The construction of highly safe and durable buildings that can bear accident damage risks including fire, earthquake, impact, and more, can be considered to be the most important goal in civil engineering technology. An experimental investigation was prepared to study the influence of adding various percentages 0%, 1.0%, and 1.5% of micro steel fiber volume fraction (Vf) to reactive powder concrete (RPC)—whose properties are compressive strength, splitting tensile strength, flexural strength, and absorbed energy—after the exposure to fire flame of various burning temperatures 300, 400, and 500 °C using gradual-, foam-, and sudden-cooling methods. The outcomes of this research proved that the maximum reduction in mechanical properties is detected in case of 0% addition at burning temperature of 500 °C using sudden cooling to be 63.90%, 55.77% and 53.8% for compressive, splitting tensile, and flexural strength, respectively, while using 1.5% produced a modification in compressive strength, splitting tensile strength, and flexural strength to 6.67%, 4.15%, and 7.00% respectively, and 7.10 kN·mm for the absorbed energy for gradual cooling at 300 °C. From the results, the adopted cooling methods can be ordered according to their negative influence by sudden, foam, and gradual, while the optimum percentage of (Vf) is 1.5% when burning at 300 °C for all methods of cooling. 1.0% is considered the optimum percentage for all burning temperatures that exceed 400 °C using sudden-cooling method.
This paper demonstrates an experimental and numerical study on the behavior of reinforced concrete (RC) columns with longitudinal steel embedded tubes positioned at the center of the column cross-section. A total of 12 pin-ended square sectional columns of 150 × 150 mm having a total height of 1400 mm were investigated. The considered variables were the steel tube diameters of 29, 58, and 76 mm and the load eccentricity (0, 50, and 150) mm. Accordingly, these columns were divided into three groups (four columns in each group) depending on the load eccentricity (e) to column depth (h) ratio (e/h = 0, 1/3, and 1). For each group, one column was solid (reference), and the other three columns contained steel tubes with hollow rat
... Show MoreThe excessive permanent deformation (rutting) in asphalt-concrete pavements resulting from frequent repetitions of heavy axle loads is studied in this paper. Rutting gradually develops with additional load applications and appears as longitudinal depressions in the wheel path. There are many causes of the rutting of asphalt roads, such as poor asphalt mixing and poor continuous aggregate gradation. All factors affecting the mixture resistance to permanent deformation must be discussed, and all must be properly considered to reduce the rutting propensity of asphalt-aggregate mixtures. In this study, several mixtures were produced with the most common techniques in rutting resistance (using the most effective additives for each mixture), and
... Show MoreIn this work, nanostructure aluminum oxide thin films were deposited on glass substrates using a direct current (DC) magnetic reactive sputtering (MRS) technique. A gaseous mixture of argon and oxygen at different mixing ratios was used to synthesize Al2O3 nanoparticles. After extracting Al2O3 powder from the glass substrate, X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), and energy-dispersive spectroscopy (EDS) were used to analyze the structural and morphological properties of the synthesized thin films. The effect of deposition time on the spectral properties, as well as on the size of the nanoparticles, was determined.
In the present study, advanced oxidation treatment, the TiO2 /UV/H2O2 process was applied to decolorisation of the reactive yellow dyes in aqueous solution. The UV radiation was carried out with a 6 W low-pressure mercury lamp. The rate of color removal was studied by measuring the absorbency at a characteristic wavelength. The effects of H2O2 dosage, dye initial concentration and pH on decolorisation kinetics in the batch photoreactor were investigated. The highest decolorisation rates were observed (98.8) at pH range between 3 and 7. The optimal levels of H2O2 needed for the process were examined. It appears that high levels of H2O2 could reduce decolori
... Show MoreDrastic threat to the natural system is caused by the uncontrolled release of synthetic pollutants, including azo dyes. This study centered on the decolorization and biodegradation of water soluble azo dye reactive blue (RB) in a batch mode sequential anaerobic-aerobic processes. A local sewage treatment plant was the source where activated sludge was collected to be used as non-adapted mixed culture with both free and the alginate immobilized cells for RB biodegradation. Under anaerobic conditions, the free and immobilized mixed cells were proved to completely decolorize 10 mg/ L of RB within 20 and 30 h, respectively. Alginate- immobilized mixed cells, resulted in 88%, 87%, and 87% maximum COD removals with samples con
... Show MoreThis study concerns the removal of a trihydrate antibiotic (Amoxicillin) from synthetically contaminated water by adsorption on modified bentonite. The bentonite was modified using hexadecyl trimethyl ammonium bromide (HTAB), which turned it from a hydrophilic to a hydrophobic material. The effects of different parameters were studied in batch experiments. These parameters were contact time, solution pH, agitation speed, initial concentration (C0) of the contaminant, and adsorbent dosage. Maximum removal of amoxicillin (93 %) was achieved at contact time = 240 min, pH = 10, agitation speed = 200 rpm, initial concentration = 30 ppm, and adsorbent dosage = 3 g bentonite per 1L of pollutant solution. The characterization of the adsorbent, modi
... Show More