Sulphated zirconia (SZ) is one of the most important solid acid catalysts was synthesize at different operating conditions, different calcination temperature and sulfonating time has been used. The prepared catalyst was distinguished by X-ray Diffraction (XRD), particle size and morphology of catalyst were checked by atomic force microscopy (AFM) and scanning electron microscopy (SEM) respectively, in addition to analysis by (DTA) Differential thermally and Energy Dispersive X-Ray (EDX). Finally, the N2 adsorption-desorption was used to measure the surface area (BET) and pore volume. High degree of tetragonal crystallinity was obtained 90 %, and surface area of 169 m2/g and pore volume of 0.39 cm3g-1 at 600°C calcination temperature for 3
... Show MoreMoisture damage is one of the most significant troubles that destroy asphaltic pavement and reduces road serviceability. Recently, academics have noticed a trend to utilize fibers to enhance the efficiency of asphalt pavement. This research explores the effect of low-cost ceramic fiber, which has high tensile strength and a very high thermal insulation coefficient, on the asphalt mixture's characteristics by adding three different proportions (0.75%, 1.5%, and 2.25%). The Marshall test and the Tensile Strength Ratio Test (TSR) were utilized to describe the impact of ceramic fiber on the characteristics of Marshall and the moisture susceptibility of the hot mix asphalt mixture. The Field Emission Scanning Electron Microsc
... Show MoreThis paper investigated the treatment of textile wastewater polluted with aniline blue (AB) by electrocoagulation process using stainless steel mesh electrodes with a horizontal arrangement. The experimental design involved the application of the response surface methodology (RSM) to find the mathematical model, by adjusting the current density (4-20 mA/cm2), distance between electrodes (0.5-3 cm), salt concentration (50-600 mg/l), initial dye concentration (50-250 mg/l), pH value (2-12 ) and experimental time (5-20 min). The results showed that time is the most important parameter affecting the performance of the electrocoagulation system. Maximum removal efficiency (96 %) was obtained at a current density of 20 mA/cm2, distance be
... Show More
The ability of pulverized walnut-shell to remove oil from aqueous solutions has been studied. It involves two-phase process which consists of using walnut-shell as a filtering bed for the accumulation and adsorption of oil onto its surface. Up to 96% oil removal from synthetic wastewater samples was achieved while tests results showed that 75% of oil can be removed from the actual wastewater discharged from Al- Duara refinery in the south of Baghdad.
Pectin is available in many plants and in this study, the peels of tomatoes and beet were used to be an economical source of pectin production instead of dumping it with waste or using it as animal feed. The pectin extracted from the peels using different solutions, namely citric acid (2 M), oxalic acid (2%) and hydrochloric acid (0.5 M) the outcome of the extraction methods, 7. 1%, 6% and 11% respectively for tomatoes peels, while the pectin of beet peels were 8%, 6.5%, and 8.3%, and the highest percentage obtained in the manner of hydrochloric acid adopted in the manufacture of yogurt.Yogurt was manufactured with four treatments, in the first treatment standard pectin was added and the second treatment in addition to the pectin extracted
... Show MoreThis investigation was carried out to study the treatment and recycling of wastewater in the cotton textile industry for an effluent containing three dyes: direct blue, sulphur black and vat yellow. The reuse of such effluent can only be made possible by appropriate treatment method such as chemical coagulation. Ferrous and ferric sulphate with and without calcium hydroxide were employed in this study as the chemical coagulants.
The results showed that the percentage removal of direct blue ranged between 91.4 and 94 , for sulphur black ranged between 98.7 and 99.5 while for vat yellow it was between 97 and 99.
Industrial development has recently increased, including that of plastic industries. Since plastic has a very long analytical life, it will cause environmental pollution, so studies have resorted to reusing recycled waste plastic (sustainable plastic) to produce environmentally friendly concrete (green concrete). In this research, producing environmentally friendly load-bearing concrete masonry units (blocks) was considered where five concrete mixtures were compressed at the blocks producing machine. The cement content reduced from 400 kg/m3 (B-400) to 300 kg/m3 (B-300) then to 200 kg/m3 (B-200). While (B-380) was produced using 380 kg/m3 cement and 20 kg/m3 nano-sil
... Show MoreOne of the important objectives of the varistor is for a sustainable environment and reduce the pollution resulting from the frequent damage of the electrical devices and power station waste. In present work, the influence of Al2O3 additives on the non –linear electrical features of SnO2 varistors, has been investigated, where SnO2 ceramic powder doped with Al2O3 in three rates (0.005, 0.01, and 0.05), the XRD test improved that SnO2 is the primary phase, while CoCr2O4, and Al2O3 represent the secondary phases. The electrical tests of all prepared samples confirmed that the increasing of Al2O3 rates and sintering temperature improves and increase the electrical features, where the best results obtained at Al2O3 (0.05) and 1000℃, the non
... Show MoreThe contamination of soil with the wastes of oil industry products that are complex mixtures of hydrocarbons increased recently due to the large development of oil industries in Iraq. This study deals with the remediation of low permeability contaminated clayey soil by using the enhanced electrokinetic technique (EK). The contaminated soil samples obtained from Thi-Qar oil refinery plant in Al-Nassyriah city, where the byproducts of refinery plant are disposed into that site. The byproduct contaminant treated as total petroleum hydrocarbons (TPH) to avoid dealing and complexity of treating the individual minerals and compounds consisting the contaminant. The initial concentrations of TPH were (702.7, 1168, 1235) ppm in the contaminated s
... Show More