The present study was conducted with a view to determine whether focal laser therapy result in visual recovery and regression of macular edema in patients with non proliferative diabetic retinopathy and maculopathy ,and whether combined focal and scatter laser therapy in patients with proliferative diabetic retinopathy and maculopathy results in visual recovery ,regression of macular edema and regression of the risk factors. In the present work, a frequency doubled Nd: YAG laser was used for the treatment of diabetic retinopathy. The study evaluates 41 eyes of 33 diabetic patients both with Insulin Dependent Diabetes Mellitus IDDM, (n=16) and Non Insulin Dependent Diabetes Mellitus NIDDM, (n=17) with diabetic retinopathy divided into two groups. Maculopathy was regressed in 32/41 treated eyes, 23/24 with maculopathy and non-proliferative diabetic retinopathy are treated by grid laser photocoagulation, 9/17 with proliferative diabetic retinopathy and maculopathy are treated by grid combined with pan retinal photocoagulation. Maculopathy was unchanged in 7/41, deterioration in 2/41. Visual acuity improved in 8/41 patients one line of Snellen chart in young patients with shorter duration and non- proliferative diabetic retinopathy, and good visual acuity prior to therapy and 31/41 stabilized visual acuity for the follow up period, 2/41 deterioration of visual acuity by one line of Snellen chart with progression of edema, hemorrhage and exudation, 3/41 patients complain of paracentral scotoma one-week post treatment improved gradually after 2 weeks. Higher power density is needed to treat the diffuse form of maculopathy regarding the severity of maculopathy and macular edema. The power density needed to have the desired effect is less in more pigmented fundus than in fair fundus in order to have the same effect.
Superconducting thin films of Bi1.6Pb0.4Sr2Ca2Cu2.2Zn0.8O10 system were prepared by depositing the film onto silicon (111) substrate by pulsed laser deposition. Annealing treatment and superconducting properties were investigated by XRD and four probe resistivity measurement. The analysis reveals the evolution of the minor phase of the films 2212 phase to 2223 phase, when the film was annealed at 820 °C. Also the films have superconducting behavior with transition temperature ≥90K.
Z-scan has been utilized for studying the non-linear properties and optical limiting behaviors of the dye Copper Phthalocyanine thin films. The refractive index is negative, which indicates a self-defocusing behavior and non-linear absorption coefficient (
Thin films of (CdO)x (CuO)1-x (where x = 0.0, 0.2, 0.3, 0.4 and 0.5) were prepared by the pulsed laser deposition. The CuO addition caused an increase in diffraction peaks intensity at (111) and a decrease in diffraction peaks intensity at (200). As CuO content increases, the band gap increases to a maximum of 3.51 eV, maximum resistivity of 8.251x 104 Ω.cm with mobility of 199.5 cm2 / V.s, when x= 0.5. The results show that the conductivity is ntype when x value was changed in the range (0 to 0.4) but further addition of CuO converted the samples to p-type.
Background: The bond strength of root canal sealers to dentin was important for maintaining the integrity of the seal in root canal filling in both static and dynamic situations. In a static situation, it should eliminate any space that allowed the percolation of fluids between the filling and the wall while in a dynamic situation; it was needed to resist dislodgement of the filling during subsequent manipulation. Materials and Methods: Forty mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments. Instrumentation was done with copious irrigation of 5.25% sodium hypochlorite. Roots were randomly divided into four groups according to the type of cleaning and method of root canal irrig
... Show MoreIn this paper deals with the effect laser irradiation on the optical properties of cobalt oxide (CoO2) thin films and that was prepared using semi computerized spray pyrolysis technique. The films deposited on glass substrate using such as an ideal value concentration of (0.02)M with a total volume of 100 ml. With substrate temperature was (350 C), spray rate (15 ml/min).The XRD diffraction given polycrystalline nature with Crystal system trigonal (hexagonal axes). The obtained films were irradiated by continuous green laser (532.8 nm) with power 140 mW for different time periods is 10 min,20min and 30min. The result was that the optical properties of cobalt oxide thin films affe