Study was made on the optical properties of Ge2oSe8othinfilms prepared by vac-uum evaporation as radiated by (0,34,69) Gy of 13 ray.The optical band gab Eg and tailing band A.Et were studied in the photon energy range ( 1 to 3)eV. The a-Ge20Se8o film was found to be indirect gap with energy gap of (1.965,1.9 , 1.82) eV at radiated by B ray with absorption doses of (0,34,69)Gy respectively.The Ea and AEt of Ge20Se80 films showed adecrease in E8 and an increase in AEt with radiation. This be-havior may be related to structural defects and dangling bonds.
In this work, (ZnO)1-x(MnO2)x compounds were synthesized with composition (x=0, 0.1, 0.2, 0.3, 0.4, and 0.5) of manganese oxide content using solid state reaction. Thin films were prepared from these compounds on glass substrates at room temperature using pulsed laser deposition method. The structure of the prepared compounds and thin films were analyzed using x-ray diffraction while the optical properties was measured using UV-visible spectrophotometry. It was found that the synthesized composites declared many peaks in the diffraction pattern which indicate polycrystalline structure with hexagonal wurtzite hexagonal structure of ZnO, and MnO2 and Mn2O3 secondary phases. A narrowing in the optical e
... Show MoreTraditional programs and the tedious and financially costly processes they require are no longer the best choice for content makers. The continuous development and development have led to the emergence of competitive software that offers capabilities that are more suitable for aesthetic needs, as it breaks down stereotypical frameworks from the familiar to the unfamiliar to be more suitable for graphic subjects in terms of dealing with the requirements of the digital content industry. Video for communication platforms, as it has more advantages than traditional software and the flexibility and high quality it offers at the level of the final product, All of this contributed to supplementing the image with aesthetic employments with data
... Show MoreThis study investigates the influence of phosphoric acid (H3PO4) molarity (2 M, 4 M, and 6 M) on the structural, thermal, optical, and electrical properties of polyvinyl alcohol (PVA)/20% graphene oxide (GO) composite films. X-ray diffraction analysis revealed a semi-crystalline nature for PVA, with characteristic peaks at 19.7 degrees and 42 degrees, and crystalline peaks for GO at 10.1 degrees and 39.8 degrees. The addition of H3PO4 to the PVA/GO composite resulted in the disappearance of GO crystalline peaks, suggesting reduced crystallinity. Differential scanning calorimetry revealed a reduction in both glass transition and melting temperatures as H3PO4 concentration increased. Pure PVA exhibited Tg and Tm values of 68.9 degrees C and 1
... Show MoreThe structure, optical, and electrical properties of SnSe and its application as photovoltaic device has been reported widely. The reasons for interest in SnSe due to the magnificent optoelectronic properties with other encouraging properties. The most applications that in this area are PV devices and batteries. In this study tin selenide structure, optical properties and surface morphology were investigated and studies. Thin-film of SnSe were deposit on p-Si substrates to establish a junction as solar cells. Different annealing temperatures (as prepared, 125,200, 275) °C effects on SnSe thin films were investigated. The structure properties of SnSe was studied through X-ray diffraction, and the results appears the increasing of the peaks
... Show MoreGamma - irradiation effect on polymethylmethacrylate (PMMA) samples has been studied using Positron Annihilation Lifetime (PAL) method. The orthopositronium (o-Ps) lifetime τ3, hence the o-ps parameters, the volume hole size (Vh) and the free volume fraction (Ꞙh) in the irradiated samples were measured as a function of gamma-irradiation dose up to 28.05 kGy. It has been shown that τ 3, Vh, and Ꞙh, are increasing in general with increasing gamma-dose, to reach a maximum percentage increment of 22.42% in τ3, 60% in Vh and 29.5% in Ꞙh, at. 2.55 kGy, whereas τ2 reaches maximum increment of 119. 7% at 7.65 kGy. The results s
... Show More