A ‘locking-bolt’ demountable shear connector (LBDSC) is proposed to facilitate the deconstruction and reuse of steel-concrete composite structures, in line with achieving a more sustainable construction design paradigm. The LBDSC is comprised of a grout-filled steel tube and a geometrically compatible partially threaded bolt. The latter has a geometry that ‘locks’ the bolt in compatible holes predrilled on the steel flange and eliminates initial slip and construction tolerance issues. The structural behaviour of the LBDSC is evaluated through nine pushout tests using a horizontal test setup. The effects of the tube thickness, strength of concrete slab, and strength of infilled grout on the shear resistance, initial stiffness, and ductility of the LBDSC are assessed. The experimental results show that the LBDSC can achieve higher shear resistance and similar initial stiffness as compared to traditional welded studs. In addition, all tested LBDSCs exhibited slip capacities ranging from 14 to 32 mm and can be classified as ductile shear connectors according to Eurocode 4. A detailed finite element model was also created and found to be reliable to reproduce the experimental behaviour. Parametric studies were subsequently conducted using the validated model to study further parameters and generalise the experimental results. Due to the specific test setup, non-negligible uplift forces were generated in the connector and the potential implications are discussed.
This study investigated the shear performance of concrete beams with GFRP stirrups vs. traditional steel stirrups. Longitudinal glass fiber‐reinforced polymer (GFRP) bars were used to doubly reinforce the tested beams at both the top and bottom of their cross sections. To accomplish this, several stirrup spacings were provided. Eight beam specimens, measuring 300 × 250 × 2400 mm, were used in an experimental program to test under a two‐point concentrated load with an equal span‐to‐depth ratio until failure. Four beams in Group I have standard mild steel stirrups of 8 mm diameter, while four beams in Group II have GFRP stirrups with the same adopted diameter. The difference betwe
Background: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreItem Difficulty and Item Discrimination Coefficient for School and College Ability Tests (SCAT) Advanced Form in Classical Test Theory (CTT) and Item Response Theory (IRT) and the Correlation among Them Mohammad moqasqas Haifa T. Albokai Assistant Professor of Measurement and Evaluation Associate Professor of Measurement and Evaluation College of Education, Taibah University The aim of this study was to study the item difficulty and item discrimination of the SCAT (advance form) with CTT, and IRT, and to study the correlation among them. To do this, the researchers used the data of their previous study, which conducted in (2011). It consisted of (3943) subject. Then, they used two-statistical programs (TAP, Bilog-MG-3) to obtain the item
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreBackground: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three
... Show MoreBackground: This study was aimed to investigate the effect of three lingual button (Nickel free / rectangular base, Nickel free / round base and Composite) and bonding environment, wet and dry enamel surface, on: the shear bond strength (SBS) of light and self-cured Resin Modified Glass Ionomer Cements, and the debonding failure sites. Materials and method: One hundred twenty no-carious, free of cracks maxillary first premolar teeth were selected. Three types of orthodontic lingual buttons were used in this study: Nickel free / rectangular base, Nickel free / round base and Composite buttons. The teeth were divided into two groups of sixty teeth each. One group was used for testing the chemically cured GC Fuji Ortho Resin modified Glass Io
... Show MoreBackground: In this study we evaluate the effect of plasma treatment (oxygen and argon) gas in two different exposure times on the surface of heat cure and light cure acrylic resin. Materials and method: 100 specimens of heat cure and light cure acrylic resin were fabricated. The measurements of the samples were (75mm, 25mm and 4.5mm) length, width and depth respectively with stopper of 3mm depth. Two types of gas used oxygen and argon in (5,10) min by using (DC-glow discharge plasma device) then we apply cold cure soft lining material, with the help of Instron machine we test the shear stress value. Results: A highly significant effect after argon and oxygen gases treatment in both 5 and 10 min exposure times on shear bond strength to soft
... Show More