR spectra Mass spectra and melting point. The compounds were characterized by techniques UV-Vis and FT-IR spectral studies, micro analysis (C.H.N), determination of atomic absorption, chloride content, molar conductivity measurements, magnetic susceptibility and melting point. The ligand acts as a monobasic tridentate, coordinating through deprotonated phenolic O and azomethine N atoms. The compounds are neutral electrolytic in dimeth
... Show MoreIn this research, the efficiency of low-cost unmodified wool fibers were used to remove zinc ion from industrial wastewater. Removal of zinc ion was achieved at 99.52% by using simple wool column. The experiment was carried out under varying conditions of (2h) contact time, metal ion concentration (50mg/l), wool fibers quantity to treated water (70g/l), pH(7) & acid concentration (0.05M). The aim of this method is to use a high sensitive, available & cheep natural material which applied successfully for industrial wastewater& synthetic water, where zinc ion concentration was reduced from (14.6mg/l) to (0.07mg/l) & consequently the hazardous effect of contamination was minimized.
Nanocomposite of carbon nanotube add to epoxy resin material of weight fraction ( 0.25, 0.5, 0.75 1.0, 1.25, 1.5, 1.75 , 2 & 2.5 wt. % ) were fabricated by dispersing within an epoxy resin using a Ultrasound machine followed by mechanical stirring. The samples were heat treated at temperature ( 80 °C for 3 hrs) The mechanical properties of the composites were investigated. Wear and hardness properties measurements indicated higher wear rate and hardness with increasing concentration of MWCNTs . The MWCNTs significantly improved the wear resistance and hardness when compare than the pure epoxy. These note show too after heat treatment of composite with ( 80 oC for 3 hrs ).
Comparison for the optical energy gap between pure
PMMA , PMMA-TiO2 micro composites and PMMA-TiO2 nano
composites have been investigated under uv – radiation , the
effect of time irradiation (0,6,12,24,48,72,96 and 120) have been
studied for these specimens to study the photic stability .The
results show that the photostability of the PMMA-TiO2
nanocomposite is higher than that of the pure PMMA and
PMMA-TiO2 micro composite under UV-light irradiation