Abstract: Objectives: To investigate the effect of temperature elevation on the bonding strength of resin cement to the zirconia ceramic using fractional CO2 laser. Background: Fractional CO2 laser is an effective surface treatment of zirconia ceramic, as it increases the bonding strength of zirconia to resin cement. Methods: Thirty sintered zirconia discs (10 mm diameter, 2 mm thickness) were prepared and divided to three groups (N=10) and five diffident pulse durations were used in each group (0.1, 0.5, 1, 5 and 10 ms). Group A was treated with 10 W power setting, group B with 20 W and group C with 30 W. During laser irradiation, temperature elevation measurement was recorded for each specimen. Luting cement was bonded to the treated zirconia surfaces and cured for 30 seconds. Shear bond strength was evaluated by a testing machine (universal) with bond failure mode determination. Results: The lowest temperature elevation measurement of the irradiated specimen which gave maximum shear bond strength was about 1.6±0.3 Ċ higher than ambient room temperature (27±0.2 ºC). Apparent micromechanical irregularities were seen in the treated samples and cracks formation with increased pulse duration and power setting were also observed. Conclusions: The temperature elevation is a vital factor in the surface roughness of zirconia ceramic with fractional CO2 laser irradiation and the lowest temperature elevation at best shear bond strength of zirconia ceramic to the resin cement is satisfied with the shorter pulse duration of 0.1 millisecond.
This study was conducted to evaluate the efficacy of Saccharomyces cerevesiae as a growth promoting agent in tomato. Soaking the seeds in yeast suspension at 5 g/L for 12h increased germination percentage, root length, root fresh and dry weight, plant height, foliage fresh and dry weight, attained 88.5% ; 8.1 cm ; 84.3 mg ; 7.03 mg ; 10.75 cm ; 839 mg and 37.75 mg compared with 80% ; 5.33 cm ; 39 mg ; 4.8 mg ; 7.35 cm ; 608 mg and 25.5 mg in seedlings grown from non treated seeds respectively. Similar results were obtained with seedling from seeds soaked in S. cerevesiae filtrate for 12 hrs. with values of 77.5% ; 6.875 cm ; 91.5 mg ; 7.5 mg ; 9.5 cm ; 777 mg and 40.35 mg compared to 66% ; 5.8 cm ; 57.7 mg ; 5.03 mg ; 5.9 cm ; 493 mg
... Show MoreThis paper aims at studying the illocutionary speech acts: direct and indirect to show the most dominant ones in a presidential speech delivered by the USA president. The speech is about the most critical health issue in the world, COVID-19 outbreak. A descriptive qualitative study was conducted by observing the first speech delivered by president Trump concerning coronavirus outbreak and surveying the illocutionary acts: directive, declarative, commissive, expressive, and representative. Searle's (1985) classification of illocutionary speech acts is adopted in the analysis.
What are the main types of the illocutionary speech acts performed by Trump in his speech?; Why does
... Show MoreKinetics study on the phenol oxidation by catalytic wet air oxidation (CWAO) using CuO.NiO/Al2O3 as heterogeneous catalyst is presented. 4 g/l phenol solution of pH 7.3 was oxidized in a trickle bed reactor with gas flow rate of 80% stochiometric excess (S.E).. In order to verify the proposed kinetics, a series of CWAO experimental tests were done at two temperatures (140 and 160° C), oxygen partial pressures (9 and 12 bar), and weight hourly space velocity (WHSV) (1, 1.5, 2, 2.5, and 3 h-1). According to Power Law, the reaction orders are found to be approximately 1 and 0.5 with respect to phenol concentration and oxygen solubility, respectively. These values favorably compare with those cited in the literature for intrinsic kinetics,
... Show MoreAA3003-H14 aluminum alloy plates were welded by friction stir welding and TIG welding.
Fatigue properties of the welded joints were evaluated based on the superior tensile properties for
FSW at 1500 rpm rotational speed and 80 mm/min welding speed. However, there is not much
information available on effect of welding parameters with evolution of fatigue life of friction stir
welds. The present study experimentally analyzed fatigue properties for base, FSW, and TIG welds
of AA 3003-H14 aluminum alloy. Fatigue properties of FSW joints were slightly lower than the
base metal and higher than TIG welding.
Background. After tooth extraction, alveolar bone resorption is inevitable. This clinical phenomenon challenges dental surgeons aiming to restore esthetic and function. Alveolar ridge preservation can be applied to minimize dimensional changes with a new socket grafting material, an autogenous dentin graft, produced by mechanically and chemically processing natural teeth. This study assessed the safety and efficacy of using autogenous dentin biomaterial in alveolar ridge preservation. Materials and Methods. Patients with nonrestorable maxillary anterior teeth bounded by natural sound teeth were included in this study. After a detailed clinical and tomographic examination, eligible participants were randomly allocated into two groups
... Show MoreExistence of these soils, sometimes with high gypsum content, caused difficult problems to the buildings and strategic projects due to dissolution and leaching of gypsum by the action of waterflow through soil mass. In this research, a new technique is adopted to investigate the performance of replacement and geosynthetic reinforcement materials to improve the gypseous soil behavior through experimential set up manufactured loaclally specially for this work. A series of tests were carried out using steel container (600*600*500) mm. A square footing (100*100) mm was placed at the center of the top surface of the bed soil. The results showed that the most effective thickness for the dune sand layer with geotextile at the interface, within
... Show MoreBackground: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.
Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.
Results: The artificially aged retainers showed a marginally
... Show More