Structural and Optical Properties for Nanostructure (Ag2O/Si & Psi) Films for Photodetector Applications
...Show More Authors

Ag2O (Silver Oxide) is an important p-type (in chasm to most oxides which were n-type), with a high conductivity semiconductor. From the optical absorbance data, the energy gap value of the Ag2O thin films was 1.93 eV, where this value substantially depends on the production method, vacuum evaporation of silver, and optical properties of Ag2O thin films are also affected by the precipitation conditions. The n-type and p-type silicon substrates were used  with porous silicon wafers to precipitate  ±125 nm, as thick Ag2O thin film by thermal evaporation techniques in vacuum and via rapid thermal oxidation of 400oC and oxidation time 95 s, then characterized by measurement of XRD, optical properties and scanning electron microscopy properties (SEM). Maximum value of photo response obtained from p-Ag2O/p-PS/Si  photodetector results revealed  two peak sat 600 nm and 800 nm. According to the x-ray diffraction four peaks appear, (111), (200), (110) and (311) Ag, respectively, (polycrystalline film) and lattice constant of (4.077 Å). Also the results showed a sharp increasing in the absorption-wave length plot of Ag2O film at UV and IR regions. The accumulation of the stars-like are semi-regular of the Ag2O nanocrystals on the surface of p-type PS and the other diffuse inside the pores in a nearly uniform distribution with a different grain size on the surface. The results of the dislocation density and strain are decreased with the grain size increasing.

Scopus Clarivate Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Thu Apr 27 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Radiation Effect on the Optical& Structural Properties of CdTe: Zn thin Films
...Show More Authors

The Films of CdTe:Zn were prepared on a glass by using vacuum vapor deposition technique .The x-ray diffraction pattern revealed that the films have polycrystalline with FCC structure and the preferred orientation was along (111) plane.  The films were exposed to a low dose of gamma ray.(5µCi for 30 days) Transmission and absorptance spectra were recorded in the range of (400-1100) nm before and after irradiation. It was found that irradiation has a clear effect on the optical and structural properties which include the transmition and absorption spectra, extinction coefficient, refractive index, and the energy gap.

View Publication Preview PDF
Publication Date
Fri Jun 01 2012
Journal Name
Advances In Materials Physics And Chemistry
The Effect of Zn Concentration on the Optical Properties of Cd10–xZnxS Films for Solar Cells Applications
...Show More Authors

ABSTRACT:In this paper, Cd10–xZnxS (x = 0.1, 0.3, 0.5) films were deposited by using chemical spray pyrolysis technique, the molar concentration precursor solution was 0.15 M/L. Depositions were done at 350°C on cleaned glass substrates. X-ray dif- fraction technique (XRD) studies for all the prepared film; all the films are crystalline with hexagonal structure .The optical properties of the prepared films were studied using measurements from VIS-UV-IR spectrophotometer at wave- length with the range 300 - 900 nm; the average transmission of the minimum doping ratio (Zn at 0.1%) was about 55% in the VIS region, it was decrease at the increasing of Zn concentration in the CdS films, The band gap of the doped CdS films was varied as 3.7, 3

... Show More
Preview PDF
Publication Date
Mon May 22 2023
Journal Name
Proceedings Of The 1st International Conference On Frontier Of Digital Technology Towards A Sustainable Society
Effect of thermal annealing on the structural and optical properties of Sb2Se3 thin films
...Show More Authors

In this paper the effect of thermal annealing on the structural and optical properties of Antimony Selenide (Sb2Se3) is investigated. Sb2Se3 powder is evaporated on clean amorphous glass substrates at room temperature under high vacuum pressure (4.5×10-6 mbar) to form thin films. The structural investigation was done with the aid of X-ray diffraction (XRD) and atomic force microscopy (AFM). The amorphous to polycrystalline transformation of these thin films was shown by X-ray diffraction analysis after thermal annealing. These films' morphology is explained. (UV-Vis ) spectra in ranges from 300 to 1100 nm was used to examine the optical properties of the films .The absorption coefficient and optical energy gap of the investigated films are

... Show More
View Publication Preview PDF
Scopus Crossref
Publication Date
Mon Apr 10 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect of Doping Cu on the Structural and Optical Properties of (CdTe) Thin Films
...Show More Authors

   In this research we studied  the structural and optical properties of (CdTe) thin films which have been prepared  by thermal evaporation deposition method on the glass substrate at R.T with thickness (450  25) nm., as  a function of doping  ratio with copper element  in (1,3,5) % rate .The structure  measurement  by X-ray diffraction (XRD) analyses shows that the single phase of (CdTe) with polycrystalline structure with a preferred orientation [111].   The optical  measurement shows that the (CdTe) films have a direct energy gap, and they decrease with the increase of doping ratio reaching to 5% . The optical constants are investigated and calculated, such as absorpti

... Show More
View Publication Preview PDF
Publication Date
Thu Feb 23 2023
Journal Name
Chalcogenide Letters
Fabrication and evaluation of CuAlSe2/Si photodetector
...Show More Authors

In this work, we have examined the spectral response of (p-CuAlSe2/n-Si) detector, (CAS) thin films deposited by thermal evaporation at RT with a thickness (450) nm, and annealing temperature at (473K) for 2 h. Optical transmission measurements displayed reasonably slight transmission besides higher absorbance trendy the visible region, energy gaps were observed by annealing, were found to be direct, and decreased with the effect of annealing. The extreme responsivity value arises at wavelength 459 nm, with improvement value of specific detectivity and quantum efficiency the annealing films be situated originate as greatest suitable aimed at numerous device application.

View Publication
Scopus Clarivate Crossref
Publication Date
Fri Mar 01 2019
Journal Name
Al-khwarizmi Engineering Journal
Design and Implementation of a Telemetry System for Environmental Applications
...Show More Authors

The Environmental Data Acquisition Telemetry System is a versatile, flexible and economical means to accumulate data from multiple sensors at remote locations over an extended period of time; the data is normally transferred to the final destination and saved for further analysis.

This paper introduces the design and implementation of a simplified, economical and practical telemetry system to collect and transfer the environmental parameters (humidity, temperature, pressure etc.) from a remote location (Rural Area) to the processing and displaying unit.

To get a flexible and practical system, three data transfer methods (three systems) were proposed (including the design and implementation) for rural area services, the fi

... Show More
View Publication Preview PDF
Publication Date
Wed Sep 12 2018
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Thickness Influence on Structural and Optical Properties of ZnO Thin Films Prepared by Thermal Evaporation
...Show More Authors

  A thermal evaporation technique was used to prepare ZnO thin films. The samples were prepared with good quality onto a glass substrate and using Zn metal. The thickness varied from (100 to 300) ±10 nm. The structure and optical properties of the ZnO thin films were studied. The results of XRD spectra confirm that the thin films grown by this technique have hexagonal wurtzite, and also aproved that ZnO films have a polycrystalline structure. UV-Vis measurement, optical transmittance spectra, showed high transmission about 90% within visible and infrared range. The energy gap is found to be between 3.26 and 3.14e.V for 100 to 300 nm thickness respectivly. Atomic Force Microscope AFM (topographic image ) shows the grain size incre

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Mon Jan 01 2018
Journal Name
Ibn Al-haitham Journal For Pure And Applied Science
Investigation of the Structural, Optical and Electrical Properties of AgInSe2 Thin Films
...Show More Authors

Publication Date
Thu May 25 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Optical and Structural Properties of SnO2 Thin Films Prepared by Sputtering Method
...Show More Authors

SnO2 thin films of different two thicknesses were prepared an glass substrate by DC magnetron sputtering. The crystal structure and orientation of the films were investigated by XRD patterns. All the deposited films are polycrystalline. The grain size was calculated as 25.35, 28.8 nm. Morphological and compositions of the films were performed by SEM and EDX analyses respectively. The films appeared compact and rougher surface in nature. The allowed direct band gap was evaluated as 3.85 eV, and other optical constants such as refractive index, extinction coefficient, real and imaginary parts of dielectric constants were determined from transmittance spectrum in the wavelength range (300-900) nm and also analyzed.
 

View Publication Preview PDF
Publication Date
Mon Oct 01 2012
Journal Name
Iraqi Journal Of Physics
Influence of substrate temperature on structural and optical properties of SnO2 films
...Show More Authors

Tin Oxide (SnO2) films have been deposited by spray pyrolysis technique at different substrate temperatures. The effects of substrate temperature on the structural, optical and electrical properties of SnO2 films have been investigated. The XRD result shows a polycrystalline structure for SnO2 films at substrate temperature of 673K. The thickness of the deposited film was of the order of 200 nm measured by Toulansky method. The energy gap increases from 2.58eV to 3.59 eV when substrate temperature increases from 473K to 673K .Electrical conductivity is 4.8*10-7(.cm)-1 for sample deposited at 473K while it increases to 8.7*10-3 when the film is deposited at 673K

View Publication Preview PDF