In this study, a Hydroxyapatite (HA) coating was prepared on a titanium implant by an electrochemical deposition process. The titanium pre-treatment by anodizing in 1.65 mol/L sulfuric acid with (10V) at room temperature. The deposition was all conducted at a constant voltage of 6.0 V, for 1 h at room temperature. The coatings thus prepared were characterized with Fourier transform infrared spectroscopy (FTIR) and thickness of the coated layer.The electrochemical deposition of HA occurred on the titanium as a cathode. Coated titanium by HA after anodizing revealed a good corrosion protection efficiency even at a temperature ranged (293-323) K in artificial saliva. Activation energy and pre-exponential factor (kinetic parameters) were calculated and discussed. Also, thermodynamic values ΔG and ΔH were calculated and it shows that corrosion reaction was non-spontaneous and exothermic in nature before treatment but after anodizing the corrosion reaction become endothermic.
Titanium alloy (Ti-6Al-4V or Gr.23) was widely used as a dental alloy. In the current study, polymerization of eugenol (PE) on Gr.23 titanium alloys was conducted by an electrochemical process before and after being treated by Micro Arc Oxidation (MAO). The formed films were characterized by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). The corrosion behavior of Gr.23 alloy in an artificial saliva environment at a temperature range of 293–323 K has been studied and assessed by means of electrochemical polarization and impedance spectroscopy techniques. Three cases are taken into consideration; bare Gr.23, Gr.23 coated by PE, and Gr.23 coated by PE after MAO treatment. The maxi
... Show MoreIraq has a huge network of pipelines, transport crude oil and final hydrocarbon products as well as portable water. These networks are exposed to extensive damage due to the underground corrosion processes unless suitable protection techniques are used. In this paper we collect the information of cathodic protection for pipeline in practical fields (Oil Group in Al Doura), to obtain data base to understand and optimize the design which is made by simulation for the environmental factors and cathodic protection variables also soil resistivity using wenner four terminal methods for survey sites; and soil pH investigations were recorded for these selected fields were within 7-8, and recording the anodes voltage and its related currents for
... Show MoreAbstract: The aim of this study was to evaluate the effect of bone density value in Hounsfield unit derived from cone beam computed tomography (CBCT), and implant dimensions in relation to implant stability parameters namely the resonance frequency analysis and the insertion torque (IT) value. It included 24 patients who received 42 dental implants (DI). The bone density of the planned implant site was preoperatively measured using cone beam computed tomography. The implant stability was measured using Osstell implant stability quotient (ISQ). The ISQ values were recorded immediately postoperatively and after 16 weeks. The IT value was categorized as 35 N/cm or > 35 N/cm. The mean (standard deviation) primary stability was 79.58 (5.27) ISQ,
... Show MoreBackground: Preparation of platelet-rich fibrin (PRF) is a simple, low cost and minimally invasive method to obtain a natural concentration of autologous growth factors that is widely used to accelerate soft and hard tissue healing, thus, PRF is used in different fields of medicine. The aim of this study was to evaluate the effect of local application PRF on stability of dental implants. Materials and methods: nineteen healthy patients with adequate alveolar bone with two or more adjacent missing teeth and/or bilaterally symmetric to the midline (split-mouth design) missing teeth participated in this study. Each patient received at least two dental implants (Dentium Co., Korea). After surgical preparation of the implant sockets, the PRF was
... Show MoreIn this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in
In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in
This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,
... Show MoreThis paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,
... Show More