In this work, the effect of anodizing duration on the morphology and photoelectrochemical properties of TiO2 nanotubes arrays (NTAs) has been investigated The samples were characterized by X-ray diffraction (XRD) and energy dispersive X-ray (EDX) to characterize their crystalline structure and compositional. Surface morphological and their dimensional variation was examined by field emission scanning electron microscopy (FESEM). The anodizing duration played a significant role in the formation of TiO2 nanotubes arrays. Moreover, the photoelectrochemical properties (PEC) were studied through photocurrent measurements. Optimum anodizing duration of 60 min at 40 V exhibited maximum photocurrent of 0.03 mA cm-2 under illumination of halogen light.
In this study, a theoretical scenario has been used to calculate the electronic current in sensitizer N3 molecule contact to TiO2 semiconductor for electrons in functional solar cells. It is known to play an important role on the compute the eficiency of solar cell. Some parameters of electronic current such as the transition energy, driving force energy, barrier height coupling overlapping values are determined. Transition energy is a necessary parameter to calculate the electronic current in solar cell with using wide polarity solvents Acetic acid, 2-Methoxyethanol, 1-Butanol, Methyl alcohol, chloroform, N,N-Dimethylacetamide and Ethyl alcohol via the quantum donor-acceptor system. Here, we show the results of transition energy can be var
... Show More(3) (PDF) Theoretical calculation of the electronic current at N3 contact with TiO2 solar cell devices. Available from: https://www.researchgate.net/publication/362780274_Theoretical_calculation_of_the_electronic_current_at_N3_contact_with_TiO2_solar_cell_devices [accessed May 01 2023].
The investigation of the effect of tempering on thermal analysis of
Al-Ti-Si alloy and its composites with MgO and SiC particles was
performed. Thermal analysis was performed before and after
tempering by DSC scan. Optical microscopy was used to identify the
phases and precipitations that may be formed in base alloy and
composites. X-ray diffraction test indicated that the Al3Ti is the main
phase in Al-Ti-Si alloy in addition to form Al5Ti7Si12 phase. Some
chemical reactions can be occurred between reinforcements and
matrix such as MgO.Al2O3 in Al-Ti/MgO, and Al4C3 and Al(OH)3 in
Al-Ti/SiC composite. X-ray florescence technique is used to
investigate the chemical composition of the fabricated specimens.
H
In this paper, the density of state (DOS) at Fe metal contact to Titanium dioxide semiconductor (TiO2) has been studied and investigated using quantum consideration approaches. The study and calculations of (DOS) depended on the orientation and driving energies. was a function of TiO2 and Fe materials' refractive index and dielectric constant. Attention has focused on the effect of on the characteristic of (DOS), which increased with the increasing of refractive index and dielectric constant of Fe metal and vice versa. The results of (DOS) and its relation with and values of system have been discussed. As for contact system is increased, (DOS) values increased at first, but the relation is disturbed later and transforms into an inve
... Show MoreIn order to scrutinize the impact of the decoration of Sc upon the sensing performance of an XN nanotube (X = Al or Ga, and XNNT) in detecting sarin (SN), the density functionals M06-2X, τ-HCTHhyb, and B3LYP were utilized. The interaction of the pristine XNNT with SN was a physical adsorption with the sensing response (SR) of approximately 5.4. Decoration of the Sc metal into the surface of the AlN and GaN led to an increase in the adsorption energy of SN from −3.4 to −18.9, and −3.8 to −20.1 kcal/mol, respectively. Also, there was a significant increase in the corresponding SR to 38.0 and 100.5, the sensitivity of metal decorated XNNT (metal@XNNT) is increased. So, we found that Sc-decorating more increases the sensitivity of GaNN
... Show MoreIn this work, an anti-reflection coating was prepared in the region (400-1000) nm of wavelength, with a double layer of silicon dioxide (SiO2) as an inner layer and the second layer of the mixture (SiO2) and titanium dioxide (TiO2) with certain ratios, as an outer layer using the chemical spraying method with a number of 6 sprays of layer SiO2 and 12 sprays of layer SiO2 - TiO2. Using the method of chemical spraying deposited on the glass as a substrate with a different number of sprays of SiO2, and a fixed number of TiO2-SiO2. The optical and structural properties were determined using UV-Vis spectroscopy and atomic force mi
... Show More