Experimental investigations had been done in this study to demonstrate the effect of natural particles used as a reinforcement material to unsaturated polyester resin. The tensile test and water absorption were investigated according to (ASTM D638) and (ASTM D570), respectively. The influence of sunflower husk and pomegranate husk particles, used as a reinforcement material, on the tensile strength, Young's modulus and water absorption with different weight fraction (3%, 7% and 10%) and particle grain size (50µm, 100 µm and 150 µm), has been investigated. The water absorption of polymer composites was studied by measuring the specimen weight before and after immersion in water for one hundred days. In the experiments of tensile test, all specimens loading was performed with (50KN) operating at a crosshead speed of 10 mm/min. It is observed that the addition of sunflower husk up to 10% and pomegranate husk particles up to 7% as reinforcement materials to polyester resin, leads to increase the tensile strength and Young's modulus of the composite material prepared and the use of sunflower husk as a reinforcement material increased the tensile strength, Young's modulus and water absorption were better than pomegranate husk at the same percentage of addition. The decrease in reinforcement material grain size led to increase the tensile strength, Young's modulus and water absorption. Therefore, all the best result seen in composites containing reinforcement material with (50µm). Finally, the best result obtained in tensile strength, Young's modulus and water absorption were with the addition of 10% sunflower husk as a reinforcement material to polyester resin.
Abstract
Binary polymer blend was prepared by mechanical mixing method of unsaturated polyester resin with Nitrile Butadiene Rubber (NBR) with different weight ratios (0, 5, 10 and 15) % of (NBR). Tensile characteristics and wear rates of these blends were studied for all mixing ratios. The microstructure of fracture surfaces of the prepared samples were investigated by optical microscope. The results were showed that strain rates of the resin material increase after blending it with rubber while the ultimate tensile strength and Young’s modulus values of it will decrease. It is also noticed that the wear rate of resin decreases with increasing of (NBR) content.
Keywords:<
... Show MoreIn this research, damping properties for composite materials were evaluated using logarithmic decrement method to study the effect of reinforcements on the damping ratio of the epoxy matrix. Three stages of composites were prepared in this research. The first stage included preparing binary blends of epoxy (EP) and different weight percentages of polysulfide rubber (PSR) (0%, 2.5%, 5%, 7.5% and 10%). It was found that the weight percentage 5% of polysulfide was the best percentage, which gives the best mechanical properties for the blend matrix. The advantage of this blend matrix is that; it mediates between the brittle properties of epoxy and the flexible properties of a blend matrix with the highest percentage of PSR. The second stage
... Show MoreIn this study, plastic wastes named (PET and PVC) were used to prepare polymer matrix composite (PMC) which can be used in different applications. Composite materials were prepared by mixing unsaturated polyester resin (UP) with plastic wastes, two types of plastic waste were used in this work included polyethylene-terephthalate (PET) and Polyvinyl chloride (PVC) with various weight fractions (0, 5,10,15, 20 and 25%) added as a filler in flakes form. In this work, some of the tests that were carried out included (tensile, bending, and compressive strength) as mechanical tests, in addition to (thermal conductivity and water absorption) as physical tests. The values of tensile, compressive strength and Young's modulus of UP increased after
... Show MoreIn this research, the effect of adding two different types of reinforcing particles was investigated, which included: nano-zirconia (nano-ZrO2) particles and micro-lignin particles that were added with different volume fractions of 0.5%, 1%, 1.5% and 2% on the mechanical properties of polymer composite materials. They were prepared in this research, as a complete prosthesis and partial denture base materials was prepared, by using cold cure poly methyl methacrylate (PMMA) resin matrix. The composite specimens in this research consist of two groups according to the types of reinforced particles, were prepared by using casting methods, type (Hand Lay-Up) method. The first group consists of PMMA resin reinforced by (nano-ZrO
... Show MoreSynthetic polymers such as polyurethane are used widely in the field of biomedical applications such as implants or part of implant systems.
This paper focuses on the preparation of base polymer matrix composite materials by (Hand Lay-Up) method, and studying the effect of selected grain size (32, 53, 63, 75, and 90) µm of (Reenia) particles on some properties of the prepared composite.
Mechanical tests were used to evaluate the prepared system (Tensile, Compression, Impact, and Hardness) tests, and a physical test of (Water absorption %), and all tests were accomplished at room temperature.
Where results showed tensile test (maximum tensile strength and modulus of elasticity) high at small grain size while
... Show MoreThis search aim to measure Hardness for Epoxy resin and for unsaturated Polyester resin as base materials for composite Hybrid and the materials used is Hybrid fiber Carbon-Kevlar. The Hand Lay-up method was used to manufacture plates of Epoxy resin (EP) and unsaturated Polyester EP,UPE backed by Hybrid fiber (Carbon-Kevlar) and with small volume fraction 5,10 and 15 for every there are Layer of fibers (1,2 and 3). The hardness test was count for material EP, UPE resin and there composites and that we notice that the Hardness (HB) decreased with increase of temperatures.
This study included preparation for the unsaturated polyester samples before and after reinforced by Alumina oxide powder and copper oxide powder of different volume fraction amounting (3%,5%,8%). And this reearch included study of some of mechanical properties such as (hardness,compressive and wear).The results showed that increase of the hardness and compressive strength after the reinforced and increase with the volume fraction increase.As the wear test show that the wear rate increases with applied load from the different load(5,10,15)N,and the wear rate decreases with the volume fraction increase.
Abstract
In the present study, composites were prepared by Hand lay-up molding. The composites constituents were epoxy resin as a matrix, 6% volume fractions of glass fibers (G.F) as reinforcement and 3%, 6% volume fractions of preparation natural material (Rice Husk Ash, Carrot Powder, and Sawdust) as filler. Studied the erosion wear behavior and coating by natural wastes (Rice Husk Ash) with epoxy resin after erosion. The results showed the non – reinforced epoxy have lower resistance erosion than natural based material composites and the specimen (Epoxy+6%glass fiber+6%RHA) has higher resistance erosion than composites reinforced with carrot powder and sawdust at 30cm , angle 60
... Show MoreThe present study investigated the impact of fuel kind on the emitted emissions at the idling period. Three types of available fuels in Iraq were tested. The tests conducted on ordinary gasoline with an octane number of 82, premium gasoline with an octane number of 92, and M20 (consist of 20% methanol and 80% regular gasoline). The 2 liters Mercedes-Benz engine was used in the experiments.
The results showed that engine operation at idle speed emits high levels of CO, CO2, HC, NOx and noise. The produced emission levels depend highly on fuel type. The premium gasoline (ON=92) represents the lower emissions level except for noise at all idling speed. Adding methanol to ordinary gasoline (ON=82) showed high levels of emi
... Show MoreIn this work polymeric composites were done from unsaturated polyester as a matrix reinforced with glass fiber type (E-glass) with two different volume fraction 20% & 40%. Fatigue tests showed that the number of fatigue cycles to failure limit for samples reinforced with uniform (woven Roving 0-90°) E-glass fiber and random (continuous fibers) with volume fraction 40% more than that for the same samples with volume fraction 20%. Also the fatigue results showed that the uniform samples failed with fatigue cycles more than that of random.