Herein, the interfacial polymerization method has been used for the synthesis of PPy/NaVO3 composites with different compositions of NaVO3 (10 %, 20 %, 30 %, 40 % and 50 %) as an efficient electrode material for supercapacitors. The successful formation and composition of the as-prepared composites (PV1-PV5) were confirmed by FTIR, XRD, EDX, and SEM analysis. The electrochemical properties were investigated by cyclic voltammetry (CV), galvanometric charge–discharge measurement (GCD), and electrochemical impedance spectroscopy (EIS) in 0.5 M H2SO4 electrolyte. As compared to other, the PV4 composite exhibit excellent specific capacitance of 391 F g−1 at a current density of 0.75 A/g with good cycling stability of ∼59 % after 1000 cycles. Furthermore, the PV4 composite also shows a high specific energy density of 14 Wh kg−1 and a specific power density of 150 W kg−1. The excellent electrochemical performance of PPy/NaVO3 composites (PV1-PV5) was attributed to the synergistic effect of conducting PPy and NaVO3 which provides the effective surface area for the efficient storage of ions and transfer of electrons and ions on the surface of the electrode. Thus, these excellent electrochemical performances reflect and suggest the practical application of PV4 electrode material for future high-energy–density supercapacitors.
Experimental investigations had been done in this study to demonstrate the effect of natural particles used as a reinforcement material to unsaturated polyester resin. The tensile test and water absorption were investigated according to (ASTM D638) and (ASTM D570), respectively. The influence of sunflower husk and pomegranate husk particles, used as a reinforcement material, on the tensile strength, Young's modulus and water absorption with different weight fraction (3%, 7% and 10%) and particle grain size (50µm, 100 µm and 150 µm), has been investigated. The water absorption of polymer composites was studied by measuring the specimen weight before and after immersion in water for one hundred days. In the experiments of tensile test,
... Show More 
Aquatic Oligochaeta is an important group of Macroinvertebrates that has been very remarkable as bioindicators for assessing water pollution and determining its degree in water bodies. Hence, the idea of the current study aims at studying the impact of Baghdad effluents on the Tigris River by using oligochaetes community as bioindicators . For this purpose, four sites along the inside of Baghdad has been chosen. Site S1 has been located upstream, site S2 and S3 has been at midstream and site S4 at the downstream of the River.This investigation has used different types of biological indicators, including the percentage of oligochaeta within benthic invertebrates, which ranged from 49.2-51.28%. The highest percentage of the tubificid w
... Show MoreIn this paper the reinforced materials manufactured from steel continues fibers are used in Aluminum matrix to build a composite material. Most of researches concentrated on reinforced materials and its position in the matrix according to its size and distribution, and their effects on the magnitude of different kinds of the stresses, so this paper presents and concentrate on the geometrical shape of reinforced material and its effects on the internal stresses and strains on the composite strength using FEM as a method for analysis after loaded by certain force showing the deference magnitudes of stresses according to the different geometrical shapes of reinforced materials.
This paper investigated the fatigue life behavior of two composite materials subjected to different times of shot peening (2, 4 and 6 min).The first material prepared from unsaturated polyester with E-glass reinforcement by 33% volume fraction. While, the second one was prepared from unsaturated polyester with aluminum powder by2.5% volume fraction. The experimental results showed that the improvement in endurance limit was obtained (for the first material) at 2, 4 and 6 min shot peening times where the percentage of maximum improvement was 25% at shot peening time of 6 min. While, the endurance limit of the second material decreased at shot peening times of 2, 4 and 6 min where the percentage of maximum reduction was 29 % at shot peenin
... Show More