Background: Acne is a common disorder experienced by adolescents and persists into adulthood in approximately 12%–14% of cases with psychological and social implications of high gravity. Fractional resurfacing employs a unique mechanism of action that repairs a fraction of skin at a time. The untreated healthy skin remains intact and actually aids the repair process, promoting rapid healing with only a day or two of downtime. Aims: This study, was designed to evaluate the safety and effectiveness of fractional photothermolysis (fractionated Er: YAG laser 2940nm) in treating atrophic acne scars. Methods: 7 females and 3 males with moderate to severe atrophic acne scarring were enrolled in this study that attained private clinic for Dermatology and Laser in Baqubah city of Diyala - Iraq during the period from 1st of June 2019 to 10th of October 2019. Fractional Er:YAG laser 2940 nm wavelength was delivered to the whole face with a single pass treatment and for the acne scar areas with two passes. Therapeutic outcomes were assessed by standardized digital photography. Results: Three patients (30%) reported excellent improvement, five patients (50%) significant improvement, one patient (10%) moderate improvement, and one patient (10%) mild improvement in the appearance of the acne scars. Conclusion: Fractional Er: YAG a safe and effective option for the treatment of acne scars in Iraqi patients by offering faster recovery time with no or mild side effects in comparison to other traditional modalities.
Many therapeutic methods used to encourage reparative processes of cartilage and accelerate their healing such as drugs, magneto-laser and so on. Twenty four adult New Zealand rabbits used in this study. They were divided in to two groups; control and treaded with He –Ne laser. A square skin flap done on the medial aspect of both auricles followed by pealing a square piece of cartilage from the auricle then the flaps sutured .The site of the operation in the rabbits of the treated group were irradiated with He –Ne laser 5mw power for seven days began after the operation directly. 3 rabbits from each group used for collection of specimens for histopathological examination at the 1, 2, 4 & 6 weeks post the operation. Significant
... Show MoreBackground: lip lengthening procedure is one of the surgical options for the correction of gummy smile in patients with short upper lip. Methods: A comparative clinical study was conducted on 15 patients requiring lip lengthening procedure for the esthetic correction of excessive gingival exposure with gummy smile. Scalpel was used in seven patients and diode laser in the remaining eight patients. Under infiltration anesthesia, about one cm strip of mucosa was excised at the vestibular depth and the mucosa of the lip was sutured to the alveolar mucosa. Results: The diode laser group demonstrated less postoperative pain and swelling. Regarding postoperative ecchymosis, three patients in the scalpel group developed ecchymosis and no cases
... Show MoreTin oxide (Sn) nanoparticles were prepared by pulsed laser ablation (PLA) method at different laser energies (400-700mJ). (UV, XRD, AFM, SEM, EDS) methods were employed to determine the properties of nanomaterials. The optical properties showed that the energy gap decreased with increasing laser power; the structural properties showed the relationship between density and angle; Miller's coefficients for net angles were determined and the morphology properties showed the element's surface shape and surface roughness. Also, Tin oxide nanoparticles with added to Staphylococcus aureus bacteria isolated from the ear and cultured by striking method on nutrient agar to know the effect of tin oxide nanoparticles on the growth o
... Show MoreThe present work investigated the effect of distance from target surface on the parameters of lead plasma excited by 1064nm Q-switched Nd:YAG laser. The excitation was conducted in air, at atmospheric pressure, with pulse length of 5 ns, and at different pulse laser energies. Electron temperature was calculated by Boltzmann plot method based on the PbI emission spectral lines (369.03 nm, 416.98 nm, 523.48, and 561.94 nm). The PbI lines were recorded at different distances from the target surface at laser pulse energies of 260 and 280 mJ. The emission intensity of plasma increased with increasing the lens-to-target distance. The results also detected an increase in electron temperature with increasing the di
... Show MoreThis work aimed to investigate the effect of Diode laser 805 nm on plasmid DNA and RNA
contents of some Gram negative bacteria represented by Escherichia coli and Proteus mirabilis isolates
.Plasmid extraction was done using two methods (Salting out and CTAB method).Different powers and
pulse repetition rates for 805 nm Diode Laser were used to study this effect. Results revealed that the
plasmid profile of the two species were highly affected using (2, 3) W at different frequencies including
5and 10 kHz as compared with 1 kHz while plasmids were gradually disappeared at 1W, 10 kHz. In the
same time the shining of RNA was also decreased gradually then disappeared with increasing powers
especially at 2W and 10 kHz cau
In this research prepare membranes pure silicon carbide (SiC) as well as gas Alloy (ammonia) and using a laser was leaked membrane of glass flooring. To Drasesh optical properties of membranes prepared depending on the technique (Swanepoel) and Adhrt results obtained in general increased permeability pure silicon membranes
Zinc Oxide (ZnO) thin films of different thickness were prepared
on ultrasonically cleaned corning glass substrate, by pulsed laser
deposition technique (PLD) at room temperature. Since most
application of ZnO thin film are certainly related to its optical
properties, so the optical properties of ZnO thin film in the
wavelength range (300-1100) nm were studied, it was observed that
all ZnO films have high transmittance (˃ 80 %) in the wavelength
region (400-1100) nm and it increase as the film thickness increase,
using the optical transmittance to calculate optical energy gap (Eg
opt)
show that (Eg
opt) of a direct allowed transition and its value nearly
constant (~ 3.2 eV) for all film thickness (150
The objective of this study is to demonstrate the corrosion behavior of dental alloys Co-Cr-Mo, Ni-Cr-Mo and Ti-Al-V in artificial saliva at pH=4 and 37oC enriched with ethyl alcohol at 8% percentage. The linear and cyclic polarizations were investigated by electrochemical measurements. Laser surface modification was achieved for the three dental alloys to improve corrosion resistance. The results show that corrosion resistance of Co-Cr-Mo and Ni-Cr-Mo alloys only were increased after laser treatment due to the fact that laser radiation has caused a smoother surface, in addition to the decrement in corrosion current densities (icorr) for Co-Cr-Mo and Ni-Cr-Mo alloys and the reverse scan in cyclic polarization became in the wider range of