Slag of aluminum is a residue which results during the melting process of primary and secondary aluminum production. Salt slag of aluminum is hazardous solid waste according to the European Catalogue for Hazardous Wastes. Hence, recovery of aluminum not only saves the environment, but also has advantages of financial and economic returns. In this research, aluminum was recovered and purified from the industrial wastes generated as waste from both of State Company for Electrical and Electronic Industries (Baghdad/AlWaziriya) and General Company for Mechanical Industries (Babylon/-Al-Escandria). It was found that these wastes contain tiny proportions of other elements such as iron, copper, nickel, titanium, lead, and potassium. Wastes were recovered for green sustainability, saving energy and cost effectiveness. The method applied for recovering aluminum was pyro-metallurgical method by smelting and refining. X-Ray fluorescence spectroscopy and X- Ray diffraction techniques of the slag sample were used to determine the chemical analysis and phases, respectively. Melting experiments were conducted by using different types of fluxes (KAlF4, NaCl, KCl and AlCl3) at different percentages (0, 5, 10 %) and different melting temperatures (700, 750, 800oC). Design of Experiment (DOE) by Taguchi method, orthogonal array L9, was used in melting experiments. Melting efficiency of aluminum was equal to 84.7%. Electro-refining of aluminum was done by using anhydrous aluminum chloride and NaCl as ionic liquids at low temperature 100 ◦C in electro-refining method producing aluminum of 99% purity.
Algae have been used in different applications in various fields such as the pharmaceutical industry, environmental treatments, and biotechnology. Studies show that the preparation of nanoparticles by a green synthesis method is a promising solution to many medical and environmental issues. In the current study, the green alga Stigeoclonium attenuatum (Hazen) F.S. Collins 1909 was isolated and identified from the Al-Hillah River (Governorate of Babylon) in the middle of Iraq. The green synthesis by the aqueous extract of algae was used to prepare the nanoflakes of ZnO. Nanoflakes of ZnO are characterized by X-Ray diffraction (XRD) and scanning electron microscope (SEM) with flakes shape and dimensions ranging be
... Show MoreAdsorption is one of the most important technologies for the treatment of polluted water from dyes. Theaim of this study is to use a low-cost adsorbent for this purpose. A novel and economical adsorbent was used to remove methyl violet dye (MV) from aqueous solutions. This adsorbent was prepared from bean peel, which is an agricultural waste. Batch adsorption experiments were conducted to study the ability of the bean peel adsorbent (BPA) to remove the methyl violet (MV) dye. The effects of different variables, such as weight of the adsorbent, pH of the MV solution, initial concentration of MV, contact time and temperature, on the adsorption behaviour were studied. It was found experimentally that the time required to achieve equilibrium
... Show MoreSeveral industrial wastewater streams may contain heavy metal ions, which must be effectively removal
before the discharge or reuse of treated waters could take place. In this paper, the removal of copper( II)
by foam flotation from dilute aqueous solutions was investigated at laboratory scale. The effects of
various parameters such as pH, collector and frother concentrations, initial copper concentration, air flow
rate, hole diameter of the gas distributor, and NaCl addition were tested in a bubble column of 6 cm inside
diameter and 120 cm height. Sodium dodecylsulfate (SDS) and Hexadecyl trimethyl ammonium bromide
(HTAB) were used as anionic and cationic surfactant, respectively. Ethanol was used as frothers and the
AlO-doped ZnO nanocrystalline thin films from with nano crystallite size in the range (19-15 nm) were fabricated by pulsed laser deposition technique. The reduction of crystallite size by increasing of doping ratio shift the bandgap to IR region the optical band gap decreases in a consistent manner, from 3.21to 2.1 eV by increasing AlO doping ratio from 0 to 7wt% but then returns to grow up to 3.21 eV by a further increase the doping ratio. The bandgap increment obtained for 9% AlO dopant concentration can be clarified in terms of the Burstein–Moss effect whereas the aluminum donor atom increased the carrier's concentration which in turn shifts the Fermi level and widened the bandgap (blue-shift). The engineering of the bandgap by low
... Show MoreDoppler broadening of the 511 keV positron annihilation ??? ? was used to estimate the concentration of defects ?? different deformation levels of pure alnminum samples. These samples were compressed at room temperature to 15, 22, 28, 38,40, and 75 % thickness reduction. The two-state ^sitron-trapping model has been employed. 'I he s and w lineshape parameters were measured using high-resolution gamma spectrometer with high pure germanium detector of 2.1 keV resolution at 1.33 MeV of 60Co. The change of defects concentration (Co) with the deformation level (e) is found to obey an empirical formula of the form Cd - A £ B where A and ? are positive constants that depend mainly on the deformation procedure and the temperature at which the def
... Show MoreThe different parameters on mechanical and microstructural properties of aluminium alloy 6061-T6 Friction stir-welded (FSW) joints were investigated in the present study. Different welded specimens were produced by employing variable rotating speeds and welding speeds. Tensile strength of the produced joints was tested at room temperature and the the effecincy was assessed, it was 75% of the base metal at rotational speed 1500 rpm and weld speed 50 mm/min. Hardness of various zones of FSW welds are presented and analyzed by means of brinell hardness number . Besides to thess tests the bending properties investigat
... Show MoreThe purpose of this study is to investigate the histopathological response of dentinopulpal
response of human teeth to the Er: YAG laser cavity preparation in comparison with the conventional
class I cavity preparation. Thirty five sound human upper and lower first premolar teeth which were
needed to be extracted for orthodontic purposes were used in the study. Regarding to the method of
cavity preparation, the teeth were grouped into three groups; Group1; Control group which consists of
seven sound teeth without cavity preparation, Group2; Conventional cavity preparation group and group
3; Er: YAG laser cavity preparation group. Each of Group2 and3 consists of fourteen teeth that is
subdivided into: A. 7teeth that e
The daily practices of humans produce various types of waste, which are a threat to the health and environment surrounding it, especially after the increase in quantities as a result of population growth and technological development, and here came the need for recycling solid waste as one of the modern concepts that achieve environmental benefits, The aim of the research is to evaluate the project of sorting and recycling of solid waste in the district of Mahmoudiya and whether its work is sustainable ,Conforming to modern standards, using standard checklists to determine the gap between the current laboratory reality and the requirements of those standards , Using the case study methodology as the most appropriate approach
... Show More