Study the properties of Cu2Se thin films for optoelectronic applications
...Show More Authors

Copper selenide (Cu2Se) thin films were prepared by thermal evaporation at RT with thickness 500 nm. The heat-treating for (400 &500) K for the absorber layer has been investigated. This research includes, studying the structural properties of X-ray diffraction (XRD) that show the Cu2Se thin film (Cubic) and has a polycrystalline orientation prevalent (220). Moreover, studying the effect of annealing on their surface morphology properties by using Atomic Force Microscopy AFM. Optical properties were considered using the transmittance and absorbance spectra had been recorded when wavelength range (400 - 1000) nm in order to study the absorption coefficient and energy gap. It was found that these films had allowed direct transition optical band gap which decreases with the increasing effect of annealing, while it increasing with the increase in the annealing temperature at all ratio UV-Visible transmission spectrum. Hall Effect results presented that all thin films have P-type. It is quite possible that the heterojunction (p-Cu2Se/n-Si) solar cell device is a buried. The illumination current- voltage (I-V) characteristics showed that the solar cell, with (t=500 nm and T=500 K ) has highest efficiency (η =1.4 %).

Scopus Clarivate Crossref
View Publication
Publication Date
Sun Mar 02 2008
Journal Name
Baghdad Science Journal
Study the Band Energy Structure and Absorption Coefficient for PbSe Thin Films
...Show More Authors

The PbSe alloy was prepared in evacuated quarts tubs by the method of melt quenching from element, the PbSe thin films prepared by thermal evaporation method and deposited at different substrate temperature (Ts) =R.T ,373 and 473K . The thin films that deposited at room temperature (R.T=303)K was annealed at temperature, Ta= R.T, 373 and 473K . By depended on D.C conductivity measurements calculated the density of state (DOS), The density of extended state N(Eext) increases with increasing the Ts and Ta, while the density of localized state N(Eloc) is decreased . We investigated the absorption coefficient (?) that measurement from reflection and transmission spectrum result, and the effect of Ts and Ta on it , also we calculated the tai

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sun Mar 05 2017
Journal Name
Baghdad Science Journal
Preparation and study of the structural and optical properties of Bi2S3 thin films by Spray pyrolysis method
...Show More Authors

In this research Bi2S3 thin films have been prepared on glass substrates using chemical spray pyrolysis method at substrate temperature (300oC) and molarity (0.015) mol. Structural and optical properties of the thin films above have been studied; XRD analysis demonstrated that the Bi2S3 films are polycrystalline with (031) orientation and with Orthorhombic structure. The optical properties were studied using the spectral of the absorbance and transmission of films in wavelength ranging (300-1100) nm. The study showed that the films have high transmission within the range of the visible spectrum. Also absorption coefficient, extinction coefficient and the optical energy gap (Eg) was calculated, found that the film have direct ener

... Show More
View Publication Preview PDF
Scopus Crossref
Publication Date
Fri Jan 01 2016
Journal Name
International Journal Of Innovative Research In Science, Engineering And Technolog
Effect Of heat Treatment On The Optical Properties Of CuInSe2 Thin Films
...Show More Authors

CuInSe2(CIS) thin films have been prepared by use vacuum thermal evaporation technique, of thickness750 nm with rate of deposition 1.8±0.1 nm/sec on glass substrate at room temperature and pressure (10-5) mbar. Heat treatment has been carried out in the range (400-600) K for all samples. The optical properties of the CIS thin films are been studied such as (absorption coefficient, refractive index, extinction coefficient, real and imaginary dielectric constant) by determined using Measurement absorption and transmission spectra. Results showed that through the optical constants we can make to control it are wide applications as an optoelectronic devices and photovoltaic applications.

View Publication
Publication Date
Thu Jan 07 2016
Journal Name
International Journal Of Innovative Research In Science, Engineering And Technology
Effect Of heat Treatment On The Optical Properties Of CuInSe2 Thin Films
...Show More Authors

CuInSe2 (CIS)thin films have been prepared by use vacuum thermal evaporation technique, of 750 nm thickness, with rate of deposition 1.8±0.1 nm/sec on glass substrate at room temperature and pressure (10-5) mbar. Heat treatment has been carried out in the range (400-600) K for all samples. The optical properties of the CIS thin films are been studied such as (absorption coefficient, refractive index, extinction coefficient, real and imaginary dielectric constant)by determined using Measurement absorption and transmission spectra. Results showed that through the optical constants we can made to control it is wide applications as an optoelectronic devices and photovoltaic applications.

Preview PDF
Publication Date
Thu Apr 13 2017
Journal Name
Journal Of Multidisciplinary Engineering Science Studies (jmess)
The Effect Of Thickness On Some Physical Properties Of CdSe Thin Films
...Show More Authors

Publication Date
Mon Jan 01 2018
Journal Name
Ibn Al-haitham Journal For Pure And Applied Science
Investigation of the Structural, Optical and Electrical Properties of AgInSe2 Thin Films
...Show More Authors

Publication Date
Sun Sep 05 2010
Journal Name
Baghdad Science Journal
Studying the effect of annealing on some electrical and optical properties for thin CdS , CdS:In films
...Show More Authors

In the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .

View Publication Preview PDF
Crossref
Publication Date
Sat Jan 01 2011
Journal Name
Iraqi Journal Of Physics
Study of annealing effect on some Optical Properties of CuIn(SexTe1-x)2 Thin Films
...Show More Authors

The optical properties for the components CuIn(SexTe1-x)2 thin films with both values of selenium content (x) [0.4 and 0.6] are studied. The films have been prepared by the vacuum thermal evaporation method with thickness of (250±5nm) on glass substrates. From the transmittance and absorbance spectra within the range of wavelength (400-900)nm, we determined the forbidden optical energy gap (Egopt) and the constant (B). From the studyingthe relation between absorption coefficient (α) photon energy, we determined the tails width inside the energy gap.
The results showed that the optical transition is direct; we also found that the optical energy gap increases with annealing temperature and selenium content (x). However, the width of l

... Show More
View Publication Preview PDF
Publication Date
Mon Apr 01 2002
Journal Name
Renewable Energy
The optoelectronic properties of CdSe:Cu photoconductive detector
...Show More Authors

View Publication
Scopus (22)
Crossref (20)
Scopus Clarivate Crossref
Publication Date
Tue Jan 08 2019
Journal Name
Iraqi Journal Of Physics
X- ray diffraction and dielectric properties of PbSe thin films
...Show More Authors

Lead selenide PbSe thin films of different thicknesses (300, 500, and 700 nm) were deposited under vacuum using thermal evaporation method on glass substrates. X-ray diffraction measurements showed that increasing of thickness lead to well crystallize the prepared samples, such that the crystallite size increases while the dislocation density decreases with thickness increasing. A.C conductivity, dielectric constants, and loss tangent are studied as function to thickness, frequency (10kHz-10MHz) and temperatures (293K-493K). The conductivity measurements confirm confirmed that hopping is the mechanism responsible for the conduction process. Increasing of thickness decreases the thermal activation energy estimated from Arhinus equation is

... Show More
View Publication Preview PDF
Crossref (2)
Crossref