The sol-gel route using an agar gel with calcium nitrate and phosphate solution as starting materials for producing hydroxyapatite (HAP). The product formed were needle like, zigzag and straight fibres. The fibrous products on sintering transformed into stoichiometric HAP with a biological Ca/P ratio of 1.67. The influences of pH, temperature, nature of base and phosphate solution on the growth of fibrous HAP were studied. The pH of the solution was found to greatly influence the growth rate and morphology of the resultant product. The optimum gel temperature was found to be 60oC and sintering temperature of 900oC for 1 hour. The crystalline, thermal, functional and morphological characteristics of the fibrous HAP were investigated.
Four mixed ligand complexes were prepared from 1,10-phenanthroline (Phen), 5-chlorosalicylic acid (CSA), and anthranilic acid (Anthra) dissolved in aqueous ethanol at a ratio of (1:1:1:1) M: Phen:CSA: Anthra, M(II)= Cu, Zn, Cd, and Hg. The prepared compounds were analyzed by flame atomic absorption, FT—IR, UV-Vis, and spectroscopic methods, as well as conductivity measurements and magnetic properties. After analyzing the prepared compounds using the acquired data, the complexes formed by mixing ligands were concluded to adopt an octahedral geometry. That study has been conducted to test the inhibitory effectiveness of the complexes (1,10-Phenanthroline (Phen), 5-Chlorosalicylic acid (CSA), Na[Cu(Phen)(CSA)(Anthra), Na[Zn(Phen)(CSA)(Anthr
... Show MoreThe study has tackled three important variables on the strategic and organizational level, that are : (Administrative skill, strategic Entrepreneurship and organizational flexibility). Through the statistical analysis is, the research hers have sought to identify the relation among them. The study has been applied on a sample of (44) private banks in Iraq. A questionnaire, which has been designed according to a number of international standards, has been used. It's made of (29) items that cover the three variables to test their hypotheses. A number of statistical tools have been used A number of conclusion have been reached and recommendations have also been suggested.
One technique used to prepare nanoparticles material is Pulsed Laser Ablation in Liquid (PLAL), Silver Oxide nanoparticles (AgO) were prepared by using this technique, where silver target was submerged in ultra-pure water (UPW) at room temperature after that Nd:Yag laser which characteristics by 1064 nm wavelength, Q-switched, and 6ns pulse duration was used to irradiated silver target. This preparation method was used to study the effects of laser irradiation on Nanoparticles synthesized by used varying laser pulse energy 1000 mJ, 500 mJ, and 100 mJ, with 500 pulses each time on the particle size. Nanoparticles are characterized using XRD, SEM, AFM, and UV-Visible spectroscopy. All the structural peaks determined by the XRD
... Show MoreA variety of liquid crystals comprising heterocyclics 1,3,4-oxadiazol ring [III], aminooxazol [IV]a, and aminothiazol [IV]b were synthesized through a number of steps, beginning of the reaction of 3, 3'- dimethyl - [1, 1'-biphenyl] -4, 4'- diamin, ethyl monochloroacetate and sodium acetate to synthesize diacetate compound[I]. The diester reacted with hydrazine hydrate(N2H4-H2O) to give dihydrazide compound [II], then reacted with Pyruvic acid and phosphorous oxychloride to produce diketone compound [III]. The last compound was reacted with urea and thiourea to give aminooxazol and aminothiazol respectively. The synthesized compounds actually characterized and determined the structures by melting points, FT-IR and 1H-NMR spectroscopies. By u
... Show MoreThis study discussed the effects of doping with silver (Ag) on the optical and structural properties of
CdO nanoparticles at different concentrations 0, 1, 2, 3, 4, 5 wt% prepared by the precipitation method. The
materials were annealed at 550˚C for 1 h. The structural, topographical, and optical properties were
diagnosed by X-ray diffraction analysis, atomic force instrument, and visible and ultraviolet spectrometers.
The results show that the average diameter of the grains depends on the percentage of added silver to the
material, as the diameter decreased from 88.8 to 59.7 nm, and it was found that the roughness increased from
5.56 to 26.5. When studying the optical properties, it was noted that th
In this paper, two types of iron oxide nanomaterial (Fe3O4) and nanocomposite (T-Fe3O4) were created from the bio-waste mass of tangerine peel. These two materials were utilized for adsorption tests to remove cefixime (CFX) from an aqueous solution. Before the adsorption application, both adsorbents have been characterized by various characterizations such as XRD, FTIR, VSM, TEM, and FESEM. The mesoporous nano-crystalline structure of Fe3O4 and T-Fe3O4 nanocomposite with less than 100-nm diameter is confirmed. The adsorption of the obtained adsorbents was evaluated for CFX removal by adjusting several operation parameters to optimize the removal. The optimal conditions for CFX removal were found to be an initial concentration of 40 and 50 m
... Show MorePraise be to God, Lord of the worlds, and peace and blessings be upon our master Muhammad and his family and companions as follows:
For God Almighty has swapped for every age a group of religious scholars who give news to the narrators, so that they can lie against the Sunnah of the Mustafa, who is among those who memorized Ibn Al-Mulqin, as he followed the ruler in his book Al-Badr Al-Munir in the Hadith of Al-Sharh Al-Kabeer, and our research included two topics, which we explained in the first topic: The sequels in which the teacher's son Al-Malqin disagreed, and we discussed in the second topic: the followings in which Ibn Al-Malqin agreed to rule.
This research included important results, th
SUMMARY. – Nanocrystalline thin fi lms of CdS are deposited on glass substrate by chemical bath deposited technique using polyvinyl alcohol (PVA) matrix solution. Crystallite size of the nanocrystalline films are determining from broading of X-ray diffraction lines and are found to vary from 0.33-0.52 nm, an increase of molarity the grain size decreases which turns increases the band gap. The band gap of nanocrystalline material is determined from the UV spectrograph. The absorption edge and absorption coefficient increases when the molarity increases and shifted towards the lower wavelength.