This work concerns the thermal and sound insulation as well as the mechanical properties of polymer matrix composite reinforced with glass fibers. These fibers may have dangerous effect during handling, for example the glass fibers might cause some damage to the eyes, lungs and even skin. For this reason the present work, investigates the behavior of polymer composite reinforced with natural fibers (Plant fibers) as replacement to glass fibers. Unsaturated Polyester resin was used as matrix material reinforced with two types of fibers, one of them is artificial (Glass fibers) and the other type is natural (Jute, Fronds Palm and Reed Fibers) by hand lay-up technique. All fibers are untreated with any chemical solvent. The Percentage of mixing was (90 wt. %) of the matrix while the weight fraction of each type of fibers was fixed (10 wt. %). The mechanical tests included impact and flexural strength tests. The results showed that the impact strength and flexural strength of the composites reinforced with Jute fibers is higher than that of Glass fibers and other natural fibers. The coefficients of thermal conductivity of the composites were measured by Lee's disc apparatus, the results show that the thermal insulation of the composite reinforced with jute fibers is higher than that of glass fibers and other natural fibers. The acoustic insulation of the composites reinforced with Jute fibers showed excellent result in insulation compared with glass fibers and other natural fibers.
In this investigation, the mechanical properties and microstructure of Metal Matrix Composites (MMCs) of Al.6061 alloy reinforced by ceramic materials SiC and Al2O3 with different additive percentages 2.5, 5, 7.5, and 10 wt.% for the particle size of 53 µm are studied. Metal matrix composites were prepared by stir casting using vortex technique and then treated thermally by solution heat treatment at 530 0C for 1 hr. and followed by aging at 175 0C with different periods. Mechanical tests were done for the samples before and after heat treatment, such as impact test, hardness test, and tensile test. Also, the microstructure of the metal matrix composites was examine
... Show MoreFor aspirin estimated, a molecularly imprinted polymer MIP-ASP electrodes were generated by electro-polymerization process, the electrodes were prepared by combining the template (aspirin) with (vinyl acetate (VA), 1-vinylimidizole (VIZ) as a functional monomer and N, N-methylene bisacrylamide (MBAA) as crosslinkers using benzoyl peroxide (BPO) as an initiator. The efficiency of the membrane electrodes was analyzed by differential pulse voltammetry (DPV). Four electrodes were synthesized using two different plasticizers, di-butyl sebacate (DBS), di-octyl phthalate (DOP) in PVC matrix. Scanning electron microscopy (SEM) was used to describe the generated MIP, studying the electrodes properties, the slope, detection limit, and life
... Show MoreA series of lanthanide metal (???) complexes have been prepared from the new azo ligand, 3-(1-methyl-2-benzimidazolylazo)-Tyrosine (MBT). The structural feature were confirmed on the basis of their elemental analysis, metal content, molar conductance, magnetic measurement, FTIR, 1 HNMR and UV-Vis spectra studies. The isolated complexes were found to have a mole ratio (1:2) (metal:ligand) stoichiometry with the general formula [Ln(MBT)2]Cl (Ln(???) = La, Ce, Pr, Nd, Sm, Eu and Gd). The chelates were found to have octahedral structures. The FTIR spectra shows that the ligand (MBT) is coordinated to lanthanide ions as a N, N, O-tridentate anion via benzimidazole nitrogen, azo nitrogen and oxygen of hydroxyl after deprotonation. Com
... Show MoreNanocomposite was prepared using unsaturated polyester (UP) resin as a matrix and graphene nanoparticles as a reinforcement material in six percentage weights (0, 0.1, 0.2, 0.3, 1 and 1.5%). Mechanical, calorimetric and thermal studies were performed on the (UP) resin/graphene nanocomposite. All tests showed a clear improvement of all mechanical properties examined (hardness, flexural strength (F.S), impact strength (I.S) and tensile strength (T.S)) with increasing graphene percentage. In addition, the temperature of glass transition and thermal conductivity of this composite increased with increasing graphene content.
Coconut milk is considered as a natural drink that enhances the immunity and it is enriched by calcium, iron, magnesium and vitamin (C) and it is also safe drink for kids and bacterial anti-oxdant, and it may be used in the natural juices instead of the whole milk (cow milk) which is added to some juices. This study aimed to determine the nutritrnal value and the sensory evaluation properties of the natural orange juice enriched by canned coconut milk &nb
... Show MoreThe fluorescence emission of Rhodamine 6G (R6G) and Acriflavine dyes in PMMA polymer have been studied by changing the irradiation and exposure time of laser light to know the effect of this parameter. It was found that the fluorescence intensity decreases in the polymer samples doped dyes as the exposure time increases and then reaches stabilization at long times, this behavior called photobleaching, which have been shown in liquid phase less than solid phase. Using 2nd harmonic with wavelength 530 nm laser, the photobleaching effect in the two dye-doped polymers different solvent but same was studied. It was observed that photobleaching of by different solution and by using dip spin coating the photobleaching seem in liquid phase more
... Show MoreThis study was done to test the activity of some plant extracts as antioxidant agents. The plants were (Morus rubra, Hibiscus sabdariffa L ., Rhus coriaria L., Anethum graveolens and Petroselinum sativum).
Ethanolic 98% (24 hours/ 25˚c) and distilled water (30 minutes/ 25˚c have been used for extraction.The Total phenols, total flavonoids, total anthocyanin, antioxidant activities were studied.
The extract of Morus rubra was chosen because it has a higher antioxidant activity.
The phenolic extract of Morus rubra was prepare and examined by application it in burger . The antioxidant activity test of Morus rubra was made before and after 3,6 days of cold storage. The sensory evaluation of all treatments were done within 5,1