The aim of this research is to employ starch as a stabilizing and reducing agent in the production of CdS nanoparticles with less environmental risk, easy scaling, stability, economical feasibility, and suitability for large-scale production. Nanoparticles of CdS have been successfully produced by employing starch as a reducing agent in a simple green synthesis technique and then doped with Sn in certain proportions (1%, 2%, 3%, 4%, and 5%).According to the XRD data, the samples were crystallized in a hexagonal pattern, because the average crystal size of pure CdS is 5.6nm and fluctuates in response to the changes in doping concentration 1, 2, 3, 4, 5 %wt Sn, to become 4.8, 3.9, 11.5, 13.1, 9.3 nm respectively. An increase in crystalline size has been noticed in the doped CdS than in the pure CdS. The particle size is within the range of 24-103 nm, according to SEM data from pure CdS and of the doped with Sn particles. The band gap's energy values, according to UV-Vis reflection spectroscopy were 3.06,2.61 ,2.63, 2.63, 2.66,2.69 eV for pure and doped with Sn 1%, 2%, 3%, 4%, 5% respectively. The grain size and roughness rate of pure CdS materials and doped with Sn are shown in AFM results 2.16,2.39,10.07,11.33, 12.47,18.56 nm and average diameter is 30.15, 11.71, 66.06, 48.27,82.011, 80.35 nm for pure and doped with tin 1%, 2%, 3%, 4%, 5% respectively.
In order to scrutinize the impact of the decoration of Sc upon the sensing performance of an XN nanotube (X = Al or Ga, and XNNT) in detecting sarin (SN), the density functionals M06-2X, τ-HCTHhyb, and B3LYP were utilized. The interaction of the pristine XNNT with SN was a physical adsorption with the sensing response (SR) of approximately 5.4. Decoration of the Sc metal into the surface of the AlN and GaN led to an increase in the adsorption energy of SN from −3.4 to −18.9, and −3.8 to −20.1 kcal/mol, respectively. Also, there was a significant increase in the corresponding SR to 38.0 and 100.5, the sensitivity of metal decorated XNNT (metal@XNNT) is increased. So, we found that Sc-decorating more increases the sensitivity of GaNN
... Show MoreIn this research study Hardness (shore D), Water absorption,
Flexural, Impact Test, and Fracture Toughness of polymer nano
composites. The polymer nano composites based on unsaturated
polyester resin reinforced with Kevlar fibers (K.F). The samples are
attended by hand lay – up method according to (Rule mixture) for
various volume fractions of unsaturated polyester resin, fiber and
carbon nanotube. The polyester resin was matrix strengthened with
3% volume fraction from Kevlar fiber and (0.5%, 1%, 1.5%, 2%)
volume fractions of carbon nanotube. The water absorption, hardness
(shore D), flexural test, impact test and toughness fracture properties
were studied. Results showed that the water absorption increas
In this work magnetite/geopolymer composite (MGP) were synthesized using a chemical co-precipitation technique. The synthesized materials were characterized using several techniques such as: “X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), vibrating sample-magnetometer (VSM), field-emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), Brunauer–Emmett–Teller (BET) and Barrentt-Joyner-Halenda (BJH)” to determine the structure and morphology of the obtained material. The analysis indicated that metal oxide predominantly appeared at the shape of the spinel structure of magnetite, and that the presence of nano-magnetite had a substantial impact on the surface area and pore st
... Show MoreThe work concerned with studying the effect of (SiO2) addition as a
filler on the adhesive properties of (PVA). Samples were prepared as
sheets by using casting method. The mechanical properties showed
that increase in tensile strength from (34MPa) to (68MPa) when
(SiO2) added to (PVA). The adhesive strength showed that joint
properties depend upon specific adhesive characteristic of material
(PVA) and (SiO2\PVA)composites at different concentrations (1.5%,
2.5%, 3.5%, 4.5wt%), the cohesive strength of the adhesive material,
the joint design, and adherent type (Sponge Rubber(SR), Natural
leather (NL), Vulcanized Rubber(VR), and Cartoon). The results
proved the tensile strength increased with (SiO2) ratio, so
To test the effect of 4 levels of nitrogen (i.e. 0, 45, 90 and 135 Kg N ha-1) as urea (46% N) and 3 levels of phosphorus (i.e. 0, 17.5 and 35 Kg P ha-1) as triple superphosphate (21.8% P) on yield and concentration of dill (Anethum graveolens L. local cultivar) seed oil this experiment was carried out during winter season of 1999 - 2000 at the experimental field of Agriculture College, Abu-Ghraib.
Both fertilizers were applied in two equal splits, first at seeds sowing and the second was added one month after emergence. Dried and ground seed samples were subjected to water distillation for extraction of volatile oils
Result indicated that fertilization of dill plants with 90 Kg N
... Show MoreIn this study, the effect of grafting with magnesium (Mg) ratios (0.1, 0.3, 0.5) on the structural and optical properties of cadmium oxide films (CdO) was studied, as these films were prepared on glass bases using the method of pulse laser deposition (PLD). The crystallization nature of the prepared membranes was examined by X-ray diffraction technique (XRD), which showed that the synthesis of the prepared membranes is polycrystalline, and (AFM) images also showed that the increased deformation with magnesium led to an increase in the grain size ratio and a decrease in surface roughness, as well as the absorption coefficient was calculated. And the optical energy gap for the prepared membranes, where it was found that the absorption coef
... Show MoreIn vivo study revealed that ZnO nanoparticles treatment of Streptococcus SPP contaminated injured skin showed good prognosis and good healing process include complete regeneration of the epithelial cells of the epidermis and increase of cellulartiy of the dermal content compared with untreated group. In conclusion, treatment of S. pyogenes infected skin with Zinc oxide nanoparticles concentration (2 mg/ml) limit the skin damage and localized the lesion to the incision site with good healing process