In this study, titanium dioxide (TiO2) nanoparticles incorporated with cement were synthesis by a simple casting method as a function concentration of TiO2 (0.2, 0.4, 0.8, 1, and 2 wt%). The prepared samples were characterized using the technique of Field Emission Scanning Electron Microscope (FESEM) and UV-Visible spectrophotometer, which was used to measure the adsorption spectra. The observed photocatalytic efficiency of TiO2 nanoparticles (NP) incorporated with cement was investigated by decomposing the dye methyl blue (MB) solution under sunlight irradiation. According to the slope, the value of the k constant at the best sample is 0.8wt%, k=0.8265 min-1. FESEM image of the TiO2/cement with 0.8 wt% content show the TiO2 NPs were well-attached to cement particles, and they covered the cement surface. The increase in photocatalytic (PC) activity was due to an increase of TiO2 concentration in the cement, which best occur of 0.8 wt% of TiO2 in cement. The degradation at the MB (5ppm) was 98.864 % after 120 min under sunlight irradiation. The method involves easily and simply preparing TiO2/cement that is used in self-cleaning and studying the effect of different festive factors, including the concentration of the dye. The preparation of TiO2/cement was successful as a photocatalyst for a self-cleaning surface.
Zinc Oxide (ZnO) is considered as one of the best materials already used as a window layer in solar cells due to its antireflective capability. The ZnO/MgF2 bilayer thin film is more efficient as antireflective coating. In this work, ZnO and ZnO/MgF2 thin films were deposited on glass substrate using pulsed laser deposition and thermal evaporation deposition methods. The optical measurements indicated that ZnO thin layer has an energy gap of (3.02 eV) while ZnO/MgF2 bilayer gives rise to an increase in the energy gap. ZnO/MgF2 bilayer shows a high energy gap (3.77 eV) with low reflectance (1.1-10 %) and refractive index (1.9) leading to high transmittance, this bilayer could be a good candidate optical material to improve the performance
... Show MoreThe most universal and basic damages caused by an earthquakes are buildings damage and human casualties. A simplified method, the RADIUS 99 Tool is used to calculate seismic intensity (shaking) distribution, buildings damage, number of casualties and lifelines damage, due to assumed earthquake scenario. In this study, Al - Kadhmiya sector in Baghdad city was chosen for assessing seismic risk, for this purpose, this area was divided into mesh of 1*1 km2 cell size, and a scenario of (Manjil) earthquake (that struck Iran in 1990) was utilized with following earthquake magnitudes (5 and 7), with epicenter distance (3, 10 and 100 km), and depths (2 and 5 km). It was found that, the best soil types for constructions are those with medium and h
... Show MoreMutans streptococci (MS) are a group of oral bacteria considered as the main cariogenic organisms. MS consists of several species of genus Streptococcus which are sharing similar phenotypes and genotypes. The aim of this study is to determine the genetic diversity of the core species of clinical strains of Streptococcus mutans, Streptococcus sobrinus and Streptococcus downei by using repitative extragenic palindromic (REP) primer. The DNA of the clinical strains of S. mutans (n=10), S. sobrinus (n=05) and S. downei (n=04) have been employed in the present study, which have been previously isolated from caries active subjects. The DNA of the clinical and reference strains was
... Show MoreTitanium alloy (Ti-6Al-4V) samples were nitrided in low pressure (1.3, 3 mbar) dc-glow discharge plasmas of nitrogen. The treating time was 5, 10 and 15 hour and the temperatures range of the samples during the nitriding process was close to 800oC. The obtained microstructures of the nitride layers were studied by x-ray diffraction and optical microscopy. The ε –Ti2N, ζ-Ti3N3-x and η-Ti3N2-x.phases were formed and addition to the solid solution of nitrogen in titanium, α (Ti,N). Micro hardness measurements exhibit an increment for the Ti-alloy specimens which nitrided at 800oC for 10 and 15h.Corrosion measurements were obtained for the Ti-6Al-4V alloy in Ringer solution after plasma nitriding. The clear improving in the corrosion r
... Show More