This work deals with preparation of zeolite 5A from Dewekhala kaolin clay in Al-Anbar region for drying and desulphurization of liquefied petroleum gas. The preparation of zeolite 5A includes treating kaolin clay with dilute hydrochloric acid 1N, treating metakaolin with NaOH solution to prepare 4A zeolite, ion exchange, and formation. For preparation of zeolite 4A, metakaolin treated at different temperatures (40, 60, 80, 90, and 100 °C) with different concentrations of sodium hydroxide solution (1, 2, 3, and 4 N) for 2 hours. The zeolite samples give the best relative crystallinity of zeolite prepared at 80 °C with NaOH concentration 3N (199%), and at 90 and 100°C with NaOH concentration solution 2N (184% and 189%, respectively). Zeolite 5A was prepared by ion exchange of zeolite 4A prepared at 90°C and 2N NaOH concentration with 1.5 N calcium chloride solution at 90 °C and 5 hours, the ion exchange percentage was 66.6%. The formation experiments included mixing the prepared powder of 5A zeolite with different percentages of kaolin clay, citric acid and tartaric acid to form an irregular shape of zeolite granules. Tartaric acid binder gives higher bulk crushing strength than that obtained by using citric acid binder with no significant difference in the surface area. 7.5 weight% tartaric acid binder has the higher bulk crushing strength 206 newton with surface area 267.4 m2/g. Kaolin clay binder with 15 weight% gives the highest surface area 356 m2/g with bulk crushing strength 123 newton, it was chose as the best binder for zeolite 5A. The prepared granules of 5A zeolite were used for the adsorption experiments of H2O, and H2S contaminants from LPG. Different flow rates of LPG (3, 4, and 5 liter/minute) were studied. It was found that H2O is the strongly adsorbed component and H2S is the weakly adsorbed component. The best flow rate in this work for H2O, and H2S adsorption is 5 liter/minute of LPG. The adsorption capacity for H2O was 7.547 g/g and for H2S was 1.734 g/g.
In this work, silver (Ag) self-metallization on a polyimide (PI) film was prepared through autocatalytic plating. PI films were prepared through the solution casting method, followed by etching with potassium hydroxide (KOH) solution, sensitization with tin chloride (SnCl2), and the use of palladium chloride (PdCl2) to activate the surface of PI. Energy-dispersive X-ray analysis (EDX) showed the highest peak in the (Ag) region and confirmed the presence of AgNPs. The diffraction peaks at 2θ = 38.2°, 44.5°, 64.6°, and 78.2° represented the 111, 200, 220, and 311 planes of Ag, respectively. The FT–IR an
... Show MoreFour batches of sertraline HCl microspheres were prepared using a poly (D-L-lactide-co-glycolide) (PLGA) polymer ( Mw. 9, 27, 30 and 83 KDa) as a delivery system. The microspheres were prepared by a dispersion/solvent extraction-evaporation method and characterized for drug loading by UV, particle size by laser diffractometry and surface morphology by scanning electron microscopy (SEM). The in vitro sertraline HCl release was studied. Spherical microspheres with a mean diameter of 21 to 26 µm loaded with 24.6 – 38.2% were produced. The in vitro drug release was shown to be depend on polymer molecular weight and also on the drug loading. Differential scanning calorimetry (DSC) was employed to investigate the physical state
... Show MoreThe grapheme Flakes were prepared by reduction graphite oxide which was prepared by Hummer’s method. X-ray diffraction (XRD) pattern showed that the graphene oxide have a sharp peak at (001) with d-spacing d001= 7.4Å at angle 2ϴ=11.85˚and graphene has broad peak at (002) with d-spacing d002=3.4Å at angle 2ϴ= 25.72˚ with lattice constant (a=2.47 Å). The particle size was calculated by using equation Debye - Scherer and Williamson - Hall equations, Scanning electron microscopy examination and particle size analyzer proved that the graphene Flakes were in nano size. Also the surface area of nanoparticles showed a value 270 m2/g . The micrographs of (scanning electron microscopy) showed that graphene oxide has a fluffy aggregation a
... Show MorePolyimide/MWCNTs nanocomposites have been fabricated by solution mixing process. In the present study, we have investigated electrical conductivity and dielectric properties of PI/MWCNT nanocomposites in frequency range of 1 kHz to 100 kHz at different MWCNTs concentrations from 0 wt.% to 15 wt.%. It has been observed that the electrical conductivity and dielectric constants are enhanced significantly by several orders of magnitude up to 15 wt.% of MWCNTs content. The electrical conductivity increases as the frequency is increased, which can be attributed to high dislocation density near the interface. The rapid increase in the dielectric constant at a high MWCNTs content can be explained by the form
Zinc Oxide (ZnO) is probably the most typical II-VI
semiconductor, which exhibits a wide range of nanostructures. In
this paper, polycrystalline ZnO thin films were prepared by chemical
spray pyrolysis technique, the films were deposited onto glass
substrate at 400 °C by using aqueous zinc chloride as a spray
solution of molar concentration of 0.1 M/L.
The crystallographic structure of the prepared film was analyzed
using X-ray diffraction; the result shows that the film was
polycrystalline, the grain size which was calculated at (002) was
27.9 nm. The Hall measurement of the film studied from the
electrical measurements show that the film was n-type. The optical
properties of the film were studied using
In this research four steps of the new derivatives of Naproxen drug have been made which are known as a high medicinal effectiveness; the first step involved converting Naproxen into the corresponding ester (A) by reaction Naproxen with methanol absolute in presence H2SO4. While the second step involved treatment methyl Naproxen ester (A) with hydrazine hydrate 80% in presence of ethanol .The third reaction requires synthesis of Schiff bases (C1-C10) by condensation. of Naproxen hydrazide (B) with many substituted aromatic aldehydes . Finally, the fourth step synthesized new tetrazole derivatives ( D1- D10) by the reaction of the prepared Schiff bases (in the third step) with Sodium azide in THF as a solvent .The prepared compounds wer
... Show MoreMansuriya Gas field is an elongated anticlinal structure aligned from NW to SE, about 25 km long and 5-6 km wide. Jeribe formation is considered the main reservoir where it contains condensate fluid and has a uniform thickness of about 60 m. The reservoir is significantly over-pressured, (TPOC, 2014).
This research is about well logs analysis, which involves the determination of Archie petrophysical parameters, water saturation, porosity, permeability and lithology. The interpretations and cross plots are done using Interactive Petrophysics (IP) V3.5 software.
The rock parameters (a, m and n) values are important in determining the water saturation where (m) can be calcul
... Show MoreIn the present work, it had been measured the concentration of radon gas (CRn) for (10) samples of cement used in constructions before and after painting them using enamel paint, purchased from the local markets, to see the extent of its ability to reduce emissions of Rn-222 in the air. These samples were obtained from different sources available in the local markets in Baghdad and other provinces. The measurements were done by the American-made detector (RAD7). The results showed that the highest CRn in the air emitted from cement samples after coating was in the cement sample (Iranian origin) where the concentration was (58.27 Bq/m3) while the lowest CRn was found in building material samples
... Show MoreIn this work, ZnO nanostructures for powder ZnO were synthesized by Hydrothermal Method. Size and shape of ZnO nanostructureas can be controlled by change ammonia concentration. In the preparation of ZnO nanostructure, zinc nitrate hexahydrate [Zn(NO3)2·6H2O] was used as a precursor. The structure and morphology of ZnO nanostructure have been characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray diffraction (XRD). The synthesized ZnO nanostructures have a hexagonal wurtzite structure. Also using Zeta potential and Particle Size Analyzers and size distribution of the ZnO powder