In this study, successive electrocoagulation (EC) and electro-oxidation (EO) processes were used to minimize some of the major pollutants in real wastewater, such as organics (detected by chemical oxygen demand (COD)), and turbidity. The wastewater utilized in the present study was collected from the Midland Refinery Company in Baghdad-Iraq. The performance of the successive batch EC-EO processes was studied by utilizing Graphite and Aluminum (Al) as monopolar anode electrodes and stainless steel (st.st.) as the cathode. The Taguchi experimental design approach was used to attain the best experimental conditions for COD reduction as a major response. Starting from chemical oxygen demand COD of (600 ppm), the effects of current density (C.D.) (10- 20 mA/cm2), pH (4- 10), time (2– 4 h), and NaCl concentration (1.5- 2.5 g/l) on the efficiency of COD reduction were examined. The results indicated that COD reduction increased with increasing C.D., NaCl conc., and electrolysis time and increased exponentially at pH (4). The best conditions for the treatment of this wastewater were: C.D. (20 mA/cm2), pH (4), time (4 h), and NaCl conc. (2.5 g/l). At these conditions, approximately 98.12 % of COD reduction was achieved with electrical energy consumption (ENC) of about 62.04 kWh/m3. The result of analysis of variance (ANOVA) revealed that the C.D. and pH have a higher influence on the performance of organics removal, while the time and NaCl conc. have a minor impact on COD Re%.
The study of the future of the international system currently appears, according to scientific data and existing facts in light of the emergence of international actors from non-states and international informal institutions, to be heading towards a non-polarity system and this trend is fueled by many variables to reduce polarity, and it is expected in the future that the international system will turn into a non-polarity.
This work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.
In this research, hand lay- up technique is used to prepare samples from epoxy resin reinforced with multi- walled carbon nanotubes in different weight fractions (0, 2, 3, 4, 5) wt%. The immersion effect by sodium hydroxide solution (NaOH) at normality (0.3N) for a period of (15 days) on the thermal conductivity of nanocomposites was studied, and compared to natural condition (before immersion). The thermal conductivity of epoxy nanocomposites specimens were carried out using Lee’s disk method. The experimental results showed that thermal conductivity increased with increase weight fraction before and after immersion for all specimens, while the immersion effect leads to decrease thermal conductive values compared to thermal conductivi
... Show MoreZSM-5 zeolite was synthesis under hydrothermal conditions at 175oC. The synthesis parameters have been investigated to find optimum synthesis method. Firstly, the crystallization time has been investigated to find the optimum crystallization time. Also, the ageing time was studied. The morphology, structure, and composition of the synthesized ZSM-5 zeolite were characterized using scanning electron microscopy (SEM), pH meter, viscometer, and X-ray powder diffraction (XRD). The bulk Si/Al ratio of ZSM-5 zeolite was in the range of 9.5—11.7. The synthesized ZSM-5 zeolite with appropriate ageing time could adjust crystal size and degree of the crystallinity. The crystal size of ZSM-5 zeolite obtained at an agei
... Show MorePure cadmium oxide films (CdO) and doped with zinc were prepared at different atomic ratios using a pulsed laser deposition technique using an ND-YAG laser from the targets of the pressed powder capsules. X-ray diffraction measurements showed a cubic-shaped of CdO structure. Another phase appeared, especially in high percentages of zinc, corresponding to the hexagonal structure of zinc. The degree of crystallinity, as well as the crystal size, increased with the increase of the zinc ratio for the used targets. The atomic force microscopy measurements showed that increasing the dopant percentage leads to an increase in the size of the nanoparticles, the particle size distribution was irregular and wide, in addition, to increase the surfac
... Show MoreIn this study two types of extraction solvents were used to extract the undesirable polyaromatics, the first solvent was furfural which was used today in the Iraqi refineries and the second was NMP (N-methyl-2-pyrrolidone).
The studied effecting variables of extraction are extraction temperature ranged from 70 to 110°C and solvent to oil ratio in the range from 1:1 to 4:1.
The results of this investigation show that the viscosity index of mixed-medium lubricating oil fraction increases with increasing extraction temperature and reaches 107.82 for NMP extraction at extraction temperature 110°C and solvent to oil ratio 4:1, while the viscosity index reaches to 101 for furfural extraction at the same extraction temperature and same
Background: Glass ionomers have good biocompatibility and the ability to adhere to both enamel and dentin. However, they have certain demerits, mainly low tensile and compressive strengths. Therefore, this study was done to assess consistency and compressive strength of glass ionomer reinforced by different amount of hydroxyapatite. Materials and Methods: In this study hydroxyapatite materials were added to glass ionomer cement at different ratios, 10%, 15%, 20%, 25% and 30% (by weight). The standard consistency test described in America dental association (ADA) specification No. 8 was used, so that all new base materials could be conveniently mixed and the results would be of comparable value and the compressive strength test described by
... Show More