In this paper, we propose a new and efficient ferroelectric nanostructure metal oxide lithium niobate [(Li1.075Nb0.625Ti0.45O3), (LNTO)] solid film as a saturable absorber (SA) for modulating passive Q-switched erbium-doped fiber laser (EDFL). The SA is fabricated as a nanocomposite solid film by the drop-casting process in which the LNTO is planted within polyvinylidene fluoride-trifluoroethylene [P(VDF-TrFE)] as host copolymer. The optical and physical characteristics of the solid film are experimentally established. The SA is incorporated within the cavity of EDFL to examine its capability for producing multi-wavelength laser. The experimental results proved that a multi-wavelength laser is produced, where stable four lines with central wavelengths at 1529.5, 1530.5, 1531.5, and 1532 nm are observed on the laser spectrum at 157 mW pumped power. Furthermore, at maximum available pumped power (157 mW), laser pulses are running with a rate of 178 kHz and pulse width of 2.64 μs. The output power of 3.7 mW is attained at pumped power of 157 mW. The result proved that the LNTO-SA could be a potential candidate for generating multi-wavelength passive Q-switched fiber laser pulses.
Spin coating technique has been applied in this work to prepared Xerogel films doped with Rhodamine 6G laser dyes. The solid host of laser dye modifies its spectroscopic properties with respect to liquid host. During the spin coating process the dye molecules suffer from changing their environment. The effects of three parameters were studied here: the spinning speed, multilayer coating and formaldehyde addition
The effect of 410nm with 100 mW output power and one centimetre spot size (0.128 W/cm2 power density) Diode laser irradiation at different exposure times on the growth of Gram-negative Pseudomonas aeruginosa and Gram-positive Staphylococcus aureus was evaluated. Seventy swap samples were collected from burn and infected wounds of 35 patients admitted to the burn-wound unit in Al-Yarmouk Teaching Hospital in Baghdad during the period from December 2014 to February 2015. These bacteria were isolated and identified depending on their growth on selective media, cultural characteristics, Gram stain morphology and biochemical tests and finally were confirmed by Vitek 2 compact system test .Susceptibility of bacterial isolates to 15antibiotics
... Show MoreIn this work, ZnS thin films have been deposited by developed laser deposition technique on glass substrates at room temperature. After deposition process, the films were annealed at different temperatures (200ºC , 300 ºC and 400ºC ) using thermal furnace.The developed technique was used to obtain homogeneous thin films of ZnS depending on vaporization of this semiconductor material by continuous CO2 laser with a simple fan to ensure obtaining homogeneous films. ZnS thin films were annealed at temperature 200ºC, 300 ºC and 400ºC for (20) minute in vacuum environment. Optical properties of ZnS thin film such as absorbance, transmittance, reflectance, optical band gap, refractive index extinction coefficient and absorption coefficien
... Show MoreIn this paper deals with the effect laser irradiation on the optical properties of cobalt oxide (CoO2) thin films and that was prepared using semi computerized spray pyrolysis technique. The films deposited on glass substrate using such as an ideal value concentration of (0.02)M with a total volume of 100 ml. With substrate temperature was (350 C), spray rate (15 ml/min).The XRD diffraction given polycrystalline nature with Crystal system trigonal (hexagonal axes). The obtained films were irradiated by continuous green laser (532.8 nm) with power 140 mW for different time periods is 10 min,20min and 30min. The result was that the optical properties of cobalt oxide thin films affe
A novel ligand ((1E)-(2-(4-fluorobenzylidene)amino)methyl) phenyl)diazenyl)-1,3,7-trimethyl-3,7-dihydro-1H-purine-2,6-dione (4-FADPD) was synthesized via the azotization reaction of 2-aminobenzylamine with caffeine, and the resultant compound was condensed with 4-fluorobenzaldehyde to form a newly azo-Schiff base ligand. Its complexes with Cu(II), Ag(I), and Au(III) were synthesized. The results of multi-identifications, including XRD, elemental analysis (C.H.N), UV-vis spectroscopy, FTIR, and 1H-NMR, were used to propose the suggested structures using molar conductivity measurements. These data were utilized to propose appropriate geometric configurations for all complexes. The azo-Schiff base ligand coordinates toward the Cu(II) i
... Show MoreIn this paper, silicon carbonitried thin films were prepared by the method of photolysis of the silane (SiH4) and ethylene (C2H4) gases, with and without ammonia gas (NH3), which is represented by the ratio between the (PNH3) and (PSiH4 + PC2H4 + PNH3), (which assign by the letter X), X has the values (0, 0.13, 0.33). This method carried out by using TEA-CO2 laser, on glass substrate at (375 oC), deposition rate (0.416-0.833) nm/pulse thin film thickness of (500-1000) nm. The optical properties of the films were studied by using Absorbance and Transmittance spectrums in wavelength range of (400-1100) nm, the results showed that the electronic transitions is indirect and the energy gap for the SiCN films increase with increasing of nitrog
... Show MoreThe goal of this investigation is to prepare zinc oxide (ZnO) nano-thin films by pulsed laser deposition (PLD) technique through Q-switching double frequency Nd:YAG laser (532 nm) wavelength, pulse frequency 6 Hz, and 300 mJ energy under vacuum conditions (10-3 torr) at room temperature. (ZnO) nano-thin films were deposited on glass substrates with different thickness of 300, 600 and 900 nm. ZnO films, were then annealed in air at a temperature of 500 °C for one hour. The results were compared with the researchers' previous theoretical study. The XRD analysis of ZnO nano-thin films indicated a hexagonal multi-crystalline wurtzite structure with preferential growth lines (100), (002), (101) for ZnO nano-thin films with different thi
... Show MoreThin films of (CdO)x (CuO)1-x (where x = 0.0, 0.2, 0.3, 0.4 and 0.5) were prepared by the pulsed laser deposition. The CuO addition caused an increase in diffraction peaks intensity at (111) and a decrease in diffraction peaks intensity at (200). As CuO content increases, the band gap increases to a maximum of 3.51 eV, maximum resistivity of 8.251x 104 Ω.cm with mobility of 199.5 cm2 / V.s, when x= 0.5. The results show that the conductivity is ntype when x value was changed in the range (0 to 0.4) but further addition of CuO converted the samples to p-type.